相变存储器材料设计与多尺度模拟的研究进展
沈雪阳, 褚瑞轩, 蒋宜辉, 张伟()
西安交通大学 金属材料强度国家重点实验室 材料创新设计中心 西安 710049
Progress on Materials Design and Multiscale Simulations for Phase-Change Memory
SHEN Xueyang, CHU Ruixuan, JIANG Yihui, ZHANG Wei()
Center for Alloy Innovation and Design (CAID), State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049, China
引用本文:

沈雪阳, 褚瑞轩, 蒋宜辉, 张伟. 相变存储器材料设计与多尺度模拟的研究进展[J]. 金属学报, 2024, 60(10): 1362-1378.
Xueyang SHEN, Ruixuan CHU, Yihui JIANG, Wei ZHANG. Progress on Materials Design and Multiscale Simulations for Phase-Change Memory[J]. Acta Metall Sin, 2024, 60(10): 1362-1378.

全文: PDF(4227 KB)   HTML
摘要: 

大数据时代人工智能、5G、云计算等先进技术对数据存储与处理的需求急剧上升,而新型非易失性存储材料与器件的研发则为大幅提升算力提供了契机。同时,人工智能技术驱动的科学研究范式也为进一步提升存储器件性能提供了新的研发模式。本文聚焦于相变存储材料与器件在计算与数据驱动下的研究进展,详细论述了大尺度第一性原理分子动力学、新材料设计与高通量材料筛选、多尺度模拟与机器学习势开发等先进材料计算方法在相变存储材料研究中的具体应用,并展望了相变存储技术发展所面临的机遇与挑战。

关键词 : 相变存储材料,  第一性原理,  高通量计算,  多尺度模拟,  机器学习势    
Abstract:

In the era of big data, the demand for data storage and processing is increasing because of advanced technologies such as artificial intelligence (AI), 5G, and cloud computing. Emerging non-volatile memory materials and devices present remarkable opportunities to enhance computing capacity. Concurrently, the AI-driven scientific research paradigm introduces a new mode for improving device performance. This review focuses on recent advances in phase-change memory materials and devices, emphasizing computational- and data-driven methodologies. Phase-change materials (PCMs) operate based on rapid and reversible phase transitions between amorphous and crystalline states, where differences in electrical and optical properties are used to encode digital information. These materials typically consist of multicomponent alloys, with phase transitions involving melting, quenching, crystallization, glass relaxation, and crystal-crystal structural changes. To achieve a detailed atomistic understanding of PCMs, large-scale density functional theory (DFT) and DFT-based ab initio molecular dynamics (AIMD) simulations are essential. Comparisons between DFT/AIMD simulations and experimental results have clarified many fundamental aspects of PCM. The first part of this review provides an overview of the history and progress in large-scale ab initio simulations of PCMs. With atomic-scale knowledge, rational materials design becomes feasible. The second part explores methods for developing new PCMs with specific properties, such as accelerating crystallization at elevated temperatures while maintaining non-volatile characteristics at room temperature. High-throughput screening's role in discovering new phase change alloys is also discussed. In the third part, we examine multiscale and cross-scale simulations of PCM for various optical and electronic phase change applications. By computing the dielectric functions of PCM during the amorphous-to-crystalline transition, we can track changes in the refractive index and extinction coefficient across visible and infrared spectra over time. These DFT-computed parameters inform coarse-grained device simulations using finite-difference time-domain (FDTD) or finite element method (FEM). Based on these multiscale simulations, we offer optimization guidelines for non-volatile color display and photonic waveguide devices. The machine learning potentials address some performance gaps between the DFT/AIMD and FEM/FDTD calculations. Machine-learning-driven molecular dynamics (MLMD) simulations serve as cross-scale simulations, with recent developments including neural networks, graph convolutional neural networks, and Gaussian approximation potentials. We discuss the role of MLMD in enabling device-scale atomistic simulations, facilitating device design and optimization with atomic-scale information. Finally, we outline future opportunities and challenges in theoretical PCM research. With ongoing AI-driven fundamental research, we anticipate the commercialization of high-performance phase change memory, neuroinspired computing, and reconfigurable nanophotonic devices, which will, in turn, foster the development of more advanced theoretical tools for research.

