| Ce对75Cr1钢洁净度、组织与耐点蚀性能的影响 |
孟泽1, 李光强1,2, 李腾飞3, 郑庆4, 曾斌4, 刘昱1( ) |
1.武汉科技大学 省部共建耐火材料与冶金国家重点实验室 武汉 430081 2.武汉科技大学 钢铁冶金及资源利用省部共建教育部重点实验室 武汉 430081 3.武汉科技大学 钢铁冶金新工艺湖北省重点实验室 武汉 430081 4.涟源钢铁有限公司 娄底 417009 |
|
| Effect of Ce on Cleanliness, Microstructure, and Pitting Corrosion Resistance of 75Cr1 Steel |
MENG Ze1, LI Guangqiang1,2, LI Tengfei3, ZHENG Qing4, ZENG Bin4, LIU Yu1( ) |
1.State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China 2.Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, China 3.Hubei Provincial Key Laboratory for New Processes of Ironmaking and Steelmaking, Wuhan University of Science and Technology, Wuhan 430081, China 4.Lianyuan Iron and Steel Co. Ltd., Loudi 417009, China |
引用本文:
孟泽, 李光强, 李腾飞, 郑庆, 曾斌, 刘昱. Ce对75Cr1钢洁净度、组织与耐点蚀性能的影响[J]. 金属学报, 2024, 60(9): 1229-1238.
Ze MENG,
Guangqiang LI,
Tengfei LI,
Qing ZHENG,
Bin ZENG,
Yu LIU.
Effect of Ce on Cleanliness, Microstructure, and Pitting Corrosion Resistance of 75Cr1 Steel[J]. Acta Metall Sin, 2024, 60(9): 1229-1238.
| 1 |
Liu D, Song Y Q, Zhang X, et al. Effect of La on microstructure and mechanical properties of 75Cr1 saw blade steel [J]. Hot Work. Technol., 2021, 50(14): 51
|
| 1 |
刘 笛, 宋艳青, 张 鑫 等. La对75Cr1锯片用钢热轧板组织和力学性能的影响 [J]. 热加工工艺, 2021, 50(14): 51
|
| 2 |
Guan J, Wang L Q, Zhang C W, et al. Effects of non-metallic inclusions on the crack propagation in bearing steel [J]. Tribol. Int., 2017, 106: 123
|
| 3 |
Zhu J, Zhang Z H, Xie J X. Plastic deformation behavior and fracture mechanism of rare earth H13 steel based on in situ TEM tensile study [J]. Acta Metall. Sin., 2020, 56: 1592
doi: 10.11900/0412.1961.2020.00141
|
| 3 |
朱 健, 张志豪, 谢建新. 基于原位TEM拉伸的稀土H13钢塑性形变行为和断裂机制 [J]. 金属学报, 2020, 56: 1592
|
| 4 |
Wang L M. Application prospects and behavior of RE in new generation high strength steels with superior toughness [J]. J. Chin. Rare Earth Soc., 2004, 22: 48
|
| 4 |
王龙妹. 稀土元素在新一代高强韧钢中的作用和应用前景 [J]. 中国稀土学报, 2004, 22: 48
|
| 5 |
Yan C L, Wang F M, Wei L J, et al. Improvement of lanthanum on impact toughness of 34CrNi3Mo steel containing Sn, Sb residual elements [J]. J. Univ. Sci. Technol. Beijing, 2004, 26: 277
|
| 5 |
严春莲, 王福明, 魏利娟 等. 残余元素锡、锑对34CrNi3Mo钢冲击韧性的影响及稀土镧的改善作用 [J]. 北京科技大学学报, 2004, 26: 277
|
| 6 |
Yang J C, Wang J, Ren L, et al. Effect of Ce on microstructure and impact properties of S32550 duplex stainless steel [J]. Iron Steel, 2020, 55(1): 86
|
| 6 |
杨吉春, 王 军, 任 磊 等. 铈对S32550双相不锈钢微观组织及冲击性能的影响 [J]. 钢铁, 2020, 55(1): 86
doi: 10.13228/j.boyuan.issn0449-749x.20190165
|
| 7 |
Zhou W J, Zhu J, Zhang Z H. Austenite grain growth behaviors of La-microalloyed H13 steel and its effect on mechanical properties [J]. Metall. Mater. Trans., 2020, 51A: 4662
|
| 8 |
Lu B, Chen F R, Zhi J G, et al. Enhanced welding properties of high strength steel via rare earth oxide metallurgy technology [J]. Acta Metall. Sin., 2020, 56: 1206
doi: 10.11900/0412.1961.2020.00052
|
| 8 |
陆 斌, 陈芙蓉, 智建国 等. 应用稀土氧化物冶金技术改善高强钢焊接性能 [J]. 金属学报, 2020, 56: 1206
|
| 9 |
Yang Q X, Liao B, Liu L G, et al. Mechanism of cracking resistance improved by rare earth oxide of hardfacing specimens of medium-high carbon steel [J]. J. Chin. Rare Earth Soc., 2006, 24: 721
|
| 9 |
杨庆祥, 廖 波, 刘利刚 等. 稀土氧化物提高中高碳钢堆焊试样抗开裂性机制的研究 [J]. 中国稀土学报, 2006, 24: 721
|
| 10 |
