| 中碳Nb合金化钢液析碳化物的析出行为 |
梁炫1,2, 侯廷平1,2( ), 张东1,2, 谭昕暘1,2, 吴开明1,2( ) |
1 武汉科技大学 省部共建耐火材料与冶金国家重点实验室 武汉 430081 2 武汉科技大学 高性能钢铁材料及其应用省部共建协同创新中心 武汉 430081 |
|
| Precipitation Behavior of Primary Carbides in Medium Carbon Nb-Alloyed Steel |
LIANG Xuan1,2, HOU Tingping1,2( ), ZHANG Dong1,2, TAN Xinyang1,2, WU Kaiming1,2( ) |
1 State Key Laboratory of Refractories and Metallury, Wuhan University of Science and Technology, Wuhan 430081, China 2 Hubei Collaborative Innovation Center for Advanced Steels, Wuhan University of Science and Technology, Wuhan 430081, China |
引用本文:
梁炫, 侯廷平, 张东, 谭昕暘, 吴开明. 中碳Nb合金化钢液析碳化物的析出行为[J]. 金属学报, 2025, 61(4): 653-664.
Xuan LIANG,
Tingping HOU,
Dong ZHANG,
Xinyang TAN,
Kaiming WU.
Precipitation Behavior of Primary Carbides in Medium Carbon Nb-Alloyed Steel[J]. Acta Metall Sin, 2025, 61(4): 653-664.
| 1 |
Yang Y. All-optical photodetector based on photothermal effect of MXene Nb2CT x [D]. Tianjin: Tianjin University of Technology, 2022
|
| 1 |
杨 洋. 基于碳化铌光热效应的全光探测器的研究 [D]. 天津: 天津理工大学, 2022
|
| 2 |
Chu S J, Mao B, Hu G K. Microstructure control and strengthening mechanism of high strength cold rolled dual phase steels for automobile applications [J]. Acta Metall. Sin., 2022, 58: 551
doi: 10.11900/0412.1961.2022.00061
|
| 2 |
储双杰, 毛 博, 胡广魁. 汽车用先进高强度冷轧双相钢的显微组织调控和强韧化机理 [J]. 金属学报, 2022, 58: 551
doi: 10.11900/0412.1961.2022.00061
|
| 3 |
Li Z Y, Li C R, Zeng Z Y, et al. Thermodynamic study of carbide and nitride precipitation of niobium in 500 MPa high-strength anti-seismic rebars [J]. J. Iron Steel Res., 2020, 32: 727
|
| 3 |
黎志英, 李长荣, 曾泽芸 等. 高强抗震钢筋中铌的碳、氮化物析出热力学研究 [J]. 钢铁研究学报, 2020, 32: 727
doi: 10.13228/j.boyuan.issn1001-0963.20190238
|
| 4 |
Zhou J, Hu C Y, Hu F, et al. Insight into the effect of Nb microalloying on the microstructure-property relationship of a novel wire rod [J]. J. Mater. Res. Technol., 2022, 16: 276
doi: 10.1016/j.jmrt.2021.11.144
|
| 5 |
Su X, Wang H X, Zhu M, et al. In-situ observation for effect of niobium on pearlite transformation in high-carbon steels [J]. Iron Steel, 2022, 57(4): 88
|
| 5 |
苏 雪, 王厚昕, 朱 敏 等. 原位观察铌对高碳钢珠光体相变的影响 [J]. 钢铁, 2022, 57(4): 88
|
| 6 |
Tian J Y, Wang H X, Zhu M, et al. Improving mechanical properties in high-carbon pearlitic steels by replacing partial V with Nb [J]. Mater. Sci. Eng., 2022, A834: 142622
|
| 7 |
Zhang Y, Li X X, Wei K, et al. Element segregation in GH4169 superalloy large-scale ingot and billet manufactured by triple-melting [J]. Acta Metall. Sin., 2020, 56: 1123
doi: 10.11900/0412.1961.2020.00101
|
| 7 |
张 勇, 李鑫旭, 韦 康 等. 三联熔炼GH4169合金大规格铸锭与棒材元素偏析行为 [J]. 金属学报, 2020, 56: 1123
|
| 8 |
Xie Y, Cheng G G, Chen L, et al. Characteristics and generating mechanism of large precipitates in Nb-Ti-microalloyed H13 tool steel [J]. ISIJ Int., 2016, 56: 995
|
| 9 |
Jiang Q C, Sui H L, Guan Q F. Thermal fatigue behavior of new type high-Cr cast hot work die steel [J]. ISIJ Int., 2004, 44: 1103
|
| 10 |
