| 两相共晶NiAl-9Mo合金的蠕变行为 |
| 任维丽 郭建亭 周继扬 |
| 大连理工大学材料工程系;大连116024 |
|
引用本文:
任维丽; 郭建亭; 周继扬 . 两相共晶NiAl-9Mo合金的蠕变行为[J]. 金属学报, 2002, 38(9): 908-913 .
[1] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whit-tenberger J D. Intermetallics, 1995; 3: 99 [2] Kumar K S, Mamar S K, Viswanadham S K. Ada Metall Mater, 1992; 40: 1201 [3] Cui C Y, Chen Y X, Guo J T, Li D X, Ye H Q. Mater Lett, 2000; 43: 303 [4] Guo J T, Cui C Y, Chen Y X, Li D X, Ye H Q. Intermetallics, 2001; 9: 28 [5] Whittenberger J D. J Mater Sci, 1987; 22: 394 [6] Whittenberger J D, Reviere R, Noebe R D, Oliver B F. Scr Metall Mater, 1992; 26: 987 [7] Whittenberger J D, Noebe R D, Johnson D R, Oliver B F. Intermetallics, 1997; 5: 173 [8] Whittenberger J D. J Mater Sci, 1988; 22: 235 [9] Qi Y H, Quo J T, Cui C Y, Li G S. Ada Metall Sin, 2001; 37: 957 (齐义辉,郭建亭,崔传勇,李谷松.金属学报,2001;37:957) [10] Yuan C, Quo J T, Yang H C, Wang S H. Acta Metall Sin,1998; 34: 858 (袁 超,郭建亭,杨洪才,王淑荷.金属学报,1998;34:858) [11] Dennison J P, Holrnes P D, Wilshire B. Mater Sci Eng,1978; 33: 35 [12] Cui C Y, Quo J T, Qi Y H, Ye H Q. Acta Metall Sin,accepted (崔传勇,郭建亭,齐义辉,叶恒强.金属学报,待发表) [13] Coble RL. J Appl Phys, 1963; 34: 1679 [14] Sherby O D, Burke P M. Prog Mater Sci, 1968; 13: 325 [15] Weetman J. J Appl Phys, 1957; 28: 362 [16] Cannon W R, Sherby O D. Metall Trans, 1970; 1: 1030 [17] Rudy M, Sauthoff G. Mater Sci Eng, 1986; 81: 525 [18] Pugh J W. Trans ASM, 1955; 47: 984 [19] Chen R S. Ph D Thesis, Dalian University of Technolodge, Dalian, 1999 (陈荣石.大连理工大学博士论文,大连,1999) [20] Ren W L, Quo J T, Li G S, Zhou J Y. J Mater Sci Technol,accepted [21] Monkman F C, Grant N. J Proc ASTM, 1956; 56: 593 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|