Ke W. China Corrosion Investigation Report [M]. Beijing: Chemical Industry Press, 2003: 55
|
| 10 |
柯 伟. 中国腐蚀调查报告 [M]. 北京: 化学工业出版社, 2003: 55
|
| 11 |
Deyab M A. Electrochemical investigations on pitting corrosion inhibition of mild steel by provitamin B5 in circulating cooling water [J]. Electrochim. Acta, 2016, 202: 262
|
| 12 |
Frankel G S, Sridhar N. Understanding localized corrosion [J]. Mater. Today, 2008, 11: 38
|
| 13 |
Rodrigues C A D, Pagotto J F, Motheo A J, et al. The effect of titanium on pitting corrosion resistance of welded supermartensitic stainless steel [J]. Corros. Eng. Sci. Technol., 2017, 52: 141
|
| 14 |
Shi W N, Yang S F, Dong A P, et al. Understanding the corrosion mechanism of spring steel induced by MnS inclusions with different sizes [J]. JOM, 2018, 70: 2513
|
| 15 |
Yang Z X, Kan B, Li J X, et al. Pitting initiation and propagation of X70 pipeline steel exposed to chloride-containing environments [J]. Materials, 2017, 10: 1076
|
| 16 |
Jin T Y, Cheng Y. In situ characterization by localized electrochemical impedance spectroscopy of the electrochemical activity of microscopic inclusions in an X100 steel [J]. Corros. Sci., 2011, 53: 850
|
| 17 |
Wang Y F, Cheng G X, Li Y. Observation of the pitting corrosion and uniform corrosion for X80 steel in 3.5 wt.% NaCl solutions using in-situ and 3-D measuring microscope [J]. Corros. Sci., 2016, 111: 508
|
| 18 |
Suter T, Böhni H. A new microelectrochemical method to study pit initiation on stainless steels [J]. Electrochim. Acta, 1997, 42: 3275
|
| 19 |
Sun Y T, Li Y W, Wu W B, et al. Effect of inclusions on pitting corrosion of C70S6 non-quenched and tempered steel doped with Ca and Mg [J]. Acta Metall. Sin., 2022, 58: 895
doi: 10.11900/0412.1961.2021.00362
|
| 19 |
孙阳庭, 李一唯, 吴文博 等. Ca、Mg掺杂下夹杂物对C70S6非调质钢点蚀行为的影响 [J]. 金属学报, 2022, 58: 895
doi: 10.11900/0412.1961.2021.00362
|
| 20 |
Zheng J C, Hu X J, Pan C, et al. Effects of inclusions on the resistance to pitting corrosion of S32205 duplex stainless steel [J]. Mater. Corros., 2018, 69: 572
|
| 21 |
Imashuku S, Wagatsuma K. Cathodoluminescence analysis of nonmetallic inclusions in steel deoxidized and desulfurized by rare-earth metals (La, Ce, Nd) [J]. Metall. Mater. Trans., 2020, 51B: 79
|
| 22 |
Liu X J, Yang J C, Ding H F, et al. Study on behavior of rare earth cerium modifying inclusions in clean steel [J]. Hot Work. Technol., 2016, 45(9): 92
|
| 22 |
刘香军, 杨吉春, 丁海峰 等. 洁净钢中稀土铈变质夹杂物行为研究 [J]. 热加工工艺, 2016, 45(9): 92
|
| 23 |
Gao S, Wang M, Guo J L, et al. Characterization transformation of inclusions using rare earth Ce treatment on Al-killed titanium alloyed interstitial free steel [J]. Steel Res. Int., 2019, 90: 1900194
|
| 24 |
Huang Y, Cheng G G, Xie Y. Modification mechanism of cerium on the inclusions in drill steel [J]. Acta Metall. Sin., 2018, 54: 1253
doi: 10.11900/0412.1961.2018.00079
|
| 24 |
黄 宇, 成国光, 谢 有. 稀土Ce对钎具钢中夹杂物的改质机理研究 [J]. 金属学报, 2018, 54: 1253
|
| 25 |
Song M M, Song B, Xin W B, et al. Effects of rare earth addition on microstructure of C-Mn steel [J]. Ironmak. Steelmak., 2015, 42: 594
|
| 26 |
Li M, Li H Z, Wang J J, et al. Effect of Ce on the microstructure, high-temperature tensile properties, and fracture mode of strip casting non-oriented 6.5%Si electrical steel [J]. Acta Metall. Sin., 2022, 58: 637
doi: 10.11900/0412.1961.2021.00115
