残余应力集中及其对疲劳极限和短裂纹扩展的影响 |
何家文;胡奈赛;张定铨 |
西安交通大学金属材料及强度研究所;教授;西安(710049);西安交通大学;西安交通大学 |
|
RESIDUAL STRESS CONCENTRATION AND ITS EFFECTS ON FATIGUE LIMIT AND SHORT CRACK GROWTH |
HE Jiawen; HU Naisai; ZHANG Dingquan (Xi'an Jiaotong University) |
引用本文:
何家文;胡奈赛;张定铨. 残余应力集中及其对疲劳极限和短裂纹扩展的影响[J]. 金属学报, 1992, 28(9): 30-34.
,
,
.
RESIDUAL STRESS CONCENTRATION AND ITS EFFECTS ON FATIGUE LIMIT AND SHORT CRACK GROWTH[J]. Acta Metall Sin, 1992, 28(9): 30-34.
1 #12 2 Fuchs H O. Exp Mech, 1971; 11: 548. 3 Wohlfahrt, H, Residual Stress and Stress Relaxation. New York: Plenum, 1982: 71 4 Bergstrom J, Ericsson T. In: Fuchs H O ed., Proc 2nd Int Conf on Shot Peening, ICSP-2, Chicago, 14-17, May, 1984, Paramus, New Jersey: American Shot Feening Society, 1984:241 5 Kloos, K H. Z Werkstofftech, 1981; 12: 359 6 徐可为,张定全,张玉华,胡奈赛,实验力学,1989;4(4) :367' |
|