| 1Cr18Ni9Ti微塑性变形行为的研究 |
| 朱平;张力宁 |
| 东南大学;东南大学 |
|
| MICROPLASTIC DEFORMATION BEHAVIOUR OF 1Cr18Ni9Ti STAINLESS STEEL |
| ZHU Ping;ZHANG Lining Southeast University; Nanjing ZHU Ping; Deportment of Material Science and Engineering; Southeast University; Nanjing |
引用本文:
朱平;张力宁. 1Cr18Ni9Ti微塑性变形行为的研究[J]. 金属学报, 1989, 25(6): 126-130.
,
.
MICROPLASTIC DEFORMATION BEHAVIOUR OF 1Cr18Ni9Ti STAINLESS STEEL[J]. Acta Metall Sin, 1989, 25(6): 126-130.
1 Kula E, Weiss V. Residual Stress and Stress Relaxation, New York: Plenum, 1982 2 #12 3 Rudchenko V V, Dudarev Ye P. Phy Met Metallogr, 1981; (6) : 175 4 Marschall C W, Marlnger R E. Dimensional Inst ability. Oxfork: Pergamon, 1977 5 Хенкин М Л,Локшин И Х.蔡安源、杜淑芳译.精密机械制造与仪器制造中金属与合金的尺寸稳定性,北京:科学出版社,1981:4 6 周邦新.金属学报,1983;19:A31* |
|