| 室温低压下脉冲等离子体生长立方氮化硼薄膜 |
| 阎鹏勋;杨思泽;孙牧;任育峰;李兵;陈熙琛 |
| 中国科学院物理研究所 |
|
| PULSED PLASMA PRODUCTION OF c-BN THIN FILMS AT ROOM TEMPERATURE AND LOW PRESSURE |
| YAN Pengxun;YANG Size;SUN Mu;REN Yufeng;LI Bing;CHEN Xichen(Institute of Physics; Chinese Academy of Sciences;Beijing 100080)(Manuscript received 1995-03-17;in revised form 1995-06-19) |
引用本文:
阎鹏勋;杨思泽;孙牧;任育峰;李兵;陈熙琛. 室温低压下脉冲等离子体生长立方氮化硼薄膜[J]. 金属学报, 1995, 31(23): 489-492.
,
,
,
,
,
.
PULSED PLASMA PRODUCTION OF c-BN THIN FILMS AT ROOM TEMPERATURE AND LOW PRESSURE[J]. Acta Metall Sin, 1995, 31(23): 489-492.
| 1WentorfRH.JChemPhys,1957;26:9562WeissmentelC.JVacSciTechnol.1981;18:1793TakahashiH,ItohH,TaheuchiA.JCrystGrowth,1979;47:2454OkamotoM,UtsumiY,OsakaY.JpnJApplPhys.1990;29:L10045ShunfieldS,WolfsonR.JVacSciTechnol,1983;41:3236FriedmannTA,McCartgKF,KlausEJ,BoehmeD.ApplPhysLett.1992;61:24067吴成,江德仪,袁定朴,杨思泽,沈志刚,李椿萱.核裂变与等离子体物理,1989;9:1788阎鹏勋,杨思泽,李兵,陈熙琛.科学通报,1994;39:15479YanPX,YangSZ,YangJ,LiQ,LiB.ChinPhysLett,1994;11:55810YanPX,YangSZ,LiB,ChenXC,NuclInstrumMethodsPhysRes,1994;B95:55 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|