| 不锈钢在循环形变中的Bauschinger效应及其位错结构 |
| 夏月波;王中光;杜秀魁 |
| 副研究员;沈阳中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| BAUSCHINGER EFFECT AND DISLOCATION STRUCTURE IN STAINLESS STEEL DURING CYCLIC DEFORMATION |
| XIA Yuebo;WANG Zhongguang;DU Xiukui Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
夏月波;王中光;杜秀魁. 不锈钢在循环形变中的Bauschinger效应及其位错结构[J]. 金属学报, 1988, 24(4): 221-227.
,
,
.
BAUSCHINGER EFFECT AND DISLOCATION STRUCTURE IN STAINLESS STEEL DURING CYCLIC DEFORMATION[J]. Acta Metall Sin, 1988, 24(4): 221-227.
1 Bauschinger J. Min Proc Inst Civil Eng, London, 1886; 87: 463 2 Mataya M C, Carr M J. Mater Sci Eng, 1983; 57: 205 3 Stoltz R E, Pclloux R M. Metall Trans, 1976; 7A: 1295 4 Saleh Y, Margolin H. Acta Metall, 1979; 27: 535 5 Abel A, Ham R K. Acta Metall, 1966; 14: 755 6 Hull D. Introduction to Dislocation, Oxford: Pergamon Press, 1968: 136 7 Daniels R C, Horn G T. Metall Trans, 1971; 2: 1161 8 Griffiths D, Riley J N. Acta Metall, 1966; 14: 755 9 Fisher J C, Hart E W, Pry R H. Acta Metall, 1953; 1: 336 10 Sowerby R, Uko D K, Tomita Y. Mater Sci Eng, 1979; 41: 43 11 Li C C, Flaseh J O, Yaker J A, Leslie W C. Metall Trans, 1978; 9A: 85 12 Hasegawa J, Yakou T, Shimizn M, Karashima S. Trans Jpn Inst Met, 1976; 17: 414 13 Odegard B C, West A J, Brooks J A. In: Thompson A W, Bernstein I M eds., Effect of Hydrogen on Behaviour of Materials, New York: AIME, 1976: 189 14 Stoltz R E, Vander Sande J B. Metall Trans, 1980; 11A: 1033 15 Thompson A W. Metall Trans, 1977; 8A: 833 16 Mughrabi H. Acta Metall, 1983; 31: 1367 17 Embury J D. Strengthening Methods in Crystals, London: Applied Science, 1971: 348 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|