| Co,Cr和Ni对Fe3Al金属间化合物相平衡的影响 |
| 马钢 夏源明 |
| 中国科学院中国科学技术大学材料力学行为和设计重点实验室;合肥230027 |
|
引用本文:
马钢; 夏源明 . Co,Cr和Ni对Fe3Al金属间化合物相平衡的影响[J]. 金属学报, 2002, 38(9): 914-919 .
[1] Yang W Y, Sheng L Z, Sun Z Q, Huang Y D, Mao W M, Zhang B S, Ye C T. Ada Metall Sin, 1996; 32: 799 (杨王(王月),盛丽珍,孙祖庆,黄原定,毛卫民,张百生,叶春 堂.金属学报,1996;32:799) [2] Saito Y, Harada H. Mater Sci Eng, 1997; 223A: 1 [3] Saito Y. Mater Sci Eng, 1997; 223A: 10 [4] Nishizawa T, Hao S M, Hasebe M, Ishida K. Acta Metal,1983; 31: 1403 [5] Hao S M, Takayama T, Ishida K, Nishizawa T. MetallTrans, 1984; 15A: 1819 [6] Colinet C, Inden G, Kikuchi R. Acta Metall Mater, 1993;41: 1109 [7] Kikuchi R. Phys Rev, 1951; 81: 988 [8] Mohri T, Sanchez J M, Defontaine D. Acta Metall, 1985;33: 1171 [9] Ma G, Saito Y. Acta Metall Sin, 2000; 36: 243 (马 钢,齐藤良行.金属学报,2000;36:243) [10] Schlatte G, Pitsch W. Z Metallkde, 1975; 66: 660 [11] Hultgren R, Desai P D, Hankins D T, Gleiser M, Kelly K K, Wagman D D. Selected Values of the Thermodynamic Properties of the Elements and Binary Alloys. Metals Park, OH: ASM, 1973 [12] Miedema A R, Boom R, De Boer F R. J Less-CommonMet, 1975; 41: 283 [13] Villars P, Calvert L D. Pearson's Handbook of Crystallo-graphic Data for Inter- Metallic Phases. American Society for Metals, November 1985 [14] Inden G. J Physique, 1977; C7: 373 [15] Inden G. Mater Res Soc Symp Proc, 1983; 19: 175 [16] Inden G. Z Metallkde , 1977; 68: 529 [17] Ma G, Xia Y M. Acta Metall Sin, 2001; 37: 1147 (马 钢,夏源明,金属学报,2001;37:1147)F |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|