| F6-21Ni-4Mn合金强脉冲磁场诱发马氏体相变的研究 |
| 孙恩喜;杨大智;徐祖耀;杨伏明;赵汝文 |
| 大连铁道学院;大连理工大学材料系;教授;大连(116024);上海交通大学;中国科学院物理研究所;中国科学院物理研究所 |
|
| PULSED MAGNETIC FIELD-INDUCED MARTENSITIC TRANSFORMATION IN AN Fe-21Ni-4Mn ALLOY |
| SUN Enxi;YANG Dazhi;XU Zuyao;YANG Fumiug;ZHAO Ruwen Dalian Institute of Railway Dalian University of Technology Shanghai Jiaotong University Institute of Physics; Academia Sinica; Beijing professor |
引用本文:
孙恩喜;杨大智;徐祖耀;杨伏明;赵汝文. F6-21Ni-4Mn合金强脉冲磁场诱发马氏体相变的研究[J]. 金属学报, 1990, 26(4): 12-17.
,
,
,
,
.
PULSED MAGNETIC FIELD-INDUCED MARTENSITIC TRANSFORMATION IN AN Fe-21Ni-4Mn ALLOY[J]. Acta Metall Sin, 1990, 26(4): 12-17.
1 Zolotarevskiy I V, Snezhnoy V L, Georgiyeya Y, Matyushenko L A, Fiz Met Metalloved, 1981; 51: 669 2 Yang D Z, Sadvik B P J, Wayman C M. Metall Trans, 1984; 15A: 1555 3 Yang D Z, Wayman C M. Acta Metall, 1984; 17: 949 4 Korenko M K, Cohen M. Pioc Int Conf on MAT-79, Cambridge, Mass., 1979: 388 5 Grangle J, Hallam G C. Proc R Soc (London), 1963; A272: 119 6 Romashev L N, Leontiev A A, Schastlivtsev V M, Sadovsky V D. Fiz Met Metalloved, 1984; 57: 768 7 Kakeshita T, Shimizu K, Kijima S, Yu Zkihong, Date M. Trans Jpn Inst Met, 1985; 26: 630 8 Kakeshita T, Shirai H, Shimizu K, Sugiyama K, Hazumi K, Date M. Trans Jpn Inst Met, 1987; 28: 891 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|