Key words: phase-change memory material    first principles    high-throughput screening    multiscale simulation    machine-learning potential
收稿日期: 2024-06-03     
ZTFLH:  TB303  
基金资助:国家重点研发计划项目(2023YFB4404500);国家自然科学基金项目(62374131)
通讯作者: 张 伟,wzhang0@mail.xjtu.edu.cn,主要从事相变存储与类脑计算方面的研究
Corresponding author: ZHANG Wei, professor, Tel: (029)82664839, E-mail: wzhang0@mail.xjtu.edu.cn
作者简介: 沈雪阳,女,1998年生,博士生
图1  相变存储材料的商业化产品、基本工作原理及人工智能(AI)驱动的新材料研究[3,34,38]
图2  Ge2Sb2Te5相变合金非晶相的第一性原理分子动力学(AIMD)建模[53,56]
图3  包含1008个原子Ge1Sb2Te4模型在约600 K下的AIMD结晶化模拟[61]
图4  超快形核Sc0.2Sb2Te3相变合金的设计与器件验证[56]
图5  无序影响的Anderson绝缘硫族化合物高通量筛选及稳定性分析[90]
图6  面向Sb2Te1相变合金光波导器件应用的多尺度模拟[111]
图7  根据文献[37,97,118,119]得到的机器学习原子间势的拟合过程及方法
图8  基于图卷积网络的Sb-Te二元合金机器学习势[121]
图9  基于Gaussian近似机器学习势的Ge1Sb2Te4合金器件尺度的原子模拟[100]
1 Wuttig M, Yamada N. Phase-change materials for rewriteable data storage [J]. Nat. Mater., 2007, 6: 824
pmid: 17972937
2 Wong H S P, Raoux S, Kim S, et al. Phase change memory [J]. Proc. IEEE, 2010, 98: 2201
3 Zhang W, Mazzarello R, Wuttig M, et al. Designing crystallization in phase-change materials for universal memory and neuro-inspired computing [J]. Nat. Rev. Mater., 2019, 4: 150
doi: 10.1038/s41578-018-0076-x
4 Zhou W, Shen X Y, Yang X L, et al. Fabrication and integration of photonic devices for phase-change memory and neuromorphic computing [J]. Int. J. Extrem. Manuf., 2024, 6: 022001
5 Zhang Z H, Wang Z W, Shi T, et al. Memory materials and devices: From concept to application [J]. InfoMat, 2020, 2: 261
6 Kwon D H, Kim K M, Jang J H, et al. Atomic structure of conducting nanofilaments in TiO2 resistive switching memory [J]. Nat. Nanotechnol., 2010, 5: 148
7 Prezioso M, Merrikh-Bayat F, Hoskins B D, et al. Training and operation of an integrated neuromorphic network based on metal-oxide memristors [J]. Nature, 2015, 521: 61
8 Liu S, Lu N D, Zhao X L, et al. Eliminating negative-SET behavior by suppressing nanofilament overgrowth in cation-based memory [J]. Adv. Mater., 2016, 28: 10623
9 Mangin S, Ravelosona D, Katine J A, et al. Current-induced magnetization reversal in nanopillars with perpendicular anisotropy [J]. Nat. Mater., 2006, 5: 210
10 Torrejon J, Riou M, Araujo F A, et al. Neuromorphic computing with nanoscale spintronic oscillators [J]. Nature, 2017, 547: 428
11 Park B H, Kang B S, Bu S D, et al. Lanthanum-substituted bismuth titanate for use in non-volatile memories [J]. Nature, 1999, 401: 682
12 Chanthbouala A, Garcia V, Cherifi R O, et al. A ferroelectric memristor [J]. Nat. Mater., 2012, 11: 860
doi: 10.1038/nmat3415 pmid: 22983431
13 Wong H S P, Salahuddin S. Memory leads the way to better computing [J]. Nat. Nanotechnol., 2015, 10: 191
doi: 10.1038/nnano.2015.29 pmid: 25740127
14 Yang J J, Strukov D B, Stewart D R. Memristive devices for computing [J]. Nat. Nanotechnol., 2013, 8: 13
doi: 10.1038/nnano.2012.240 pmid: 23269430
15 Service R F. The brain chip [J]. Science, 2014, 345: 614
doi: 10.1126/science.345.6197.614 pmid: 25104367
16 Lanza M, Sebastian A, Lu W D, et al. Memristive technologies for data storage, computation, encryption, and radio-frequency communication [J]. Science, 2022, 376: eabj9979
17 Liu B, Wei T, Hu J, et al. Universal memory based on phase-change materials: From phase-change random access memory to optoelectronic hybrid storage [J]. Chin. Phys., 2021, 30B: 058504
18 Kau D, Tang S, Karpov I V, et al. A stackable cross point phase change memory [A]. Proceedings of 2009 IEEE International Electron Devices Meeting [C]. Baltimore: IEEE, 2009: 1
19 Cheng H Y, Carta F, Chien W C, et al. 3D cross-point phase-change memory for storage-class memory [J]. J. Phys., 2019, 52D: 473002
20 Li X, Chen H P, Xie C C, et al. Enhancing the performance of phase change memory for embedded applications [J]. Phys. Status Solidi (RRL), 2019, 13: 1800558
