| 二元过渡族金属合金非晶态形成规律 |
| 欧阳义芳 钟夏平 陈红梅 |
| 广西大学物理系;南宁 530004 |
|
引用本文:
欧阳义芳; 钟夏平; 陈红梅 . 二元过渡族金属合金非晶态形成规律[J]. 金属学报, 1999, 35(10): 1095-1098 .
[1] Benjamin J S Metall Trans, 1970;1: 294 [2] Benjamin J S. Mater Sci Forum, 1992; 88-90: 1 [3] Koch C C, Cavin O B Mckamey C G, Scarbrongh J O. Appl Phys Lett, 1983; 43:1017 [4] Weeber A W, Bakker H. Physica, 1988; B153: 93 [5] Zhang H Zhang B W, Wu L J Wan Z Q. Acta Phyx Sin, 1994;43:1638 (张恒,张邦维,吴力军,万志齐,物理学报,1994;43:1638) [6] Bakker H, Zhou G F Yang H Prog Mater Sco, 1995; 39: 159 [7] Ma E Atzmon M. Mater Chem Phys, 1995; 39: 249 [8] Chen H S. Mater Sci Eng, 1976; 25: 59 [9]Chen H S.Acta Metall, 1974;22:1505 [10] Mader S Nowick A S, Widmer H Acta Metall, 1967; 15: 203 [11] Liu B X Johnson W L, Nicolet M A. Appl Phys Lett, 1983;42:45 [12] Zhang B W.J Mate, Sci, 1988; 7: 681 [13] Cahoon J R Sherby O D. Metall Trans, 1992; A23: 2491 [14] De Boer F R, Boom R, Mattens W C M, Miedema A R, Niessen A K. Coheaion in Metals. Amsterdam: North-Halland 1988: 1 [15] Hong L B, Fultz B. Acta Mater, 1998; 46: 2937 [16] Buldokhin Y V, Kaloshkin S D Shelekhov E V, Tomilin I A cherdyntsev V V,Fiz Met Metalloved, 1997;84:154 [17] Tcherdyntsev V V, Kaloshkin S D, Shelekhov E V, Tomilin I A Baldokhin Y V, Mater Sci Forum, 1998; 269-272: 145 [18] Froes F H,Baburaj E G,Clark C R,Bryskin B D.Matet Manuf Processes, 1998; 13: 657 [19]Yang Y J,Cui K,Li X G,Zhang J,zhang T J.J Alloy Compd,1996; 242:153 [20] Sell T, Mehrer H. Z Metallkd, 1997; 88: 842 [21]Kuyama J, Ishihara K N,Shingu P H.J Jpn Soc Powder Powder Metall, 1991;38:910 (久山纯司,石原庆一,新宫秀夫,日本粉末学会粉末冶金会报, 1991:38:910)5 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|