| 易切削钢冲击断口分维的随机分形分析 |
| 李学良;林建新 |
| 合肥工业大学 |
|
| RANDOM FRACTAL STUDY OF FRACTURE SURFACE OF FREE-MACHINING STEELS |
| LI Xueliang;LIN Jianxin (Hefei Polytechnical University) |
引用本文:
李学良;林建新. 易切削钢冲击断口分维的随机分形分析[J]. 金属学报, 1994, 30(8): 380-384.
,
.
RANDOM FRACTAL STUDY OF FRACTURE SURFACE OF FREE-MACHINING STEELS[J]. Acta Metall Sin, 1994, 30(8): 380-384.
| 1MandelbrotBB.PassojaDE,PaulldyAJNature1984;308:7212苏辉,张玉贵,阎振綮.金属学报,1989;25:A4663pandeCS,RichnrdsLE,LouatN,DempseyBD,SchwoebleAJActaMetall.1987:35:16334苏辉,张玉贵,阎振綮,材料科学进展,1990;4:3395LungCWIn:PietroneroL.TosattiEeds.FractalsinPhysicsAmsterdarm:ElsevierScience,1986:1896苏辉,陈冷,阎振綮.科学通报,1991;36:15107江来珠,崔 .金属学报,1992:28:A278江来珠.华中理工大学博士学位论文.19909FalconerK,FractalGeometry──MathematicalFoundationsandApplicationsNewYork:Wily1990:23010关治,陈景良数值计算方法,北京:清华大学出版社,1990:188X |
|