| 亚共晶Al-Si合金中微量元素La变质共晶Si的关键影响因素 |
张丽丽1, 吉宗威2, 赵九洲1( ), 何杰1, 江鸿翔1 |
1.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2.南方科技大学 材料科学与工程学院 深圳 518055 |
|
| Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La |
ZHANG Lili1, JI Zongwei2, ZHAO Jiuzhou1( ), HE Jie1, JIANG Hongxiang1 |
1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2.Department of Materials Science and Engineering, Southern University of Science and Technology, Shenzhen 518055, China |
引用本文:
张丽丽, 吉宗威, 赵九洲, 何杰, 江鸿翔. 亚共晶Al-Si合金中微量元素La变质共晶Si的关键影响因素[J]. 金属学报, 2023, 59(11): 1541-1546.
Lili ZHANG,
Zongwei JI,
Jiuzhou ZHAO,
Jie HE,
Hongxiang JIANG.
Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. Acta Metall Sin, 2023, 59(11): 1541-1546.
| 1 |
Liu X R, Zhang Y D, Beausir B, et al. Twin-controlled growth of eutectic Si in unmodified and Sr-modified Al-12.7%Si alloys investigated by SEM/EBSD [J]. Acta Mater., 2015, 97: 338
doi: 10.1016/j.actamat.2015.06.041
|
| 2 |
Tsai Y C, Chou C Y, Lee S L, et al. Effect of trace La addition on the microstructures and mechanical properties of A356 (Al-7Si-0.35Mg) aluminum alloys [J]. J. Alloys Compd., 2009, 487: 157
doi: 10.1016/j.jallcom.2009.07.183
|
| 3 |
Jiang W M, Fan Z T, Dai Y C, et al. Effects of rare earth elements addition on microstructures, tensile properties and fractography of A357 alloy [J]. Mater. Sci. Eng., 2014, A597: 237
|
| 4 |
Jung J G, Ahn T Y, Cho Y H, et al. Synergistic effect of ultrasonic melt treatment and fast cooling on the refinement of primary Si in a hypereutectic Al-Si alloy [J]. Acta Mater., 2018, 144: 31
doi: 10.1016/j.actamat.2017.10.039
|
| 5 |
Makhlouf M M, Guthy H V. The aluminum-silicon eutectic reaction: Mechanisms and crystallography [J]. J. Light Met., 2001, 1: 199
doi: 10.1016/S1471-5317(02)00003-2
|
| 6 |
Nogita K, McDonald S D, Dahle A K. Eutectic modification of Al-Si alloys with rare earth metals [J]. Mater. Trans., 2004, 45: 323
doi: 10.2320/matertrans.45.323
|
| 7 |
Pourbahari B, Emamy M. Effects of La intermetallics on the structure and tensile properties of thin section gravity die-cast A357 Al alloy [J]. Mater. Des., 2016, 94: 111
doi: 10.1016/j.matdes.2016.01.039
|
| 8 |
Li B. Modification evolution of eutectic silicon in AlSi7Mg alloy and micro-mechanism [D]. Harbin: Harbin Institute of Technology, 2011
|
| 8 |
李 豹. AlSi7Mg合金共晶硅变质规律及其微观机制 [D]. 哈尔滨: 哈尔滨工业大学, 2011
|
| 9 |
Dong G M, Sun G X, Liao H C. Modification of eutectic silicon in Al-Si cast alloys [J]. Foundry, 2005, 54: 1
|
| 9 |
董光明, 孙国雄, 廖恒成. 共晶硅的变质 [J]. 铸造, 2005, 54: 1
|
| 10 |
Pan F S. Current status and prospects of rare earth aluminum alloy [J]. Mater. Rep., 1990, (1): 21
|
| 10 |
潘复生. 我国稀土铝合金的现状和展望 [J]. 材料导报, 1990, (1): 21
|
| 11 |
Jiang H X, Li S X, Zheng Q J, et al. Effect of minor lanthanum on the microstructures, tensile and electrical properties of Al-Fe alloys [J]. Mater. Des., 2020, 195: 108991
doi: 10.1016/j.matdes.2020.108991
|
| 12 |
Zhang L L, Zheng Q J, Jiang H X, et al. Effect of La addition on microstructure evolution of hypoeutectic Al-6Si alloys [J]. J. Mater. Sci., 2020, 55: 7546
doi: 10.1007/s10853-020-04522-9
|
| 13 |
