金属学报  2015, Vol. 51 Issue (4): 385-392    DOI: 10.11900/0412.1961.2014.00434
  本期目录 | 过刊浏览 |
低碳钢烘烤硬化机制的内耗研究
李维娟(), 张恒毅, 付豪, 张建平, 戚翔宇
辽宁科技大学材料与冶金学院, 鞍山 114051
INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL
LI Weijuan(), ZHANG Hengyi, FU Hao, ZHANG Jianping, QI Xiangyu
School of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051
引用本文:

李维娟, 张恒毅, 付豪, 张建平, 戚翔宇. 低碳钢烘烤硬化机制的内耗研究[J]. 金属学报, 2015, 51(4): 385-392.
Weijuan LI, Hengyi ZHANG, Hao FU, Jianping ZHANG, Xiangyu QI. INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL[J]. Acta Metall Sin, 2015, 51(4): 385-392.

全文: PDF(3639 KB)   HTML
摘要: 

测试了低碳钢不同退火温度下烘烤态的应力-应变曲线和烘烤硬化(BH)值以及变形态和烘烤态的内耗曲线, 研究了不同退火温度下的烘烤硬化机制. 结果表明, 退火温度由750 ℃逐渐提高到880 ℃, 应力-应变曲线均表现不连续屈服现象, 且屈服平台的锯齿状越来越明显, 屈服点延伸量不断增大. 退火温度由750 ℃提高到780 ℃, BH值降低, 变形态和烘烤态的Snoek峰高差值增大, SKK峰高降低, Kê峰变化不大, 固溶强化对烘烤硬化起主导作用. 退火温度由780 ℃逐渐提高到880 ℃, BH值不断增大, 变形态和烘烤态的Snoek峰高差值逐渐减小, SKK峰的驰豫强度逐渐增大, Kê峰变化不大, Cottrell气团强化对烘烤硬化的作用逐渐增强. 烘烤硬化机制是固溶强化、Cottrell气团强化和沉淀强化的共同作用.

关键词 : 烘烤硬化,  内耗,  固溶强化,  Cottrell气团强化,  沉淀强化    
Abstract:

High strength steel plates are being applied more extensively in automobile industry under higher demands of weight reduction, safety and environmental protection. As one of the high strength steel plates for automobile body panel, bake-hardening steel plate is featured by low yield strength and good formability during stamping, and is particularly featured by improved yield strength through following paint baking process, exhibiting higher strength and anti-dent ability in service. Bake-hardening (BH) is closely related to interactions between interstitial atoms and crystal defects during baking process. In this work, BH mechanisms in low carbon steel are studied under different annealing temperatures by measuring and analyzing stress-strain curves and BH values in baked conditions, and internal friction curves in both deformed and baked conditions. The results show that when the annealing temperature increases gradually from 750 to 880 ℃, the stress-strain curves exhibit discontinuous yielding behavior with stronger serration of yield platform and continuous elongation of yield point. With the increase of the annealing temperature from 750 to 780 ℃, BH value decreases, difference between Snoek peak values in deformed and baked conditions increases, SKK peak value decreases, and Kê peak value does not change significantly, which indicates that solid solution strengthening dominates the BH. When the annealing temperature increases from 780 to 880 ℃, BH value continuously increases, difference between Snoek peak values in deformed and baked conditions gradually decreases, relaxation strength of SKK peak gradually increases, and Kê peak is stable, which indicates that Cottrell atmosphere strengthening is playing an increasing role in the BH. The BH is due to a combined mechanism contributed by solid solution strengthening Cottrell atmosphere strengthening and precipitation strengthening.

Key words: bake-hardening    internal friction    solid solution strengthening    Cottrell atmosphere strengthening    precipitation strengthening
    
