| Ti含量对(Zr0.59Cu0.18Ni0.13Al0.10)100-xTix合金非晶形成能力的影响 |
| 邢大伟 孙剑飞 沈 军 王 刚 严 明 柳 宇 |
| 哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001 |
|
| EFFECT OF Ti ADDITION ON THE GLASS--FORMING ABILITY OF (Zr0.59Cu0.18Ni0.13Al0.10)100-xTix ALLOYS |
| XING Dawei; SUN Jianfei; SHEN Jun; WANG Gang; YAN Ming; LIU Yu |
| School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001 |
引用本文:
邢大伟; 孙剑飞; 沈军; 王刚; 严明; 柳宇 . Ti含量对(Zr0.59Cu0.18Ni0.13Al0.10)100-xTix合金非晶形成能力的影响[J]. 金属学报, 2004, 40(4): 416-420 .
,
,
,
,
,
.
EFFECT OF Ti ADDITION ON THE GLASS--FORMING ABILITY OF (Zr0.59Cu0.18Ni0.13Al0.10)100-xTix ALLOYS[J]. Acta Metall Sin, 2004, 40(4): 416-420 .
[1] Wang W H, Wang W K, Bai H Y. Science in China, 1998;A7: 756 [2] Li C F, Saida J J, Matsushida M, Inoue A. Scr Mater,2000; 42: 923 [3] Zhang Y, Zhao D Q, Pan M X, Wang W H. J Non-CrystSolids, 2003; 315: 206 [4] de Boer F R, Boom R, Miedema A R, Niessen A K. Co- hesion in Metals. North Holland, Amsterdam, Elsevier Science, 1989: 378 [5] Lu Z P, Li Y, Ng S C. J Non-Cryst Solids, 2000; 270: 103 [6] Zhang H F, Ding B Z, Hu Z Q. Ada Metall Sin, 2001; 37: 1131(张海峰,丁炳哲,胡壮麒.金属学报,2001;37:1131) [7] Inoue A. Bulk Amorphous Alloys-Preparation and Fundamental Characteristics, Switzerland: Trans Tech Publications LTD., 1998: 3 [8] Lin X H. Ph.D. Thesis, California Institute of Technology, 1997: 63 [9] Johnson W L. MRS Bulletin, 1999; 10: 42 |
|