Jiang H X, Li S X, Zhang L L, et al. The influence of rare earth element lanthanum on the microstructures and properties of as-cast 8176 (Al-0.5Fe) aluminum alloy [J]. J. Alloys Compd., 2021, 859: 157804
doi: 10.1016/j.jallcom.2020.157804
|
| 14 |
Zheng Q J, Zhang L L, Jiang H X, et al. Effect mechanisms of micro-alloying element La on microstructure and mechanical properties of hypoeutectic Al-Si alloys [J]. J. Mater. Sci. Technol., 2020, 47: 142
doi: 10.1016/j.jmst.2019.12.021
|
| 15 |
Zheng Q J, Ye Z F, Jiang H X, et al. Effect of micro-alloying element La on solidification microstructure and mechanical properties of hypoeutectic Al-Si alloys [J]. Acta Metall. Sin., 2021, 57: 103
doi: 10.11900/0412.1961.2020.00158
|
| 15 |
郑秋菊, 叶中飞, 江鸿翔 等. 微合金化元素La对亚共晶Al-Si合金凝固组织与力学性能的影响 [J]. 金属学报, 2021, 57: 103
doi: 10.11900/0412.1961.2020.00158
|
| 16 |
StJohn D H, Qian M, Easton M A, et al. The interdependence theory: The relationship between grain formation and nucleant selection [J]. Acta Mater., 2011, 59: 4907
doi: 10.1016/j.actamat.2011.04.035
|
| 17 |
Balluffi R W, Allen S M, Carter W C. Kinetics of Materials [M]. Hoboken: Wiley-Interscience, 2005: 543
|
| 18 |
Fan T X, Yang G, Zhang D. Thermodynamic effect of alloying addition on in-situ reinforced TiB2/Al composites [J]. Metall. Mater. Trans., 2005, 36A: 225
|
| 19 |
Zhang L L, Zheng Q J, Jiang H X, et al. Interfacial energy between Al melt and TiB2 particles and efficiency of TiB2 particles to nucleate α-Al [J]. Scr. Mater., 2019, 160: 25
doi: 10.1016/j.scriptamat.2018.09.042
|
| 20 |
Niessen A K, de Boer F R, Boom R, et al. Model predictions for the enthalpy of formation of transition metal alloys II [J]. Calphad, 1983, 7: 51
doi: 10.1016/0364-5916(83)90030-5
|
| 21 |
Miedema A R, de Châtel P F, de Boer F R. Cohesion in alloys—Fundamentals of a semi-empirical model [J]. Physica B + C, 1980, 100: 1
doi: 10.1016/0378-4363(80)90054-6
|
| 22 |
Ji Z W, Hu C H, Wang D H, et al. Mechanical properties and chemical bonding of the Os-B system: A first-principles study [J]. Acta Mater., 2012, 60: 4208
doi: 10.1016/j.actamat.2012.04.015
|
| 23 |
Kaptay G. Modelling interfacial energies in metallic systems [J]. Mater. Sci. Forum, 2005, 473-474: 1
doi: 10.4028/www.scientific.net/MSF.473-474
|
| 24 |
Dinsdale A T. SGTE data for pure elements [J]. Calphad, 1991, 15: 317
doi: 10.1016/0364-5916(91)90030-N
|
| 25 |
Hosseinifar M, Malakhov D V. The sequence of intermetallics formation during the solidification of an Al-Mg-Si alloy containing La [J]. Metall. Mater. Trans., 2011, 42A: 825
|
| 26 |
Wang T M, Zhao Y F, Chen Z N, et al. Combining effects of TiB2 and La on the aging behavior of A356 alloy [J]. Mater. Sci. Eng., 2015, A644: 425
|
| 27 |
Alkahtani S A, Elgallad E M, Tash M M, et al. Effect of rare Earth metals on the microstructure of Al-Si based alloys [J]. Materials, 2016, 9: 45
doi: 10.3390/ma9010045
|
| 28 |
Elgallad E M, Ibrahim M F, Doty H W, et al. Microstructural characterisation of Al-Si cast alloys containing rare earth additions [J]. Philos. Mag., 2018, 98: 1337
doi: 10.1080/14786435.2018.1435917
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|