| 氮对HK50合金组织和力学性能的影响 |
| 于永泗;曹智本;王富岗;郭晓冰 |
| 大连理工大学材料工程系;讲师;大连(116024);大连理工大学;大连理工大学;锦州工学院 |
|
| EFFECT OF NITROGEN ON MICROSTRUCTURE AND PROPERTIES OF HK50 ALLOY |
| YU Yongsi;CAO Zhiben;WANG Fugang;GUO Xiaobing Dalian University of Technology Jinzhou Institute of Technology lecturer;Department of Materials Engineering;Dalian University of Technology; Dalian 116024 |
引用本文:
于永泗;曹智本;王富岗;郭晓冰. 氮对HK50合金组织和力学性能的影响[J]. 金属学报, 1990, 26(2): 16-20.
,
,
,
.
EFFECT OF NITROGEN ON MICROSTRUCTURE AND PROPERTIES OF HK50 ALLOY[J]. Acta Metall Sin, 1990, 26(2): 16-20.