|
| 26 |
李 民, 李昊泽, 王继杰 等. 稀土Ce对薄带连铸无取向6.5%Si钢组织、高温拉伸性能和断裂模式的影响 [J]. 金属学报, 2022, 58: 637
|
| 27 |
Yang Q X, Gao Y W, Liao B, et al. Discussion of inclusions as heterogeneous nuclei of primary austenite of medium-high carbon steel during hardfacing [J]. J. Chin. Rare Earths Soc., 2000, 18: 138
|
| 27 |
杨庆祥, 高聿为, 廖 波 等. 夹杂物在中高碳钢堆焊金属中成为初生奥氏体非均质形核核心的探讨 [J]. 中国稀土学报, 2000, 18: 138
|
| 28 |
Liu C, Revilla R I, Liu Z Y, et al. Effect of inclusions modified by rare earth elements (Ce, La) on localized marine corrosion in Q460NH weathering steel [J]. Corros. Sci., 2017, 129: 82
|
| 29 |
Nishimoto M, Muto I, Sugawara Y, et al. Micro-electrochemical properties of CeS inclusions in stainless steel and inhibiting effects of Ce3+ ions on pitting [J]. J. Electrochem. Soc., 2017, 164: C901
|
| 30 |
Nishimoto M, Muto I, Sugawara Y, et al. Cerium addition to CaS inclusions in stainless steel: Insolubilizing water-soluble inclusions and improving pitting corrosion resistance [J]. Corros. Sci., 2021, 180: 109222
|
| 31 |
Liu H L. Effect of rare earth on microstructure and property of X80 pipeline Steel [D]. Shenyang: Northeastern University, 2011
|
| 31 |
刘宏亮. 稀土对X80管线钢组织和性能的影响 [D]. 沈阳: 东北大学, 2011
|
| 32 |
Shi C B, Chen X C, Guo H J, et al. Assessment of oxygen control and its effect on inclusion characteristics during electroslag remelting of die steel [J]. Steel Res. Int., 2012, 83: 472
|
| 33 |
Liu Y, Zhang Z, Li G Q, et al. Evolution of desulfurization and characterization of inclusions in dual alloy ingot processed by electroslag remelting [J]. Steel Res. Int., 2017, 88: 1700058
|
| 34 |
Adabavazeh Z, Hwang W S, Su Y H. Effect of adding cerium on microstructure and morphology of Ce-based inclusions formed in low-carbon steel [J]. Sci. Rep., 2017, 7: 46503
doi: 10.1038/srep46503
pmid: 28485376
|
| 35 |
Hino M, Ito K. Thermodynamic Data for Steelmaking [M]. Sendai, Japan: Tohuku University Press, 2010: 1
|
| 36 |
Huang Y, Cheng G G, Li S J, et al. Precipitation mechanism and thermal stability of primary carbide in Ce microalloyed H13 steel [J]. Acta Metall. Sin., 2019, 55: 1487
doi: 10.11900/0412.1961.2019.00147
|
| 36 |
黄 宇, 成国光, 李世健 等. Ce微合金化H13钢中一次碳化物的析出机理及热稳定性研究 [J]. 金属学报, 2019, 55: 1487
|
| 37 |
Guo M X, Suito H. Dispersion of primary inclusions of Ce2O3 and CeS in Fe-0.20 mass%C-0.02 mass%P alloy [J]. ISIJ Int., 1999, 39: 678
|
| 38 |
Wang Y G, Liu C J. Agglomeration characteristics of various inclusions in Al-killed molten steel containing rare earth element [J]. Metall. Mater. Trans., 2020, 51B: 2585
|
| 39 |
Vahed A, Kay D A R. Thermodynamics of rare earths in steelmaking [J]. Metall. Trans., 1976, 7B: 375
|
| 40 |
Bao D H, Cheng G G, Huang Y, et al. Refinement of solidification structure of H13 steel by rare earth sulfide [J]. Steel Res. Int., 2022, 93: 2100304
|
| 41 |
Liu Y Q, Wang L J, Chou K C. Effects of cerium on resistance to pitting corrosion of spring steel used in fasteners of high-speed railway [J]. Steel Res. Int., 2014, 85: 1510
|
| 42 |
Cao Y X. Effect of rare earth Ce on the corrosion resistance and weldability of high-strength low-alloy steels [D]. Wuhan: Wuhan University of Science and Technology, 2021
|
| 42 |
曹羽鑫. 稀土Ce对低合金高强钢耐点蚀性能和焊接性能的影响 [D]. 武汉: 武汉科技大学, 2021
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|