| 3A21铝合金-20钢管磁脉冲连接实验研究 |
| 于海平, 徐志丹, 李春峰, 赵志学 |
1) 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001
2) 哈尔滨工业大学现代焊接生产技术国家重点实验室, 哈尔滨 150001 |
|
| EXPERIMENTAL RESEARCH ON MAGNETIC PULSE JOINING OF 3A21 ALUMINUM ALLOY-20 STEEL TUBES |
| YU Haiping, XU Zhidan, LI Chunfeng, ZHAO Zhixue |
1) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
2) State Key Laboratory of Advanced Welding Production Technology, Harbin Institute of Technology, Harbin 150001 |
引用本文:
于海平 徐志丹 李春峰 赵志学. 3A21铝合金-20钢管磁脉冲连接实验研究[J]. 金属学报, 2011, 47(2): 197-202.
,
,
,
.
EXPERIMENTAL RESEARCH ON MAGNETIC PULSE JOINING OF 3A21 ALUMINUM ALLOY-20 STEEL TUBES[J]. Acta Metall Sin, 2011, 47(2): 197-202.
| [1] Yu H P, Xu D G, Li C F. Forg Stamp Technol, 2009; 34(2): 1(于海平, 徐殿国, 李春峰. 锻压技术, 2009; 34(2): 1)[2] Benedyk J C. Light Met Age, 2001; 59: 48[3] Sun M R. Weld Technol, 1999; 6: 13(孙明如. 焊接技术, 1999; 6: 13)[4] Kochan A. Assemb Auto, 2000; 20: 129[5] Anthony L, Velocci J. Aviat Week Space Technol, 1993; 139: 59[6] Uhlmann E, Hahn R, Jurgasch D. Steel Res Int, 2005; 76: 245[7] Marya M, Priem D, Marya S. Mater Sci Forum, 2003; 426–432: 4001[8] Kimchi M, Shao H, Cheng W, Krishnaswamy P. Weld World, 2004; 48: 19[9] Shribman V, Stern A, Livs Y, Gafri O. Weld J, 2002; 4: 33[10] Marya M, Marya S. Sci Technol Weld Join, 2004; 9: 541[11] Stern A, Aizenshtein M. Sci Technol Weld Join, 2002; 7: 339[12] Aizawa T, Kashani M, Okagawa K. Weld World, 2005; 49: 212[13] Ben–Artzy A, Stern A, Frage N, Shribman V, Sadot O. Int J Impact Eng, 2010; 37: 307[14] Watanabe M, Kumai S, Hagimoto G, Zhang Q S, Nakayama K. Mater Trans, 2009; 50: 279[15] Kore S D, Date P P, Kulkarni S V. Int J Impact Eng, 2007; 34: 1327[16] Ben–Artzy A, Stern A, Frage N. Sci Technol Weld Join, 2008; 13: 402[17] Wang Y H. Research and Practice of Explosive Welding of Metal Plates. Beijing: National Defense Industry Press, 2007: 31(王耀华. 金属板材爆炸焊接研究与实践. 北京: 国防工业出版社, 2007: 31) |
|