| INCONEL718型合金中γ″和γ′的复合及单独析出对组织稳定性的影响 |
| 董建新;谢锡善;章守华 |
| 北京科技大学材料系;博士研究生;北京100083;北京科技大学;北京科技大学 |
|
| INFLUENCES OF ASSOCIATED AND SEPARATE PRECIPITATION OFγ′WITH γ" ON THERMAL STRUCTURE STABILITY IN INCONEL718 TYPE ALLOYS |
| XIE Xishan;ZHANG Shouhua University of Science and Technology BeijingDONG Jianxin;Department of Materials Science and Egnineering University of Science and Technology Beijing |
引用本文:
董建新;谢锡善;章守华. INCONEL718型合金中γ″和γ′的复合及单独析出对组织稳定性的影响[J]. 金属学报, 1993, 29(6): 28-32.
,
,
.
INFLUENCES OF ASSOCIATED AND SEPARATE PRECIPITATION OFγ′WITH γ" ON THERMAL STRUCTURE STABILITY IN INCONEL718 TYPE ALLOYS[J]. Acta Metall Sin, 1993, 29(6): 28-32.