| 低碳钢烘烤硬化机制的内耗研究 |
李维娟( ), 张恒毅, 付豪, 张建平, 戚翔宇 |
| 辽宁科技大学材料与冶金学院, 鞍山 114051 |
|
| INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL |
LI Weijuan( ), ZHANG Hengyi, FU Hao, ZHANG Jianping, QI Xiangyu |
| School of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051 |
引用本文:
李维娟, 张恒毅, 付豪, 张建平, 戚翔宇. 低碳钢烘烤硬化机制的内耗研究[J]. 金属学报, 2015, 51(4): 385-392.
Weijuan LI,
Hengyi ZHANG,
Hao FU,
Jianping ZHANG,
Xiangyu QI.
INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL[J]. Acta Metall Sin, 2015, 51(4): 385-392.
| [1] |
De A K, Vandeputte S, De Coomana B C. Scr Mater, 1999; 41: 831
|
| [2] |
De A K, Blauwe K D, Vandeputteb S, De Cooman B C. J Alloys Compd, 2000; 310: 405
|
| [3] |
Zhao J Z, De A K, De Cooman B C. ISIJ Int, 2000; 40: 725
|
| [4] |
Speer G J, Matlock K D. JOM, 2002; 54(7): 19
|
| [5] |
Jiang H T, Kang Y L, Yu H. Auto Technol Mater, 2005; (3): 1
|
| [5] |
(江海涛, 康永林, 于 浩. 汽车工艺与材料, 2005; (3): 1)
|
| [6] |
Zhao J Z, De A K, De Cooman B C. Metall Mater Trans, 2001; 32A: 417
|
| [7] |
Baird J D. Int Mater Rev, 1971; 16(1): 1
|
| [8] |
Vasilyev A A, Leeb H C, Kuzmin L N. Mater Sci Eng, 2008; A485: 282
|
| [9] |
Zhao J Z, De A K, De Cooman B C. Mater Lett, 2000; 44: 374
|
| [10] |
De A K, Vandeputte S, De Cooman B C. Scr Mater, 2001; 44: 695
|
| [11] |
Cottrell A H, Bilby B A. Phys Soc London, 1949; 62(1)A: 49
|
| [12] |
Soenen B, De A K, Vandeputte S, De Cooman B C. Acta Mater, 2004; 52: 3483
|
| [13] |
Wert C, Marx J. Acta Metall, 1953; 1: 113
|
| [14] |
Wert C A. Phys Rev, 1950; 79: 601
|
| [15] |
Wert C A. Physics, 1949; 20: 943
|
| [16] |
Bagramov R, Mari D, Benoit W. Philos Mag, 2001; 81A: 2797
|
| [17] |
Ji J W, Yu N. Prog Phys, 2006; 26: 296
|
| [17] |
(戢景文, 于 宁. 物理学进展, 2006; 26: 296)
|
| [18] |
Fang Q F, Wang X P, Wu X B, Lu H. Physics, 2011; 40: 786
|
| [18] |
(方前锋, 王先平, 吴学邦, 鲁 卉. 物理, 2011; 40: 786)
|
| [19] |
Ji J W, Liu F D, Wang D J, Che Y Y, Hua Q Z, Liu J M, Huang Z R. Acta Metall Sin, 1999; 35: 913
|
| [19] |
(戢景文, 刘芬娣, 王登京, 车韵怡, 华桥柱, 刘建民, 黄镇如. 金属学报, 1999; 35: 913)
|
| [20] |
Yu N, Liu Y G, Zhang Z B, Zhan H, Zhang J, Ji J W. J ShangHai JiaoTong Univ, 2010; 44: 624
|
| [20] |
(于 宁, 刘永刚, 张志波, 詹 华, 张 建, 戢景文. 上海交通大学学报, 2010; 44: 624)
|
| [21] |
Che Y Y, Sun Y J, Ji J W. J Northeastern Univ (Nat Sci), 1997; 18: 676
|
| [21] |
(车韵怡, 孙玉杰, 戢景文. 东北大学学报(自然科学版), 1997; 18: 676)
|
| [22] |
Che Y Y, Liu F D, Zeng G Y, Xu Y C, Ji J W. Acta Metall Sin, 1998; 34: 831
|
| [22] |
(车韵怡, 刘芬娣, 曾桂仪, 许余昌, 戢景文. 金属学报, 1998; 34: 831)
|
| [23] |
Yu N, Ji J W. Acta Metall Sin, 2002; 38: 230
|
| [23] |
(于 宁, 戢景文. 金属学报, 2002; 38: 230)
|
| [24] |
Ge T S. Solid Internal Friction Theoretical Basis. Beijing: Science Press, 2000: 62
|
| [24] |
(葛庭燧. 固体内耗理论基础. 北京: 科学出版社, 2000: 62)
|
| [25] |
De A K, Vandeputte S, De Cooman B C. J Mater Eng Perform, 2001; 10: 567
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|