ZTFLH:  TG142.1  
基金资助:* 国家自然科学基金资助项目51274121
作者简介: null

李维娟, 女, 1966生, 教授

图1  低碳钢在不同退火温度下的显微组织
图2  低碳钢烘烤硬化(BH)态的应力-应变曲线
图3  低碳钢不同退火温度下的BH值
图4  低碳钢不同退火温度下的内耗曲线
图5  不同退火温度的变形态Snoek峰高(hs)和变形态与烘烤态Snoek峰高的差值(ht)
图6  不同退火温度下变形态与烘烤态的Kê峰
[1] De A K, Vandeputte S, De Coomana B C. Scr Mater, 1999; 41: 831
[2] De A K, Blauwe K D, Vandeputteb S, De Cooman B C. J Alloys Compd, 2000; 310: 405
[3] Zhao J Z, De A K, De Cooman B C. ISIJ Int, 2000; 40: 725
[4] Speer G J, Matlock K D. JOM, 2002; 54(7): 19
[5] Jiang H T, Kang Y L, Yu H. Auto Technol Mater, 2005; (3): 1
[5] (江海涛, 康永林, 于 浩. 汽车工艺与材料, 2005; (3): 1)
[6] Zhao J Z, De A K, De Cooman B C. Metall Mater Trans, 2001; 32A: 417
[7] Baird J D. Int Mater Rev, 1971; 16(1): 1
[8] Vasilyev A A, Leeb H C, Kuzmin L N. Mater Sci Eng, 2008; A485: 282
[9] Zhao J Z, De A K, De Cooman B C. Mater Lett, 2000; 44: 374
[10] De A K, Vandeputte S, De Cooman B C. Scr Mater, 2001; 44: 695
[11] Cottrell A H, Bilby B A. Phys Soc London, 1949; 62(1)A: 49
[12] Soenen B, De A K, Vandeputte S, De Cooman B C. Acta Mater, 2004; 52: 3483
[13] Wert C, Marx J. Acta Metall, 1953; 1: 113
[14] Wert C A. Phys Rev, 1950; 79: 601
[15] Wert C A. Physics, 1949; 20: 943
[16] Bagramov R, Mari D, Benoit W. Philos Mag, 2001; 81A: 2797
[17] Ji J W, Yu N. Prog Phys, 2006; 26: 296
[17] (戢景文, 于 宁. 物理学进展, 2006; 26: 296)
[18] Fang Q F, Wang X P, Wu X B, Lu H. Physics, 2011; 40: 786
[18] (方前锋, 王先平, 吴学邦, 鲁 卉. 物理, 2011; 40: 786)
[19] Ji J W, Liu F D, Wang D J, Che Y Y, Hua Q Z, Liu J M, Huang Z R. Acta Metall Sin, 1999; 35: 913
[19] (戢景文, 刘芬娣, 王登京, 车韵怡, 华桥柱, 刘建民, 黄镇如. 金属学报, 1999; 35: 913)
[20] Yu N, Liu Y G, Zhang Z B, Zhan H, Zhang J, Ji J W. J ShangHai JiaoTong Univ, 2010; 44: 624
[20] (于 宁, 刘永刚, 张志波, 詹 华, 张 建, 戢景文. 上海交通大学学报, 2010; 44: 624)
[21] Che Y Y, Sun Y J, Ji J W. J Northeastern Univ (Nat Sci), 1997; 18: 676
[21] (车韵怡, 孙玉杰, 戢景文. 东北大学学报(自然科学版), 1997; 18: 676)
[22] Che Y Y, Liu F D, Zeng G Y, Xu Y C, Ji J W. Acta Metall Sin, 1998; 34: 831
[22] (车韵怡, 刘芬娣, 曾桂仪, 许余昌, 戢景文. 金属学报, 1998; 34: 831)
[23] Yu N, Ji J W. Acta Metall Sin, 2002; 38: 230
[23] (于 宁, 戢景文. 金属学报, 2002; 38: 230)
[24] Ge T S. Solid Internal Friction Theoretical Basis. Beijing: Science Press, 2000: 62
[24] (葛庭燧. 固体内耗理论基础. 北京: 科学出版社, 2000: 62)
[25] De A K, Vandeputte S, De Cooman B C. J Mater Eng Perform, 2001; 10: 567
[1] 韩林至, 牟娟, 周永康, 朱正旺, 张海峰. 热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响[J]. 金属学报, 2022, 58(9): 1159-1168.
[2] 张银辉, 冯强. W对新型Nb稳定化奥氏体耐热铸钢1000 ℃蠕变行为的影响[J]. 金属学报, 2017, 53(9): 1025-1037.
[3] 王小娜, 韩利战, 顾剑锋. NZ30K镁合金时效析出动力学与强化模型的研究*[J]. 金属学报, 2014, 50(3): 355-360.
[4] 陈俊, 唐帅,刘振宇,王国栋. 冷却方式对Nb-Ti微合金钢组织和性能及沉淀行为的影响[J]. 金属学报, 2012, 48(4): 441-449.
[5] 杜刚 杨文 闫德胜 戎利建. 铸态Al-Mg-Sc-Zr合金退火过程中的硬化行为[J]. 金属学报, 2011, 47(3): 311-316.
[6] 王华 史文 何燕霖 符仁钰 李麟. Mn和P在超低碳烘烤硬化钢中的分布形态及对其拉伸行为的影响研究[J]. 金属学报, 2011, 47(3): 263-268.
[7] 冷崇燕 周荣 张旭 卢德宏 刘洪喜. Ag和Ta离子双注入改善Ti6Al4V合金耐磨性能[J]. 金属学报, 2009, 45(6): 764-768.
[8] 吴杰 崔洪芝 迟静 姚树玉 韩福生. B2 Fe-Al合金有序化过程中的内耗峰[J]. 金属学报, 2009, 45(4): 396-399.
[9] 张建; 李秀艳; 赵明久; 戎利建 . 晶界相对Fe-Ni-Cr奥氏体合金氢脆的影响[J]. 金属学报, 2008, 44(9): 1095-1098 .
[10] 孙蔚; 韩福生; 吴杰 . Fe-Al合金中与Al反位置原子弛豫有关的内耗峰[J]. 金属学报, 2007, 43(3): 311-314 .
[11] 张建; 李秀艳; 戎利建; 郑永男; 朱升云 . Fe-Ni基合金氢脆的正电子湮没寿命谱研究[J]. 金属学报, 2006, 42(5): 469-473 .
[12] 汪宏斌; 王晓宇; 张骥华; 徐祖耀 . 纳米晶Fe-25%Ni合金块材的内耗研究[J]. 金属学报, 2004, 40(5): 523-526 .
[13] 张华力; 刘卫; 苏金瑞; 丁锦文; 陈初升 . La2NiO4.147体系相变的低频内耗[J]. 金属学报, 2003, 39(11): 1157-1159 .
[14] 马永青; 宋文海; 戴建明; 张瑞丽; 杨杰; 杜家驹; 孙玉平 . 钙钛矿结构锰氧化物La0.67Ca0.33MnO3的内耗研究[J]. 金属学报, 2003, 39(11): 1173-.
[15] 李合琴; 陈志宝 . 低掺杂La0.82Sr0.18MnO3巨磁电阻块材的低频内耗[J]. 金属学报, 2003, 39(11): 1170-1172 .