| 高频等离子法制取超细氮化钛反应动力学研究 |
| 朱联锡;邹四维 |
| 成都科技大学环境科学及工程系;副教授成都(610065);成都科技大学 |
|
| KINETICS OF PREPARATION OF ULTRAFINE TiN POWDER BY HIGH FREQUENCY PLASMA |
| ZHU Lianxi;ZOU Siwei Chengdu University of Science and Technology Department of Environmental Science and Engineering;Chengdu University of Science and Technology;Chengdu 610065 |
引用本文:
朱联锡;邹四维. 高频等离子法制取超细氮化钛反应动力学研究[J]. 金属学报, 1990, 26(1): 135-140.
,
.
KINETICS OF PREPARATION OF ULTRAFINE TiN POWDER BY HIGH FREQUENCY PLASMA[J]. Acta Metall Sin, 1990, 26(1): 135-140.
1 福原幹夫,永井弘,三谷裕康.日本金属学会志,1978;42:588 2 Zhu Lianxi (朱联锡), Jin Peng (金鹏), Ran Junguo (冉均国). Proc Int Conf on Plasma Science and Technology, Beijing: Science Press, 1986: 329 3 Zhu Lianxi (朱联锡), Jin Peng (金鹏), Xiao Xian-Zhi (肖显志). Proc 8th Int Symp. on Plasma Chemistry, Tokyo, 1987: 2087 4 Saeki Y, Matsuzaki R, Yajima A, Akiyama M. Bull Chem Soc Jpn, 1982; 55: 3193 5 #12i |
|