Please wait a minute...
金属学报  2026, Vol. 62 Issue (10): 1627-1634    DOI: 10.11900/0412.1961.2026.00091
  ★名家经典★ 本期目录 | 过刊浏览 |
原位自生硼化物增强高强-高导铜基复合材料设计与制备
梁淑华1,2(), 姜伊辉1,2, 石浩1,2, 曹飞1,2
1 西安理工大学 材料科学与工程学院 导电材料与复合技术教育部工程研究中心 西安 710048
2 西安理工大学 材料科学与工程学院 陕西省电工材料与熔渗技术重点实验室 西安 710048
Design and Fabrication of High-Strength, High-Conductivity Copper Matrix Composites Reinforced with In Situ-Formed Borides
LIANG Shuhua1,2(), JIANG Yihui1,2, SHI Hao1,2, CAO Fei1,2
1 Engineering Research Center of Conducting Materials and Composite Technology (Ministry of Education), School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
2 Shaanxi Province Key Laboratory of Electrical Materials and Infiltration Technology, School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
引用本文:

梁淑华, 姜伊辉, 石浩, 曹飞. 原位自生硼化物增强高强-高导铜基复合材料设计与制备[J]. 金属学报, 2026, 62(10): 1627-1634.
Shuhua LIANG, Yihui JIANG, Hao SHI, Fei CAO. Design and Fabrication of High-Strength, High-Conductivity Copper Matrix Composites Reinforced with In Situ-Formed Borides[J]. Acta Metall Sin, 2026, 62(10): 1627-1634.

全文: PDF(2188 KB)   HTML
摘要: 

铜基复合材料因优异的抗高温软化能力成为面向极端服役环境应用的关键导电材料。然而,传统铜基复合材料存在强度-电导率倒置关系的科学难题。对此,作者团队提出了基于材料加工过程中原位反应时机的精准调控从而设计多元多尺度增强相的思路,分别针对铸造与粉末冶金等成形技术特点,设计出混杂增强与多级构型等具有特定结构的铜基复合材料,基于多元多尺度增强相的协同效应提升增强相的强化效率,有效缓解铜基复合材料综合性能倒置关系。本文以原位自生硼化物增强铜基复合材料体系为代表,系统阐述了在铸造与粉末冶金等传统金属材料制造技术框架下,将材料体系特征与制备技术特点相融合的高强-高导铜基复合材料组织设计方法,发展出了颗粒与晶须增强相混杂、微米与纳米尺度增强相混杂、颗粒微团簇与纳米相协同的多级构型等设计策略,实现了强度与电导率的协同优化

关键词 : 铜基复合材料,  硼化物,  混杂增强,  多级构型    
Abstract:

Copper matrix composites exhibit excellent softening resistance at elevated temperatures. Therefore, they are promising electrically conductive materials for applications in demanding service environments. However, conventional copper matrix composites face a persistent tradeoff between mechanical strength and electrical conductivity. Therefore, to address this challenge, this study proposes a design strategy based on the precise control of in situ reaction timings during copper matrix composites fabrication via dual-beam melt mixing control technique, enabling the formation of reinforcements with multiple compositions, morphologies, and length scales. Considering the different processing characteristics of casting and powder metallurgy, copper matrix composites are designed and fabricated with hybrid and hierarchical reinforcement architectures. The strengthening efficiency of these reinforcements is improved via the synergistic effects of multitype and multiscale reinforcements, thereby overcoming the tradeoff between mechanical strength and electrical conductivity. Using copper matrix composites containing in situ-formed boride phases as a representative material system, this study systematically examines microstructural design principles for developing high-strength, high-conductivity materials. The analysis integrates the intrinsic characteristics of the Cu-boride system with the processing features of conventional metallic manufacturing routes, including casting and powder metallurgy. This study presents several design strategies, including the hybridization of particle and whisker reinforcements, hybridization of microscale and nanoscale reinforcements, and construction of hierarchical architectures comprising particle microclusters and nanoprecipitates. These strategies enable the simultaneous improvement of mechanical strength and electrical conductivity.

Key words: copper matrix composites    boride    hybrid reinforcement    hierarchical architecture
收稿日期: 2026-03-30     
ZTFLH:  TG146.1  
基金资助:国家自然科学基金项目(52127802);国家自然科学基金项目(52431008);国家自然科学基金项目(52322409)
通讯作者: 梁淑华,liangsh@xaut.edu.cn,主要从事铜基材料成型技术、结构功能一体化异质金属熔浸渗技术、难熔金属及粉末冶金技术等方面的研究
Corresponding author: LIANG Shuhua, professor, Tel: (029)82312185, E-mail: liangsh@xaut.edu.cn
作者简介: 梁淑华,女,1968年生,教授,博士,西安理工大学副校长。荣获全国创新争先奖状、国家百千万人才工程及有突出贡献中青年专家、中国青年科技奖等荣誉称号。科技部高等学校学科创新引智基地、教育部导电材料与复合技术工程研究中心等平台主任。主要从事先进铜材料设计与成型研究工作,面向国家重大工程中高端装备关键部件用铜材料寿命不足的共性难题,发明了耐烧、耐热、隔磁等不同功能系列铜材料,创制了铜/异质金属结构功能一体化部件成型技术,提出了原位制备铜基复合材料粉末的新方法,开发出复杂异形薄壁部件近净成形技术,系列产品应用于电力、航空、航天等领域。
图1  混杂增强铜基复合材料设计示意图
图2  通过反应铸造成形技术制备的颗粒与晶须混杂增强铜基复合材料[11~13]
图3  原位自生铜基复合材料粉末制备原理及其宏、微观特征[15,18]
图4  粉末冶金成形多级构型铜基复合材料的组织和性能[5,13,18,20]
[1] Yang K, Wang Y H, Guo M X, et al. Recent development of advanced precipitation-strengthened Cu alloys with high strength and conductivity: A review[J]. Prog. Mater. Sci., 2023, 138: 101141
doi: 10.1016/j.pmatsci.2023.101141
[2] Zhang Z F, Hou J P, Liu R, et al. Quantitative relationships between the strength-plasticity and strength-electrical conductivity of metallic materials[J]. Acta Metall. Sin., 2026, 62: 253
[2] 张哲峰, 侯嘉鹏, 刘 睿 等. 金属材料强度-塑性及强度-电导率定量关系[J]. 金属学报, 2026, 62: 253
doi: 10.11900/0412.1961.2025.00248
[3] Jiang Y H, Zhang X D, Cai P T, et al. Precipitation behavior and microstructural evolution during thermo-mechanical processing of precipitation hardened Cu-Hf based alloys[J]. Acta Mater., 2023, 245: 118659
doi: 10.1016/j.actamat.2022.118659
[4] Wang H, Min X M, Wang W M, et al. Quantum chemistry calculation on titanium diboride crystal[J]. Chin. J. Nonferrous Met., 2002, 12: 1229
[4] 王 皓, 闵新民, 王为民 等. 二硼化钛电子结构的量子化学计算[J]. 中国有色金属学报, 2002, 12: 1229
[5] Liang S H, Li W Z, Jiang Y H, et al. Microstructures and properties of hybrid copper matrix composites reinforced by TiB whiskers and TiB2 particles[J]. J. Alloys Compd., 2019, 797: 589
doi: 10.1016/j.jallcom.2019.05.129
[6] Zhang X D, Jiang Y H, Cao F, et al. Hybrid effect on mechanical properties and high-temperature performance of copper matrix composite reinforced with micro-nano dual-scale particles[J]. J. Mater. Sci. Technol., 2024, 172: 94
doi: 10.1016/j.jmst.2023.06.054
[7] Huang B, Duan Y H, Hu W C, et al. Structural, anisotropic elastic and thermal properties of MB (M = Ti, Zr and Hf) monoborides[J]. Ceram. Int., 2015, 41: 6831
doi: 10.1016/j.ceramint.2015.01.132
[8] Paul B, Okamoto N L, Kusakari M, et al. Plastic deformation of single crystals of CrB2, TiB2 and ZrB2 with the hexagonal AlB2 structure[J]. Acta Mater., 2021, 211: 116857
doi: 10.1016/j.actamat.2021.116857
[9] Jiang Y H, Li D, Liang S H, et al. Phase selection of titanium boride in copper matrix composites during solidification[J]. J. Mater. Sci., 2017, 52: 2957
doi: 10.1007/s10853-016-0592-2
[10] Xu Q, Zhang X H, Han J C, et al. Combustion synthesis and densification of titanium diboride-copper matrix composite[J]. Mater. Lett., 2003, 57: 4439
doi: 10.1016/S0167-577X(03)00338-0
[11] Pang Y H, Li P T, Jiang Y H, et al. First-principles calculations reveal two interface mechanisms to improve dispersion and strength of TiB2/Cu composites[J]. Mater. Lett., 2026, 409: 140159
doi: 10.1016/j.matlet.2026.140159
[12] Cao F, Zhang X D, Dong G Z, et al. Microstructures and properties of in situ (TiB2p + TiBw)/Cu composites with different Ce content[J]. Adv. Eng. Mater., 2022, 24: 2200251
doi: 10.1002/adem.v24.8
[13] Cao F, Dong G Z, Jiang Y H, et al. Effect of La addition on microstructures and properties of TiB2(-TiB)/Cu hybrid composites prepared by in situ reaction[J]. Mater. Sci. Eng., 2020, A789: 139605
[14] Ren J Q, Liang S H, Jiang Y H, et al. Research on the microstructure and properties of in situ (TiB2-TiB)/Cu composites[J]. Acta Metall. Sin., 2019, 55: 126
[14] 任建强, 梁淑华, 姜伊辉 等. 原位(TiB2-TiB)/Cu复合材料组织与性能研究[J]. 金属学报, 2019, 55: 126
doi: 10.11900/0412.1961.2017.00532
[15] Shi H, Zhao Y, Gao H B, et al. In-situ spherical TiB2/Cu composite powder: A new method of liquid phase reaction coupled with gas atomization[J]. Mater. Charact., 2022, 191: 112096
doi: 10.1016/j.matchar.2022.112096
[16] Perminov A, Bartzsch G, Franke A, et al. Manufacturing Fe-TiC composite powder via inert gas atomization by forming reinforcement phase in situ[J]. Adv. Eng. Mater., 2021, 23: 2000717
doi: 10.1002/adem.v23.3
[17] Li X G, Heisterüber L, Achelis L, et al. Multiscale descriptions of particle-droplet interactions in multiphase spray processing[J]. Int. J. Multiphase Flow, 2016, 80: 15
doi: 10.1016/j.ijmultiphaseflow.2015.10.013
[18] Shi H, Jiang Y H, Li P T, et al. A novel hierarchical structure of in-situ copper matrix composites reinforced with micro-clusters of TiB2 particles and nano-precipitates of B24Cu particles[J]. Composites, 2025, 297B: 112311
[19] Shi H, Cao F, Zhang H D, et al. Densification behavior, mechanical and electrical properties of in-situ TiB2p/Cu composite powder via vacuum hot pressing[J]. Mater. Charact., 2023, 202: 113004
doi: 10.1016/j.matchar.2023.113004
[20] Davis J R. ASM Specialty Handbook: Copper and Copper Alloys[M]. Materials Park: ASM International, 2001: 1
[1] 吴洲, 吴凡, 王一茗, 甘有良, 付雪松, 陈国清, 周文龙, 祖宇飞. Mo表面硅化物-硼化物复合涂层的微观组织与高温氧化行为[J]. 金属学报, 2026, 62(6): 1069-1081.
[2] 姜伊辉, 张兴德, 石浩, 曹飞, 马文君, 王艳芳, 梁淑华. 先进导电铜基复合材料设计与制备研究进展[J]. 金属学报, 2026, 62(2): 289-308.
[3] 赵乃勤, 郭斯源, 张翔, 何春年, 师春生. 基于增强相构型设计的石墨烯/Cu复合材料研究进展[J]. 金属学报, 2021, 57(9): 1087-1106.
[4] 王希,刘仁慈,曹如心,贾清,崔玉友,杨锐. 冷却速率对β凝固γ-TiAl合金硼化物和室温拉伸性能的影响[J]. 金属学报, 2020, 56(2): 203-211.
[5] 王慧远,李超,李志刚,徐进,韩洪江,管志平,宋家旺,王珵,马品奎. 纳米增强体强化轻合金复合材料制备及构型设计研究进展与展望[J]. 金属学报, 2019, 55(6): 683-691.
[6] 任建强, 梁淑华, 姜伊辉, 杜翔. 原位(TiB2-TiB)/Cu复合材料组织与性能研究[J]. 金属学报, 2019, 55(1): 126-132.
[7] 马秀良, 胡肖兵. 高温合金中硼化物精细结构的高空间分辨电子显微学研究[J]. 金属学报, 2018, 54(11): 1503-1524.
[8] 丁贤飞,刘东方,郑运荣,冯强. B微合金化对HK40合金铸造疏松的影响[J]. 金属学报, 2015, 51(9): 1121-1128.
[9] 杨莉莉 郑立静 肖志霞 闫洁 张虎. 抽拉速率对定向凝固Ti-47Al-2Cr-2Nb-0.8B合金组织的影响[J]. 金属学报, 2010, 46(7): 879-884.
[10] 刘仲礼; 李言祥; 陈祥; 胡开华 . 高硼铁基合金在不同铸型中凝固组织与力学性能的影响[J]. 金属学报, 2007, 43(5): 477-481 .
[11] 符寒光; 蒋志强 . 耐磨铸造Fe-B-C合金的研究[J]. 金属学报, 2006, 42(5): 545-548 .
[12] 胡坚;林一坚;许嘉龙;张士勋. Nb对液态激冷Fe_(70)Cr_(18)Mo_2B_9Si_1合金组织及性能的影响[J]. 金属学报, 1993, 29(7): 85-88.
[13] 蒋百灵;雷廷权. 渗硼层生长的控制因素及其动力学过程分析[J]. 金属学报, 1991, 27(1): 11-15.