| 模拟近海大气环境下结构钢锈蚀表面特征随机模型 |
王友德1,2( ), 周晓东1,2, 马蕊2,3, 徐善华1,2 |
1.西安建筑科技大学 省部共建西部绿色建筑国家重点实验室 西安 710055 2.西安建筑科技大学 工程结构安全与耐久重点实验室 西安 710055 3.西安交通大学 第一附属医院 西安 710061 |
|
| Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere |
WANG Youde1,2( ), ZHOU Xiaodong1,2, MA Rui2,3, XU Shanhua1,2 |
1.State Key Laboratory of Green Building in Western China, Xi'an University of Architecture and Technology, Xi'an 710055, China 2.Key Lab of Engineering Structural Safety and Durability, Xi'an University of Architecture and Technology, Xi'an 710055, China 3.First Affiliated Hospital, Xi'an Jiaotong University, Xi'an 710061, China |
引用本文:
王友德, 周晓东, 马蕊, 徐善华. 模拟近海大气环境下结构钢锈蚀表面特征随机模型[J]. 金属学报, 2021, 57(6): 811-821.
Youde WANG,
Xiaodong ZHOU,
Rui MA,
Shanhua XU.
Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere[J]. Acta Metall Sin, 2021, 57(6): 811-821.
| 1 |
Hui Y L, Lin Z S, Li R. Experimental study and analysis on the property of corroded rebar [J]. Ind. Constr., 1997, 27(6): 10
|
| 1 |
惠云玲, 林志伸, 李 荣. 锈蚀钢筋性能试验研究分析 [J]. 工业建筑, 1997, 27(6): 10
|
| 2 |
Schumacher M M. Seawater Corrosion Handbook [M]. New Jersey: Noyes Data Corporation, 1979: 87
|
| 3 |
Garbatov Y, Soares C G, Wang G. Non-linear time dependent corrosion wastage of deck plates of ballast and cargo tanks of tankers [J]. J. Offshore Mech. Arct. Eng., 2007, 129: 48
|
| 4 |
Melchers R E. Corrosion uncertainty modelling for steel structures [J]. J. Constr. Steel Res., 1999, 52: 3
|
| 5 |
Mu X, Wei J, Dong J H, et al. Electrochemical study on corrosion behaviors of mild steel in a simulated tidal zone [J]. Acta Metall. Sin., 2012, 48: 420
|
| 5 |
穆 鑫, 魏 洁, 董俊华等. 低碳钢在模拟海洋潮差区的腐蚀行为的电化学研究 [J]. 金属学报, 2012, 48: 420
|
| 6 |
Chen L. Study on the deterioration properties of corroded steel [D]. Xi'an: Xi'an University of Architecture & Technology, 2010
|
| 6 |
陈 露. 腐蚀后钢材材料性能退化研究 [D]. 西安: 西安建筑科技大学, 2010
|
| 7 |
Xu S H, Wang Y D. Estimating the effects of corrosion pits on the fatigue life of steel plate based on the 3D profile [J]. Int. J. Fatigue, 2015, 72: 27
|
| 8 |
Melchers R E. Pitting corrosion of mild steel in marine immersion environment-part 1: Maximum pit depth [J]. Corrosion, 2004, 60: 824
|
| 9 |
Melchers R E. Pitting corrosion of mild steel in marine immersion environment-part 2: Variability of maximum pit depth [J]. Corrosion, 2004, 60: 937
|
| 10 |
Wang Y W. Ultimate strength of ship structures with corrosion wastage [D]. Shanghai: Shanghai Jiao Tong University, 2008
|
| 10 |
王燕舞. 考虑腐蚀影响船舶结构极限强度研究 [D]. 上海: 上海交通大学, 2008
|
| 11 |
Wang Y W, Huang X P, Cui W C. Pitting corrosion model of mild and low-alloy steel in marine environment-part 1: Maximum pit depth [J]. J. Ship Mech., 2007, 11: 577
|
| 11 |
王燕舞, 黄小平, 崔维成. 船舶结构钢海洋环境点蚀模型研究之一: 最大点蚀深度时变模型 [J]. 船舶力学, 2007, 11: 577
|
| 12 |