21 Arnaud F, Ferreira P, Piazza F, et al. High density embedded PCM cell in 28 nm FDSOI technology for automotive micro-controller applications [A]. Proceedings of 2020 IEEE International Electron Devices Meeting [C]. San Francisco: IEEE, 2020: 24.2.1
22 Cappelletti P, Annunziata R, Arnaud F, et al. Phase change memory for automotive grade embedded NVM applications [J]. J. Phys., 2020, 53D: 193002
23 Sebastian A, Le Gallo M, Khaddam-Aljameh R, et al. Memory devices and applications for in-memory computing [J]. Nat. Nanotechnol., 2020, 15: 529
doi: 10.1038/s41565-020-0655-z pmid: 32231270
24 Xu M, Mai X L, Lin J, et al. Recent advances on neuromorphic devices based on chalcogenide phase-change materials [J]. Adv. Funct. Mater., 2020, 30: 2003419
25 Shastri B J, Tait A N, Ferreira de Lima T, et al. Photonics for artificial intelligence and neuromorphic computing [J]. Nat. Photonics, 2021, 15: 102
26 Liu H L, Dong W L, Wang H, et al. Rewritable color nanoprints in antimony trisulfide films [J]. Sci. Adv., 2020, 6: eabb7171
27 Cheng Z G, Milne T, Salter P, et al. Antimony thin films demonstrate programmable optical nonlinearity [J]. Sci. Adv., 2021, 7: eabd7097
28 Ríos C, Stegmaier M, Hosseini P, et al. Integrated all-photonic non-volatile multi-level memory [J]. Nat. Photonics, 2015, 9: 725
doi: 10.1038/NPHOTON.2015.182
29 Cheng Z G, Ríos C, Pernice W H P, et al. On-chip photonic synapse [J]. Sci. Adv., 2017, 3: e1700160
30 Wuttig M, Bhaskaran H, Taubner T. Phase-change materials for non-volatile photonic applications [J]. Nat. Photonics, 2017, 11: 465
31 Wu C M, Yu H S, Lee S, et al. Programmable phase-change metasurfaces on waveguides for multimode photonic convolutional neural network [J]. Nat. Commun., 2021, 12: 96
doi: 10.1038/s41467-020-20365-z pmid: 33398011
32 Ríos C, Youngblood N, Cheng Z G, et al. In-memory computing on a photonic platform [J]. Sci. Adv., 2019, 5: eaau5759
33 Feldmann J, Youngblood N, Karpov M, et al. Parallel convolutional processing using an integrated photonic tensor core [J]. Nature, 2021, 589: 52
34 Zhang W, Mazzarello R, Ma E. Phase-change materials in electronics and photonics [J]. MRS Bull., 2019, 44: 686
doi: 10.1557/mrs.2019.201
35 Curtarolo S, Hart G L W, Nardelli M B, et al. The high-throughput highway to computational materials design [J]. Nat. Mater., 2013, 12: 191
doi: 10.1038/nmat3568 pmid: 23422720
36 Xie J X, Su Y J, Xue D Z, et al. Machine learning for materials research and development [J]. Acta Metall. Sin., 2021, 57: 1343
doi: 10.11900/0412.1961.2021.00357
36 谢建新, 宿彦京, 薛德祯 等. 机器学习在材料研发中的应用 [J]. 金属学报, 2021, 57: 1343
doi: 10.11900/0412.1961.2021.00357
37 Friederich P, Häse F, Proppe J, et al. Machine-learned potentials for next-generation matter simulations [J]. Nat. Mater., 2021, 20: 750
doi: 10.1038/s41563-020-0777-6 pmid: 34045696
38 Li H, Xu Y, Duan W H. Ab initio artificial intelligence: Future research of Materials Genome Initiative [J]. MGE Adv., 2023, 1: e16
39 Su Y J, Fu H D, Bai Y, et al. Progress in materials genome engineering in China [J]. Acta Metall. Sin., 2020, 56: 1313
doi: 10.11900/0412.1961.2020.00199
39 宿彦京, 付华栋, 白 洋 等. 中国材料基因工程研究进展 [J]. 金属学报, 2020, 56: 1313
doi: 10.11900/0412.1961.2020.00199
40 Xie J X. Prospects of materials genome engineering frontiers [J]. MGE Adv., 2023, 1: e17
41 Feng R, Zhang C, Gao M C, et al. High-throughput design of high-performance lightweight high-entropy alloys [J]. Nat. Commun., 2021, 12: 4329
doi: 10.1038/s41467-021-24523-9 pmid: 34267192
42 Rao Z Y, Tung P Y, Xie R W, et al. Machine learning-enabled high-entropy alloy discovery [J]. Science, 2022, 378: 78
doi: 10.1126/science.abo4940 pmid: 36201584
43 Xu Y F, Elcoro L, Song Z D, et al. High-throughput calculations of magnetic topological materials [J]. Nature, 2020, 586: 702
44 Choudhary K, Garrity K F, Jiang J, et al. Computational search for magnetic and non-magnetic 2D topological materials using unified spin-orbit spillage screening [J]. npj Comput. Mater., 2020, 6: 49
45 Gorai P, Stevanović V, Toberer E S. Computationally guided discovery of thermoelectric materials [J]. Nat. Rev. Mater., 2017, 2: 17053
46 Wang X D, Tan J L, Ouyang J, et al. Designing inorganic semiconductors with cold-rolling processability [J]. Adv. Sci., 2022, 9: 2203776
47 Gao Z Q, Wei T R, Deng T T, et al. High-throughput screening of 2D van der Waals crystals with plastic deformability [J]. Nat. Commun., 2022, 13: 7491
doi: 10.1038/s41467-022-35229-x pmid: 36470897
48 Jain A, Ong S P, Hautier G, et al. Commentary: The Materials Project: A materials genome approach to accelerating materials innovation [J]. APL Mater., 2013, 1: 011002
49 Hicks D, Toher C, Ford D C, et al. AFLOW-XtalFinder: A reliable choice to identify crystalline prototypes [J]. npj Comput. Mater., 2021, 7: 30
50 Wang G J, Li K Q, Peng L Y, et al. High-throughput automatic integrated material calculations and data management intelligent platform and the application in novel alloys [J]. Acta Metall. Sin., 2022, 58: 75
doi: 10.11900/0412.1961.2021.00041
50 王冠杰, 李开旗, 彭力宇 等. 高通量自动流程集成计算与数据管理智能平台及其在合金设计中的应用 [J]. 金属学报, 2022, 58: 75
doi: 10.11900/0412.1961.2021.00041
51 Yamada N, Ohno E, Akahira N, et al. High speed overwritable phase change optical disk material [J]. Jpn. J. Appl. Phys., 1987, 26(s4): 61
52 Yamada N, Ohno E, Nishiuchi K, et al. Rapid-phase transitions of GeTe-Sb2Te3 pseudobinary amorphous thin films for an optical disk memory [J]. J. Appl. Phys., 1991, 69: 2849
53 Caravati S, Bernasconi M, Kühne T D, et al. Coexistence of tetrahedral- and octahedral-like sites in amorphous phase change materials [J]. Appl. Phys. Lett., 2007, 91: 171906
54 Akola J, Jones R O. Structural phase transitions on the nanoscale: The crucial pattern in the phase-change materials Ge2Sb2Te5 and GeTe [J]. Phys. Rev., 2007, 76B: 235201
55 Kohara S, Kato K, Kimura S, et al. Structural basis for the fast phase change of Ge2Sb2Te5: Ring statistics analogy between the crystal and amorphous states [J]. Appl. Phys. Lett., 2006, 89: 201910
56 Rao F, Ding K Y, Zhou Y X, et al. Reducing the stochasticity of crystal nucleation to enable subnanosecond memory writing [J]. Science, 2017, 358: 1423
doi: 10.1126/science.aao3212 pmid: 29123020
57 Orava J, Greer A L, Gholipour B, et al. Characterization of supercooled liquid Ge2Sb2Te5 and its crystallization by ultrafast-heating calorimetry [J]. Nat. Mater., 2012, 11: 279
doi: 10.1038/nmat3275 pmid: 22426461
58 Jeyasingh R, Fong S W, Lee J, et al. Ultrafast characterization of phase-change material crystallization properties in the melt-quenched amorphous phase [J]. Nano Lett., 2014, 14: 3419
doi: 10.1021/nl500940z pmid: 24798660
59 Ronneberger I, Zhang W, Eshet H, et al. Crystallization properties of the Ge2Sb2Te5 phase-change compound from advanced simulations [J]. Adv. Funct. Mater., 2015, 25: 6407
60 Ronneberger I, Zhang W, Mazzarello R. Crystal growth of Ge2Sb2Te5 at high temperatures [J]. MRS Commun., 2018, 8: 1018
61 Xu Y Z, Zhou Y X, Wang X D, et al. Unraveling crystallization mechanisms and electronic structure of phase-change materials by large-scale ab initio simulations [J]. Adv. Mater., 2022, 34: 2109139
62 ten Wolde P R, Ruiz-Montero M J, Frenkel D. Simulation of homogeneous crystal nucleation close to coexistence [J]. Faraday Discuss., 1996, 104: 93
63 Bartók A P, Csányi G. Gaussian approximation potentials: A brief tutorial introduction [J]. Int. J. Quantum Chem., 2015, 115: 1051
64 Kalikka J, Akola J, Jones R O. Crystallization processes in the phase change material Ge2Sb2Te5: Unbiased density functional/molecular dynamics simulations [J]. Phys. Rev., 2016, 94B: 134105
65 Raty J Y, Zhang W, Luckas J, et al. Aging mechanisms in amorphous phase-change materials [J]. Nat. Commun., 2015, 6: 7467
doi: 10.1038/ncomms8467 pmid: 26105012
66 Li X B, Liu X Q, Liu X, et al. Role of electronic excitation in the amorphization of Ge-Sb-Te alloys [J]. Phys. Rev. Lett., 2011, 107: 015501
67 Zalden P, Quirin F, Schumacher M, et al. Femtosecond X-ray diffraction reveals a liquid-liquid phase transition in phase-change materials [J]. Science, 2019, 364: 1062
doi: 10.1126/science.aaw1773 pmid: 31197008
68 Kalikka J, Akola J, Larrucea J, et al. Nucleus-driven crystallization of amorphous Ge2Sb2Te5: A density functional study [J]. Phys. Rev., 2012, 86B: 144113
69 Kalikka J, Akola J, Jones R O. Simulation of crystallization in Ge2Sb2Te5: A memory effect in the canonical phase-change material [J]. Phys. Rev., 2014, 90B: 184109
70 Loke D, Lee T H, Wang W J, et al. Breaking the speed limits of phase-change memory [J]. Science, 2012, 336: 1566
doi: 10.1126/science.1221561 pmid: 22723419
71 Zhang B, Zhang W, Shen Z J, et al. Element-resolved atomic structure imaging of rocksalt Ge2Sb2Te5 phase-change material [J]. Appl. Phys. Lett., 2016, 108: 191902
72 Xu M, Zhang W, Mazzarello R, et al. Disorder control in crystalline GeSb2Te4 using high pressure [J]. Adv. Sci., 2015, 2: 1500117
73 Zheng Y H, Xia M J, Cheng Y, et al. Direct observation of metastable face-centered cubic Sb2Te3 crystal [J]. Nano Res., 2016, 9: 3453
74 Li Z, Si C, Zhou J, et al. Yttrium-doped Sb2Te3: A promising material for phase-change memory [J]. ACS Appl. Mater. Interfaces, 2016, 8: 26126
75 Liu B, Li K Q, Liu W L, et al. Multi-level phase-change memory with ultralow power consumption and resistance drift [J]. Sci. Bull., 2021, 66: 2217
doi: 10.1016/j.scib.2021.07.018 pmid: 36654113
76 Zhou Y X, Sun L, Zewdie G M, et al. Bonding similarities and differences between Y-Sb-Te and Sc-Sb-Te phase-change memory materials [J]. J. Mater. Chem., 2020, 8C: 3646
77 Chen B, Chen Y M, Ding K Y, et al. Kinetics features conducive to cache-type nonvolatile phase-change memory [J]. Chem. Mater., 2019, 31: 8794
doi: 10.1021/acs.chemmater.9b02598
78 Hu S W, Liu B, Li Z, et al. Identifying optimal dopants for Sb2Te3 phase-change material by high-throughput ab initio calculations with experiments [J]. Comput. Mater. Sci., 2019, 165: 51
79 Zewdie G M, Zhou Y X, Sun L, et al. Chemical design principles for cache-type Sc-Sb-Te phase-change memory materials [J]. Chem. Mater., 2019, 31: 4008
80 Wang X P, Li X B, Chen N K, et al. Time-dependent density-functional theory molecular-dynamics study on amorphization of Sc-Sb-Te alloy under optical excitation [J]. npj Comput. Mater., 2020, 6: 31
81 Qiao C, Guo Y R, Wang S Y, et al. Local structure origin of ultrafast crystallization driven by high-fidelity octahedral clusters in amorphous Sc0.2Sb2Te3 [J]. Appl. Phys. Lett., 2019, 114: 071901
82 Ding K Y, Chen B, Chen Y M, et al. Recipe for ultrafast and persistent phase-change memory materials [J]. NPG Asia Mater., 2020, 12: 63
83 Ding K Y, Wang J J, Zhou Y X, et al. Phase-change heterostructure enables ultralow noise and drift for memory operation [J]. Science, 2019, 366: 210
doi: 10.1126/science.aay0291 pmid: 31439757
84 Yang Z, Li B W, Wang J J, et al. Designing conductive-bridge phase-change memory to enable ultralow programming power [J]. Adv. Sci., 2022, 9: 2103478
85 Wang J J, Wang X Z, Cheng Y D, et al. Tailoring the oxygen concentration in Ge-Sb-O alloys to enable femtojoule-level phase-change memory operations [J]. Mater. Futures, 2022, 1: 045302
86 Liu Y T, Li X B, Zheng H, et al. High-throughput screening for phase-change memory materials [J]. Adv. Funct. Mater., 2021, 31: 2009803
87 Zhang W, Zhang H M, Sun S Y, et al. Metavalent bonding in layered phase-change memory materials [J]. Adv. Sci., 2023, 10: 2300901
88 Wuttig M, Deringer V L, Gonze X, et al. Incipient metals: Functional materials with a unique bonding mechanism [J]. Adv. Mater., 2018, 30: 1803777
89 Wuttig M, Schön C F, Lötfering J, et al. Revisiting the nature of chemical bonding in chalcogenides to explain and design their properties [J]. Adv. Mater., 2023, 35: 2208485
90 Xu Y Z, Wang X D, Zhang W, et al. Materials screening for disorder-controlled chalcogenide crystals for phase-change memory applications [J]. Adv. Mater., 2021, 33: 2006221
91 Zhang W, Thiess A, Zalden P, et al. Role of vacancies in metal-insulator transitions of crystalline phase-change materials [J]. Nat. Mater., 2012, 11: 952
doi: 10.1038/nmat3456 pmid: 23064498
92 Jiang T T, Wang X D, Wang J J, et al. In situ characterization of vacancy ordering in Ge-Sb-Te phase-change memory alloys [J]. Fundam. Res., 2022, DOI: 10.1016/j.fmre.2022.09.010
93 Esser M, Deringer V L, Wuttig M, et al. Orbital mixing in solids as a descriptor for materials mapping [J]. Solid State Commun., 2015, 203: 31
94 Wang Y Z, Ning J, Lu L, et al. A scheme for simulating multi-level phase change photonics materials [J]. npj Comput. Mater., 2021, 7: 183
95 Khan A I, Daus A, Islam R, et al. Ultralow-switching current density multilevel phase-change memory on a flexible substrate [J]. Science, 2021, 373: 1243
doi: 10.1126/science.abj1261 pmid: 34516795
96 Ghazi Sarwat S, Philip T M, Chen C T, et al. Projected mushroom type phase-change memory [J]. Adv. Funct. Mater., 2021, 31: 2106547
97 Deringer V L, Caro M A, Csányi G. Machine learning interatomic potentials as emerging tools for materials science [J]. Adv. Mater., 2019, 31: 1902765
98 Wang H, Zhang L F, Han J Q, et al. DeePMD-kit: A deep learning package for many-body potential energy representation and molecular dynamics [J]. Comput. Phys. Commun., 2018, 228: 178
99 Wang G J, Wang C R, Zhang X G, et al. Machine learning interatomic potential: Bridge the gap between small-scale models and realistic device-scale simulations [J]. iScience, 2024, 27: 109673
100 Zhou Y X, Zhang W, Ma E, et al. Device-scale atomistic modelling of phase-change memory materials [J]. Nat. Electron., 2023, 6: 746
101 Du K K, Li Q, Lyu Y B, et al. Control over emissivity of zero-static-power thermal emitters based on phase-changing material GST [J]. Light Sci. Appl., 2017, 6: e16194
102 Qu Y R, Li Q, Cai L, et al. Thermal camouflage based on the phase-changing material GST [J]. Light Sci. Appl., 2018, 7: 26
103 Li C L, Liu D J, Dai D X. Multimode silicon photonics [J]. Nanophotonics, 2019, 8: 227
doi: 10.1515/nanoph-2018-0161
104 Hosseini P, Wright C D, Bhaskaran H. An optoelectronic framework enabled by low-dimensional phase-change films [J]. Nature, 2014, 511: 206
105 Wang D N, Zhao L, Yu S Y, et al. Non-volatile tunable optics by design: From chalcogenide phase-change materials to device structures [J]. Mater. Today, 2023, 68: 334
106 Siegrist T, Jost P, Volker H, et al. Disorder-induced localization in crystalline phase-change materials [J]. Nat. Mater., 2011, 10: 202
doi: 10.1038/nmat2934 pmid: 21217692
107 Hu C Q, Yang Z B, Bi C B, et al. “All-crystalline” phase transition in nonmetal doped germanium-antimony-tellurium films for high-temperature non-volatile photonic applications [J]. Acta Mater., 2020, 188: 121
108 Matsunaga T, Umetani Y, Yamada N. Structural study of a Ag3.4In3.7Sb76.4Te16.5 quadruple compound utilized for phase-change optical disks [J]. Phys. Rev., 2001, 64B: 184116
109 Matsunaga T, Akola J, Kohara S, et al. From local structure to nanosecond recrystallization dynamics in AgInSbTe phase-change materials [J]. Nat. Mater., 2011, 10: 129
doi: 10.1038/nmat2931 pmid: 21217690
110 Zhang W, Ronneberger I, Zalden P, et al. How fragility makes phase-change data storage robust: Insights from ab initio simulations [J]. Sci. Rep., 2014, 4: 6529
doi: 10.1038/srep06529 pmid: 25284316
111 Wang X D, Zhou W, Zhang H M, et al. Multiscale simulations of growth-dominated Sb2Te phase-change material for non-volatile photonic applications [J]. npj Comput. Mater., 2023, 9: 136
112 Wang V, Xu N, Liu J C, et al. VASPKIT: A user-friendly interface facilitating high-throughput computing and analysis using VASP code [J]. Comput. Phys. Commun., 2021, 267: 108033