Tchuindjang J T, Lecomte-Beckers J. Fractography survey on high cycle fatigue failure: Crack origin characterisation and correlations between mechanical tests and microstructure in Fe-C-Cr-Mo-X alloys [J]. Int. J. Fatigue, 2007, 29: 713
|
| 11 |
Jang J H, Lee C H, Heo Y U, et al. Stability of (Ti, M)C (M = Nb, V, Mo and W) carbide in steels using first-principles calculations [J]. Acta Mater., 2012, 60: 208
|
| 12 |
Fang C M, van Huis M A, Zandbergen H W. Structural, electronic, and magnetic properties of iron carbide Fe7C3 phases from first-principles theory [J]. Phys. Rev., 2009, 80B: 224108
|
| 13 |
Zhang D, Zheng H, Hou T P, et al. Hardness increases due to (Fe, Cr)2C carbide precipitated during natural aging in high chromium cast iron [J]. Vacuum, 2023, 209: 111766
|
| 14 |
Klymko T, Sluiter M H F. Computing solubility products using ab initio methods precipitation of NbC in low alloyed steel [J]. J. Mater. Sci., 2012, 47: 7601
|
| 15 |
Arroyave R, Shin D, Liu Z K. Ab initio thermodynamic properties of stoichiometric phases in the Ni-Al system [J]. Acta Mater., 2005, 53: 1809
|
| 16 |
Shang S L, Wang Y, Kim D, et al. First-principles thermodynamics from phonon and Debye model: Application to Ni and Ni3Al [J]. Comput. Mater. Sci., 2010, 47: 1040
|
| 17 |
Voller V R. Modeling micro scale phenomena for application in solidification process simulations [A]. Proceedings of the Second International Conference on Processing Materials for Properties [C]. San Francisco: TMS, 2000: 1011
|
| 18 |
Scheil E. Bemerkungen zur Schichtkristallbildung [J]. Int. J. Mater. Res., 1942, 34(3): 70
|
| 19 |
Brody H D, Flemings M C. Solute redistribution in dendritic solidification [J]. Trans. Met. Soc. AJIME, 1966, 236: 615
|
| 20 |
Ohnaka I. Mathematical analysis of solute redistribution during solidification with diffusion in solid phase [J]. Trans. ISIJ, 1986, 26: 1045
|
| 21 |
Clyne T W, Kurz W. Solute redistribution during solidification with rapid solid state diffusion [J]. Metall. Trans., 1981, 12A: 965
|
| 22 |
Voller V R, Beckermann C. Approximate models of microsegregation with coarsening [J]. Metall. Mater. Trans., 1999, 30A: 3016
|
| 23 |
Voller V R, Beckermann C. A unified model of microsegregation and coarsening [J]. Metall. Mater. Trans., 1999, 30A: 2183
|
| 24 |
Liang X, Hou T P, Zhang D, et al. New evaluation of the thermodynamics stability for bcc-Fe [J]. J. Phys.: Condens. Matter., 2022, 34: 455801
|
| 25 |
Otero-de-la-Roza A, Luaña V. GIBBS2: A new version of the quasi-harmonic model code. I. Robust treatment of the static data [J]. Comput. Phys. Commun., 2011, 182: 1708
|
| 26 |
Otero-de-la-Roza A, Abbasi-Pérez D, Luaña V. GIBBS2: A new version of the quasiharmonic model code. II. Models for solid-state thermodynamics, features and implementation [J]. Comput. Phys. Commun., 2011, 182: 2232
|
| 27 |
Wolverton C, Zunger A. First-principles theory of short-range order, electronic excitations, and spin polarization in Ni-V and Pd-V alloys [J]. Phys. Rev., 1995, 52B: 8813
|
| 28 |
Kresse G, Furthmüller J. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set [J]. Comput. Mater. Sci., 1996, 6: 15
|
| 29 |
Blöchl P E. Projector augmented-wave method [J]. Phys. Rev., 1994, 50B: 17953
|
| 30 |
Togo A, Tanaka I. First principles phonon calculation in materials science [J]. Scr. Mater., 2015, 108: 1
|
| 31 |
Guo W, Long M J, Wu J L, et al. Effect of solute partition coefficient and TiN precipitation on micro-segregation of 22MnB5 steel [J]. Iron Steel, 2022, 57(3): 44
|
| 31 |
郭 伟, 龙木军, 吴家璐 等. 22MnB5钢溶质分配系数及TiN析出对微观偏析的影响 [J]. 钢铁, 2022, 57(3): 44
|
| 32 |
Won Y M, Thomas B G. Simple model of microsegregation during solidification of steels [J]. Metall. Mater. Trans., 2001, 32A: 1755
|
| 33 |
Fu Y X, Zhu L G, Sun L G, et al. Calculation of high temperature solidification characteristics and high temperature physical properties of high strength steel containing niobium [J]. Steelmaking, 2020, 36(2): 34
|
| 33 |
付雨潇, 朱立光, 孙立根 等. 含Nb高强钢高温凝固特性与物性参数的计算 [J]. 炼钢, 2020, 36(2): 34
|
| 34 |
Chen M W, Wang Z D. The evolution and morphological stability of a particle in a binary alloy melt [J]. J. Cryst. Growth, 2023, 607: 127113
|
| 35 |
Villars P, Calvet L D. Pearson's Handbook of Crystallographic Data for Intermetallic Phases [M]. Metals Park: American Society for Metals, 1985: 1
|
| 36 |
Nartowski A M, Parkin I P, MacKenzie M, et al. Solid state metathesis routes to transition metal carbides [J]. J. Mater. Chem., 1999, 9: 1275
|
| 37 |
Singh D J, Klein B M. Electronic structure, lattice stability, and superconductivity of CrC [J]. Phys. Rev., 1992, 46B: 14969
|
| 38 |
Zhao C C, Xing X L, Guo J, et al. Micro-properties of (Nb, M)C carbide (M = V, Mo, W and Cr) and precipitation behavior of (Nb, V)C in carbide reinforced coating [J]. J. Alloys Compd., 2019, 788: 852
|
| 39 |
Wang R, Wang S F, Wu X Z. Ab initio study of the thermodynamic properties of rare-earth-magnesium intermetallics MgRE (RE = Y, Dy, Pr, Tb) [J]. Phys. Scr., 2011, 83: 065707
|
| 40 |
Gui L T, Long M J, Huang Y W, et al. Effects of inclusion precipitation, partition coefficient, and phase transition on microsegregation for high-sulfur steel solidification [J]. Metall. Mater. Trans., 2018, 49B: 3280
|
| 41 |
Zhang X W, Zhang L F, Yang W, et al. Thermodynamics and dynamics of MnS inclusions precipitation during solidification process in heavy rail steels [J]. Iron Steel, 2016, 51(9): 30
|
| 41 |
张学伟, 张立峰, 杨 文 等. 重轨钢中MnS析出热力学和动力学分析 [J]. 钢铁, 2016, 51(9): 30
doi: 10.13228/j.boyuan.issn0449-749x.20160079
|
| 42 |
Chen J X. Data Manual of Common Steelmaking Charts [M]. Beijing: Metallurgical Industry Press, 1984: 565
|
| 42 |
陈家祥. 炼钢常用图表数据手册 [M]. 北京: 冶金工业出版社, 1984: 565
|
| 43 |
Liu Z Z, Wei J, Cai K K. A coupled mathematical model of microsegregation and inclusion precipitation during solidification of silicon steel [J]. ISIJ Int., 2002, 42: 958
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|