| 高速钢W18Cr4V离子渗氮层组织对TiN膜与基体结合强度的影响 |
| 谢飞 何家文 |
| 江苏石油化工学院机械工程系; 常州 213016 |
|
引用本文:
谢飞; 何家文 . 高速钢W18Cr4V离子渗氮层组织对TiN膜与基体结合强度的影响[J]. 金属学报, 2000, 36(10): 1099-1103 .
[1] Gredic T, Zlatanovic M, Popovic N, Bogdanov Z. SurfCoat Technol, 1992; 54/55: 502 [2] van Stappen M, Malliet B, Stals L, de Schepper L, RocsJ R, Cells J P. Mater Sci Eng, 1991; A140: 554 [3] Spies H J, Larisch B, Hock K, Broszeit E, Schroder H-J.Surf Coat Technol, 1995; 74/75: 178 [4] Zlatanovic M. Surf Coat Technol, 1991; 48: 19 [5] Zlatanovic M, Kakas D, Mazibrada L, Kunosic A, MunzW-D. Surf Coat Technol, 1994; 64: 173 [6] Aming Y, Yufei L, Xiang G, Pengxing L. Proc Conf onHeat Treatment and Surface Engineering, Chicago, III,1988, Cincinnati, Ohio: ASM International, 1988: 43 [7] Dingremont N, Pianelli A, Bergmann E, MiChel H. SurfCoat Technol, 1993; 61: 187 [8] Buecken B, Leonhardt G, Wilberg R, Hoeck K, Spies H-J.Surf Coat Technol, 1994; 68/69: 244 [9] Zlatanovic M, Gredic T, Kunosic A, Backovic N, WhittleN. Surf Coat Technol, 1994; 63: 35 [10] Xie F, Yuan J W, Xu K W, He J W. Tool Eng, 1997;31(11): 3(谢飞,袁军伟,徐可为,何家文工具技术,1997;31(11):3) [11] Hultman L, Hentzell H T G, Sundgren J-E, JohanssonB-O, Helmersson U. Thin Solid Films, 1985; 124: 163 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|