113 IncAnsys. Lumerical FDTD solutions [EB/OL].
114 Zheng Y H, Song W X, Song Z T, et al. A complicated route from disorder to order in antimony-tellurium binary phase change materials [J]. Adv. Sci., 2024, 11: 2301021
115 Belsky A J, Hellenbrandt M, Karen V L, et al. New developments in the Inorganic Crystal Structure Database (ICSD): Accessibility in support of materials research and design [J]. Acta Crystallogr., 2002, 58B: 364
116 Pickard C J, Needs R J. Ab initio random structure searching [J]. J. Phys.: Condens. Matter, 2011, 23: 053201
117 Thompson A P, Aktulga H M, Berger R, et al. LAMMPS—A flexible simulation tool for particle-based materials modeling at the atomic, meso, and continuum scales [J]. Comput. Phys. Commun., 2022, 271: 108171
118 Behler J. First principles neural network potentials for reactive simulations of large molecular and condensed systems [J]. Angew. Chem. Int. Ed., 2017, 56: 12828
doi: 10.1002/anie.201703114 pmid: 28520235
119 Xie T, Grossman J C. Crystal graph convolutional neural networks for an accurate and interpretable prediction of material properties [J]. Phys. Rev. Lett., 2018, 120: 145301
120 Behler J. Atom-centered symmetry functions for constructing high-dimensional neural network potentials [J]. J. Chem. Phys., 2011, 134: 074106
121 Wang G J, Sun Y Q, Zhou J, et al. PotentialMind: Graph convolutional machine learning potential for Sb-Te binary compounds of multiple stoichiometries [J]. J. Phys. Chem., 2023, 127C: 24724
122 Bartók A P, Payne M C, Kondor R, et al. Gaussian approximation potentials: The accuracy of quantum mechanics, without the electrons [J]. Phys. Rev. Lett., 2010, 104: 136403
123 Deringer V L, Bartók A P, Bernstein N, et al. Gaussian process regression for materials and molecules [J]. Chem. Rev., 2021, 121: 10073
doi: 10.1021/acs.chemrev.1c00022 pmid: 34398616
124 Sosso G C, Miceli G, Caravati S, et al. Neural network interatomic potential for the phase change material GeTe [J]. Phys. Rev., 2012, 85B: 174103
125 Sosso G C, Miceli G, Caravati S, et al. Fast crystallization of the phase change compound GeTe by large-scale molecular dynamics simulations [J]. J. Phys. Chem. Lett., 2013, 4: 4241
doi: 10.1021/jz402268v pmid: 26296172
126 Gabardi S, Baldi E, Bosoni E, et al. Atomistic simulations of the crystallization and aging of GeTe nanowires [J]. J. Phys. Chem., 2017, 121C: 23827
127 Abou El Kheir O, Bonati L, Parrinello M, et al. Unraveling the crystallization kinetics of the Ge2Sb2Te5 phase change compound with a machine-learned interatomic potential [J]. npj Comput. Mater., 2024, 10: 33
128 Dragoni D, Behler J, Bernasconi M. Mechanism of amorphous phase stabilization in ultrathin films of monoatomic phase change material [J]. Nanoscale, 2021, 13: 16146
129 Shi M C, Li J H, Tao M, et al. Artificial intelligence model for efficient simulation of monatomic phase change material antimony [J]. Mater. Sci. Semicond. Process., 2021, 136: 106146
