| 金属-氢共晶定向凝固热力学模型* |
李再久, 金青林( ), 杨天武, 周荣, 蒋业华 |
| 昆明理工大学材料科学与工程学院, 昆明 650093 |
|
| A THERMODYNAMIC MODEL FOR DIRECTIONAL SOLIDIFICATION OF METAL-HYDROGEN EUTECTIC |
LI Zaijiu, JIN Qinglin( ), YANG Tianwu, ZHOU Rong, JIANG Yehua |
| Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093 |
引用本文:
李再久, 金青林, 杨天武, 周荣, 蒋业华. 金属-氢共晶定向凝固热力学模型*[J]. 金属学报, 2014, 50(4): 507-514.
Zaijiu LI,
Qinglin JIN,
Tianwu YANG,
Rong ZHOU,
Yehua JIANG.
A THERMODYNAMIC MODEL FOR DIRECTIONAL SOLIDIFICATION OF METAL-HYDROGEN EUTECTIC[J]. Acta Metall Sin, 2014, 50(4): 507-514.
| [1] |
Shapovalov V I. US Pat, 5181549, 1993
|
| [2] |
Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2004; 40: 1121
|
| [2] |
(刘 源, 李言祥, 张华伟. 金属学报, 2004; 40: 1121 )
|
| [3] |
Liu P S. Introduction to Cellular Materials. Beijing: Tsinghua University Press, 1999: 6
|
| [3] |
(刘培生. 多孔材料引论. 北京: 清华大学出版社, 1999: 6)
|
| [4] |
Simone A E, Gibson L J. Acta Mater, 1996; 44: 1437
|
| [5] |
Nakajima H, Hyun S K, Ohashi K, Ota K, Murakami K. Colloids Surf, 2001; 179A: 209
|
| [6] |
Li Z J, Jin Q L, Yang T W, Jiang Y H, Zhou R. Acta Metall Sin, 2013; 49: 757
|
| [6] |
(李再久, 金青林, 杨天武, 蒋业华, 周 荣. 金属学报, 2013; 49: 757)
|
| [7] |
Liu Y, Li Y X, Zhang H W, Wan J. Acta Metall Sin, 2005; 41: 886
|
| [7] |
(刘 源, 李言祥, 张华伟, 万 疆. 金属学报, 2005; 41: 886 )
|
| [8] |
Xie J X, Liu X H, Liu X F, Fang Y C, Wang H. Chin J Nonferrous Met, 2005; 15: 1869
|
| [8] |
(谢建新, 刘新华, 刘雪峰, 方玉诚, 王 浩. 中国有色金属学报, 2005; 15: 1869)
|
| [9] |
Simone A E, Gibson L J. J Mater Sci, 1997; 32: 451
|
| [10] |
Nakajima H. Progr Mater Sci, 2007; 52: 1091
|
| [11] |
Peng Z, Yang T W, Li Z J, Li Z H, Jin Q L, Zhou R. Chin J Nonferrous Met, 2011; 21: 1045
|
| [11] |
(彭 震, 杨天武, 李再久, 黎振华, 金青林, 周 荣. 中国有色金属学报, 2011; 21: 1045)
|
| [12] |
Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1165
|
| [12] |
(张华伟, 李言祥, 刘 源. 金属学报, 2006; 42: 1165)
|
| [13] |
Liu Y, Li Y X. Scr Mater, 2003; 49: 379
|
| [14] |
Upadhyaya G S,Dube R K. Problems in Metallurgical Thermodynamics and Kinetics. Oxford: Pergamon Press, 1977: 144
|
| [15] |
Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2007; 43: 113
|
| [15] |
(张华伟, 李言祥, 刘 源. 金属学报, 2007; 43: 113)
|
| [16] |
Zhang H W. PhD Dissertation, Tsinghua University, Beijing, 2006
|
| [16] |
(张华伟. 清华大学博士学位论文, 北京, 2006)
|
| [17] |
Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2005; 41: 55
|
| [17] |
(张华伟, 李言祥, 刘 源. 金属学报, 2005; 41: 55)
|
| [18] |
Flemings M C. Solidification Processing. Newyork: McGraw-Hill Book Company, 1974: 264
|
| [19] |
Nishizawa T. Translated by Hao S M. Thermodynamics of Microstructure. Beijing: Chemical Industry Press, 2006: 264
|
| [19] |
(Nishizawa T著. 郝士明 译. 微观组织热力学. 北京: 化学工业出版社, 2006: 264)
|
| [20] |
Liu Y, Li Y X, Liu R F, Zhou R, Jiang Y H, Li Z H. Acta Metall Sin, 2010; 46: 129
|
| [20] |
(刘 源, 李言祥, 刘润发, 周 荣, 蒋业华, 黎振华. 金属学报, 2010; 46: 129)
|
| [21] |
Yamamura S, Shiota H, Murakami K, Nakajima H. Mater Sci Eng, 2001; A318: 137
|
| [22] |
Drenchev L, Sobczak J, Sobczak N, Sha W, Malinov S. Acta Mater, 2007; 55: 6459
|
| [23] |
Sacris E M, Parlee A D. Metall Trans, 1970; 1: 3377
|
| [24] |
Martin J W,Doherty. Stability of Microstructure in Metallic System. London: Cambridge University Press, 1976: 159
|
| [25] |
Park J S, Hyun S K, Suzuki S, Nakajima H. Acta Mater, 2007; 55: 5646
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |