| 铸造Al-Si合金中Sr与B间反应产物的研究 |
| 廖恒成; 孙国雄 |
| 东南大学机械工程系; 南京210018 |
|
| Investigations on the Resultant Between Sr and B in Al-Si Casting Alloys |
| LIAO Hengcheng; SUN Guoxiong |
| Department of Mechanical Engineering; Southeast University; Nanjing 210018 |
引用本文:
廖恒成; 孙国雄 . 铸造Al-Si合金中Sr与B间反应产物的研究[J]. 金属学报, 2003, 39(2): 155-158 .
,
.
Investigations on the Resultant Between Sr and B in Al-Si Casting Alloys[J]. Acta Metall Sin, 2003, 39(2): 155-158 .
[1] Kulunk B, Zulian D J. JOM, 1996; 48: 60 [2] Lu S Z, Hellawell A. J Cryst Growth, 1985; 73: 316 [3] Lu S Z, Hellawell A. Metall Trans, 1987; 18A: 1721 [4] Pekguleryuz M O, Gruzleski J E. AFS Trans, 1988; 96:55 [5] Sigworth G K. AFS Trans, 1983; 91: 7 [6] Chai G, Backrud L. AFS Trans, 1992; 100: 847 [7] Liao H C. PhD Thesis, Nanjing, Southeast University,2000: 40(廖恒成.东南大学博士学位论文,南京, 2000:40) [8] Liao H C, Ding Y, Sun G X. Acta Metall Sin, 2002; 38: 245(廖恒成,丁 毅,孙国雄.金属学报, 2002;38:245) [9] Liao H C, Ding Y, Sun G X. Foundry, 2002; 51: 148(廖恒成,丁 毅,孙国雄.铸造,2002;51:48) [10] Liao H C, Ding Y, Sun G X. Foundry, 2002, 51:(廖恒成,丁 毅,孙国雄.铸造, 2002;51:) [11] Lu H T, Wang L C, Kong S K. J Chin Foundryman'sAssociation, 1981; 29: 10 [12] Sigworth G K, Guzowski M M. AFS Trans, 1985; 93: 907 [13] Apelian D, Cheng J A. AFS Trans, 1986; 94: 797 [14] Sritharan T, Li H. J Mater Sci Technol, 1997; 63: 585 [15] Liao H C, Sun Y, Sun G X, Tang C X. Foundry, 2000; 49:251(廖恒成,孙瑜,孙国雄,汤崇熙.铸造, 2000;49:251) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|