130 Li K Q, Liu B, Zhou J, et al. Revealing the crystallization dynamics of Sb-Te phase change materials by large-scale simulations [J]. J. Mater. Chem., 2024, 12C: 3897
131 Mocanu F C, Konstantinou K, Lee T H, et al. Modeling the phase-change memory material, Ge2Sb2Te5, with a machine-learned interatomic potential [J]. J. Phys. Chem., 2018, 122B: 8998
132 Mocanu F C, Konstantinou K, Elliott S R. Quench-rate and size-dependent behaviour in glassy Ge2Sb2Te5 models simulated with a machine-learned Gaussian approximation potential [J]. J. Phys., 2020, 53D: 244002
133 Konstantinou K, Mocanu F C, Lee T H, et al. Revealing the intrinsic nature of the mid-gap defects in amorphous Ge2Sb2Te5 [J]. Nat. Commun., 2019, 10: 3065
134 Konstantinou K, Mocanu F C, Akola J, et al. Electric-field-induced annihilation of localized gap defect states in amorphous phase-change memory materials [J]. Acta Mater., 2022, 223: 117465
135 Zhou Y X, Zhang W, Ma E, et al. Device-scale atomistic modelling of phase-change memory materials [J]. Nat. Electron., 2023, 6: 746
136 Mo P H, Li C, Zhao D, et al. Accurate and efficient molecular dynamics based on machine learning and non von Neumann architecture [J]. npj Comput. Mater., 2022, 8: 107
137 Li H, Wang Z, Zou N L, et al. Deep-learning density functional theory Hamiltonian for efficient ab initio electronic-structure calculation [J]. Nat. Comput. Sci., 2022, 2: 367
138 Gong X X, Li H, Zou N L, et al. General framework for E(3)-equivariant neural network representation of density functional theory Hamiltonian [J]. Nat. Commun., 2023, 14: 2848
doi: 10.1038/s41467-023-38468-8 pmid: 37208320
[1] 王京京, 姚志浩, 张鹏, 赵杰, 张迈, 王蕾, 董建新, 陈迎. 镍基高温合金中S元素对基体与热障涂层界面稳定性的影响[J]. 金属学报, 2024, 60(9): 1250-1264.
[2] 周彦余, 李江旭, 刘晨, 赖俊文, 高强, 马会, 孙岩, 陈星秋. 金属间化合物Pt7Sb投影Berry相位与析氢催化关联的第一性原理计算[J]. 金属学报, 2024, 60(6): 837-847.
[3] 程坤, 陈树明, 曹烁, 刘建荣, 马英杰, 范群波, 程兴旺, 杨锐, 胡青苗. 第一性原理研究钛合金中的沉淀强化[J]. 金属学报, 2024, 60(4): 537-547.
[4] 文通其, 刘怀忆, 龚小国, 叶贝琳, 刘思宇, 李卓远. 深度势能方法在材料科学中的应用[J]. 金属学报, 2024, 60(10): 1299-1311.
[5] 赵晋彬, 王建韬, 何东昌, 李俊林, 孙岩, 陈星秋, 刘培涛. 氢化物超导体临界转变温度的机器学习模型[J]. 金属学报, 2024, 60(10): 1418-1428.
[6] 王福容, 张永梅, 柏国宁, 郭庆伟, 赵宇宏. Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023, 59(6): 812-820.
[7] 李昕, 江河, 姚志浩, 董建新. O原子对高温合金基体Ni、Co和NiCr晶界作用的理论计算分析[J]. 金属学报, 2023, 59(2): 309-318.
[8] 任师浩, 刘永利, 孟凡顺, 祁阳. 应变工程中Bi(111)薄膜的半导体-半金属转变及其机理[J]. 金属学报, 2022, 58(7): 911-920.
[9] 李亚敏, 张瑶瑶, 赵旺, 周生睿, 刘洪军. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究[J]. 金属学报, 2022, 58(2): 241-249.
[10] 王硕, 王俊升. Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究[J]. 金属学报, 2022, 58(10): 1325-1333.
[11] 王冠杰, 李开旗, 彭力宇, 张壹铭, 周健, 孙志梅. 高通量自动流程集成计算与数据管理智能平台及其在合金设计中的应用[J]. 金属学报, 2022, 58(1): 75-88.
[12] 毛斐, 吕皓, 唐法威, 郭凯, 刘东, 宋晓艳. Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算[J]. 金属学报, 2021, 57(7): 948-958.
[13] 崔洋, 李寿航, 应韬, 鲍华, 曾小勤. 基于第一性原理的金属导热性能研究[J]. 金属学报, 2021, 57(3): 375-384.
[14] 张海军, 邱实, 孙志梅, 胡青苗, 杨锐. 无序β-Ti1-xNbx合金自由能及弹性性质的第一性原理计算:特殊准无序结构和相干势近似的比较[J]. 金属学报, 2020, 56(9): 1304-1312.
[15] 盖逸冰, 唐法威, 侯超, 吕皓, 宋晓艳. 合金化元素对W-Cu体系多类界面特征影响的第一性原理计算[J]. 金属学报, 2020, 56(7): 1036-1046.