Silva J E, Garbatov Y, Soares C G. Ultimate strength assessment of rectangular steel plates subjected to a random localised corrosion degradation [J]. Eng. Struct., 2013, 52: 295
|
| 13 |
Qiu B. The study on surface characteristics and eccentric compressive load-capacity of corroded H-shape steel members at neutral salt fog environment [D]. Xi'an: Xi'an University of Architecture & Technology, 2014
|
| 13 |
邱 斌. 中性盐雾环境下锈蚀H型钢表面特征及偏压承载性能研究 [D]. 西安: 西安建筑科技大学, 2014
|
| 14 |
Wang R H, Shenoi R A, Sobey A. Ultimate strength assessment of plated steel structures with random pitting corrosion damage [J]. J. Constr. Steel Res., 2018, 143: 331
|
| 15 |
Wang Y D, Xu S H, Li H, et al. Surface characteristics and stochastic model of corroded structural steel under general atmospheric environment [J]. Acta Metall. Sin., 2020, 56: 148
|
| 15 |
王友德, 徐善华, 李 晗等. 一般大气环境下锈蚀结构钢表面特征与随机模型 [J]. 金属学报, 2020, 56: 148
|
| 16 |
He J X, Qin X Z, Yi P, et al. Corrosion exposure study on Q235 steel in marine atmospheric [J]. Surf. Technol., 2006, 35(4): 21
|
| 16 |
何建新, 秦晓洲, 易 平等. Q235钢海洋大气腐蚀暴露试验研究 [J]. 表面技术, 2006, 35(4): 21
|
| 17 |
Liang C F, Hou W T. Sixteen-year atmospheric corrosion exposure study of steels [J]. J. Chin. Soc. Corros. Prot., 2005, 25: 1
|
| 17 |
梁彩凤, 侯文泰. 碳钢、低合金钢16年大气暴露腐蚀研究 [J]. 中国腐蚀与防护学报, 2005, 25: 1
|
| 18 |
Melchers R E. Probabilistic models for corrosion in structural reliability assessment [J]. J. Offshore Mech. Arct., 2003, 125: 272
|
| 19 |
Wang Y K, Wharton J A, Shenoi R A. Ultimate strength analysis of aged steel-plated structures exposed to marine corrosion damage: A review [J]. Corros. Sci., 2014, 86: 42
|
| 20 |
Melchers R E, Ahammed M, Jeffrey R, et al. Statistical characterization of surfaces of corroded steel plates [J]. Mar. Struct., 2010, 23: 274
|
| 21 |
Li C G. Characterization of 3D surface micro-topography by 2D power spectrum [J]. Acta Metrol. Sin., 2004, 25: 11
|
| 21 |
李成贵. 三维表面微观形貌的二维功率谱表征 [J]. 计量学报, 2004, 25: 11
|
| 22 |
Liang S X, Sun W L, Li J. Simulation of multi-dimensional random fields by stochastic harmonic functions [J]. J. Tongji Univ. (Nat. Sci.), 2012, 40: 965
|
| 22 |
梁诗雪, 孙伟玲, 李 杰. 随机场的随机谐和函数表达 [J]. 同济大学学报(自然科学版), 2012, 40: 965
|
| 23 |
Wang Y D, Xu S H, Wang H, et al. Predicting the residual strength and deformability of corroded steel plate based on the corrosion morphology [J]. Constr. Build. Mater., 2017, 152: 777
|
| 24 |
Chen J B, Li J. Stochastic harmonic function and spectral representations [J]. Chin. J. Theor. Appl. Mech., 2011, 43: 505
|
| 24 |
陈建兵, 李 杰. 随机过程的随机谐和函数表达 [J]. 力学学报, 2011, 43: 505
|
| 25 |
Shinozuka M, Deodatis G. Simulation of multi-dimensional Gaussian stochastic fields by spectral representation [J]. Appl. Mech. Rev., 1996, 49: 29
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|