Ti含量对(Zr0.59Cu0.18Ni0.13Al0.10)100-xTix合金非晶形成能力的影响
邢大伟 孙剑飞 沈 军 王 刚 严 明 柳 宇
哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001
EFFECT OF Ti ADDITION ON THE GLASS--FORMING ABILITY OF (Zr0.59Cu0.18Ni0.13Al0.10)100-xTix ALLOYS
XING Dawei; SUN Jianfei; SHEN Jun; WANG Gang; YAN Ming; LIU Yu
School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001
引用本文:

邢大伟; 孙剑飞; 沈军; 王刚; 严明; 柳宇 . Ti含量对(Zr0.59Cu0.18Ni0.13Al0.10)100-xTix合金非晶形成能力的影响[J]. 金属学报, 2004, 40(4): 416-420 .
, , , , , . EFFECT OF Ti ADDITION ON THE GLASS--FORMING ABILITY OF (Zr0.59Cu0.18Ni0.13Al0.10)100-xTix ALLOYS[J]. Acta Metall Sin, 2004, 40(4): 416-420 .

全文: PDF(200 KB)  
摘要: Ti具有明显降低(Zr0.59Cu0.18Ni0.13Al0.10)100-xTix(x=0, 1, 2, ......6)合金液相线温度Tl并提高约化玻璃转变温度Trg的作用. 含Ti量不同的合金楔形试样中的非晶组织区域对比表明, x等于4左右的合金Zr56.64Cu17.28Ni{12.48Al9.6Ti4具有最好的玻璃 形成能力. 此时ΔTx=77.6℃, Trg(Tg/Tl)=0.65. 以电弧熔炼铜模铸造的方法可制备出此成分合金尺寸为直径10 mm、长70 mm的圆柱形完全非晶试样. 对含Ti量不同的楔形试样中过渡区(结晶--非晶混合组织区)结晶相的分析表明, 适量Ti的加入, 促进了合金熔体中多种金属间相的同时析出, 从而使各种结晶相之间的相互竞争和阻碍作用更强烈, 因而有助于 玻璃形成能力的提高.
关键词 : Zr基块体非晶合金,  Ti含量,  玻璃形成能力    
Abstract:The effect of Ti on glass--forming ability of bulk (Zr0.59Cu0.18Ni0.13Al0.10)100-xTix (x=0, 1, 2, ...... 6) alloys has been investigated by differential scanning calorimetry (DSC), differential thermal analysis (DTA), and X--ray diffraction (XRD). It is shown that the liquidus temperature Tl decreases obviously when Ti content (x) increases from 0 to 4, meanwhile the reduced glass temperature (Trg) increases from 0.62 to 0.65. When x exceeds 4, however, Tl increases and Trg decreases respectively with increasing Ti content. The wedge--shaped sample with x=4 has the largest amorphous region, i.e., has the highest relative glass--forming ability, and the relevant supercooled liquid region ΔTx is 77.6℃. The alloy with this composition can be cast into cylinder--like amorphous alloy with 10 mm in diameter and 70 mm in length or sheet--like with 3 mm thickness by arc melting and copper mold casting. More intermetallics phases exist in the amorphous--crystallization zone of the wedge--shape sample with x=4 than those of alloys with x=0 and x=2 as indicated by XRD results. It is suggested that the crystallization would be retarded by the interaction and competition of various phases, thus enabling a higher glass--forming ability.
Key words: Zr--based bulk amorphous alloy    Ti addition    glass--forming ability
收稿日期: 2003-04-16     
ZTFLH:  TG139.8  
[1] Wang W H, Wang W K, Bai H Y. Science in China, 1998;A7: 756
[2] Li C F, Saida J J, Matsushida M, Inoue A. Scr Mater,2000; 42: 923
[3] Zhang Y, Zhao D Q, Pan M X, Wang W H. J Non-CrystSolids, 2003; 315: 206
[4] de Boer F R, Boom R, Miedema A R, Niessen A K. Co- hesion in Metals. North Holland, Amsterdam, Elsevier Science, 1989: 378
[5] Lu Z P, Li Y, Ng S C. J Non-Cryst Solids, 2000; 270: 103
[6] Zhang H F, Ding B Z, Hu Z Q. Ada Metall Sin, 2001; 37: 1131(张海峰,丁炳哲,胡壮麒.金属学报,2001;37:1131)
[7] Inoue A. Bulk Amorphous Alloys-Preparation and Fundamental Characteristics, Switzerland: Trans Tech Publications LTD., 1998: 3
[8] Lin X H. Ph.D. Thesis, California Institute of Technology, 1997: 63
[9] Johnson W L. MRS Bulletin, 1999; 10: 42
[1] 杨群, 彭思旭, 卜庆周, 于海滨. 非晶态Ni80P20合金的玻璃转变和过冷液体性质[J]. 金属学报, 2021, 57(4): 553-558.
[2] 吕宝臣 刘海涛 任鑫 王晓亮 李刚 孙跃军. 高溶质浓度(伪)三元系金属玻璃原子密堆垛模型[J]. 金属学报, 2012, 48(2): 240-244.
[3] 胡强 曾燮榕 钱海霞 谢胜辉 盛洪超. 铁基块体非晶合金玻璃形成能力与特征自由体积的关系[J]. 金属学报, 2012, 48(11): 1329-1334.
[4] 吴泽宇 郭胜锋 李宁 柳林. Co对Fe--B--Y--Nb块体非晶合金玻璃形成能力及软磁性能的影响[J]. 金属学报, 2009, 45(2): 249-252.
[5] 孙亚娟 魏先顺 黄永江 沈 军. 稀土Gd掺杂对锆基块体非晶合金玻璃形成能力及力学性能的影响[J]. 金属学报, 2009, 45(2): 243-248.
[6] 董盼; 张甲; 常新春; 侯万良; 全明秀; 王建强 . Al--Co--Y体系中富 Al区非晶相的形成与结构演化[J]. 金属学报, 2008, 44(2): 227-232 .
[7] 徐民; 孙羽; 全明秀; 王沿东; 左良 . Fe--Co--Nd--Nb--B非晶合金的形成和软磁性能[J]. 金属学报, 2007, 43(7): 699-704 .
[8] 李宏祥; Seonghoon.Yi; 张新房; 王晓东 . Fe--C--Si--B--P--Cr--Mo--Al块体非晶合金的制备与压缩性能[J]. 金属学报, 2006, 42(7): 777-780 .
[9] 贺林; 孙军 . 氧对Zr-Cu-Ni-Al-Ti块体非晶合金热稳定性的影响[J]. 金属学报, 2006, 42(2): 134-138 .
[10] 彭德林; 沈军; 孙剑飞; 陈玉勇 . 氢对锆基块体非晶合金热膨胀系数和有效原子作用势的影响[J]. 金属学报, 2005, 41(8): 835-838 .
[11] 刘冬艳; 王成; 张海峰; 胡壮麒 . 铁基块状非晶合金的制备及性能[J]. 金属学报, 2005, 41(2): 209-213 .
[12] 门华; 徐坚 . Mg-CU-Zn-y块体金属玻璃的形成[J]. 金属学报, 2001, 37(12): 1243-1246 .
[13] 张恒;张邦维;谭肇升. Cu_(74)Ni_(12-x)Sn_xP_(14)合金的非晶形成趋势[J]. 金属学报, 1992, 28(12): 49-54.