|
|
|
| Al-Mn系合金的组织控制与高温性能研究 |
刘贤翠, 潘冶( ), 唐智骄, 何为桥, 陆韬 |
| 东南大学材料科学与工程学院江苏省先进金属材料高技术研究重点实验室 南京 211189 |
|
| Microstructure Control and High Temperature Properties of Al-Mn-Based Alloys |
Xiancui LIU, Ye PAN( ), Zhijiao TANG, Weiqiao HE, Tao LU |
| Jiangsu Key Laboratory for Advanced Metallic Materials, School of Materials Science and Engineering, Southeast University, Nanjing 211189, China |
引用本文:
刘贤翠, 潘冶, 唐智骄, 何为桥, 陆韬. Al-Mn系合金的组织控制与高温性能研究[J]. 金属学报, 2017, 53(11): 1487-1494.
Xiancui LIU,
Ye PAN,
Zhijiao TANG,
Weiqiao HE,
Tao LU.
Microstructure Control and High Temperature Properties of Al-Mn-Based Alloys[J]. Acta Metall Sin, 2017, 53(11): 1487-1494.
| [1] | Li G Q, Zuo X R, Song T F, et al.Application situation and progress of wrought Al-Mn alloy[J]. Hot Working Technol., 2006, 35(5): 63(李广钦, 左秀荣, 宋天福等. 变形铝锰系合金的应用现状及发展动态[J]. 热加工工艺, 2006, 35(5): 63) | | [2] | Chris Co., LTD. Materials of Al alloy used in radiator [P].Chin Pat, 02821519.2, 2005(克里斯有限公司. 用于制造散热片材料的铝合金 [P].中国专利, 02821519.2, 2005) | | [3] | Fukumoto A, Niikura A, Negura K, et al.Aluminum alloy brazing sheet [P]. US Pat, 20070166565A1, 2010 | | [4] | Yun S C, Kim K S, Euh K J.Effect of intermediate heat treatment on the mechanical properties of 3003/4343 aluminum clad sheet manufactured by strip casting/clad rolling[J]. Mater. Trans., 2015, 56: 242 | | [5] | Kahl S, Ekstr?m H E, Mendoza J.Tensile, fatigue, and creep properties of aluminum heat exchanger tube alloys for temperatures from 293 K to 573 K (20 ℃ to 300 ℃)[J]. Metall. Mater. Trans., 2013, 45A: 663 | | [6] | Northwood D O, Smith I O.Stress change tests during the steady state creep of aluminum alloy 3004 at 300 ℃[J]. Mater. Sci. Eng., 1986, A79: 175 | | [7] | Liu K, Chen X G.Development of Al-Mn-Mg 3004 alloy for applications at elevated temperature via dispersoid strengthening[J]. Mater. Des., 2015, 84: 340 | | [8] | Tangen S, Sj?lstad K, Furu T, et al.Effect of concurrent precipitation on recrystallization and evolution of the p-texture component in a commercial Al-Mn alloy[J]. Metall. Mater. Trans., 2010, 41A: 2970 | | [9] | Dehmas M, Aeby-Gautier E, Archambault P, et al.Interaction between eutectic intermetallic particles and dispersoids in the 3003 aluminum alloy during homogenization treatments[J]. Metall. Mater. Trans., 2013, 44A: 1059 | | [10] | Li Y J, Arnberg L.Quantitative study on the precipitation behavior of dispersoids in DC-cast AA3003 alloy during heating and homogenization[J]. Acta Mater., 2003, 51: 3415 | | [11] | Tu Y Y, Qian H, Zhou X F, et al.Effect of scandium on the interaction of concurrent precipitation and recrystallization in commercial AA3003 aluminum alloy[J]. Metall. Mater. Trans., 2014, 45A: 1883 | | [12] | Zhang J.Effect of rolling and annealing process on properties of 4343/3003/7072 layered aluminum foil [D]. Changsha: Central South University, 2013(张静. 轧制及退火工艺对4343/3003/7072钎焊箔性能的影响 [D]. 长沙: 中南大学, 2013) | | [13] | Copper M, Robinson K.The crystal structure of the ternary alloy α-AlMnSi[J]. Acta Crystallogr., 1966, 20: 614 | | [14] | Poková M ?, Zimina M, Cieslar M.Effect of pre-annealing on microstructure evolution of TRC AA3003 aluminum alloy subjected to ECAP[J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 627 | | [15] | Zhang J S.High Temperature Deformation and Fracture of Materials [M]. Beijing: Science Press, 2007: 4(张俊善. 材料的高温变形与断裂 [M]. 北京: 科学出版社, 2007: 4) | | [16] | Casting and Smelting of Non-Ferrous Alloys Joint Editorial. Casting and Smelting of Non-ferrous Alloys [M]. Beijing: National Defence Industry Press, 1980: 186(《铸造有色合金及其熔炼》联合编写组. 铸造有色合金及其熔炼 [M]. 北京: 国防工业出版社, 1980: 186) | | [17] | Kim W J, Chung S W, Chung C S, et al.Superplasticity in thin magnesium alloy sheets and deformation mechanism maps for magnesium alloys at elevated temperatures[J]. Acta Mater., 2001, 49: 3337 | | [18] | Yan J L, Sun Y S, Xue F, et al.An investigation on the creep behavior of pure magnesium[J]. Acta Metall. Sin., 2008, 44: 1354(晏井利, 孙扬善, 薛峰等. 纯Mg的蠕变行为研究[J]. 金属学报, 2008, 44: 1354) | | [19] | Kaufman J G.Properties of Aluminum Alloys: Tensile, Creep, and Fatigue Data at High and Low Temperatures[M]. Materials Park, Ohio: ASM International, 2000: 93 | | [20] | Meng Q E, Xi X R.Correlation between stacking fault energy and creep property of solid solution strengthening superalloys[J]. Acta Metall. Sin., 1987, 23: 344(孟庆恩, 郗秀荣. 固溶强化高温合金堆垛层错能与高温蠕变性能的关系[J]. 金属学报, 1987, 23: 344) | | [21] | Somekawa H, Hirai K, Watanabe H, et al.Dislocation creep behavior in Mg-Al-Zn alloys[J]. Mater. Sci. Eng., 2005, A407: 53 | | [22] | Chung S W, Watanabe H, Kim W J.Creep deformation mechanisms in coarse-grained solid solution Mg alloys[J]. Mater. Trans., 2004, 45: 1266 | | [23] | Luiggi N.Isochronal study of Al-Mg, Al-Mn and Al-Mn-0.3Mg alloys using electrical resistivity and thermoelectric power[J]. Mater. Res., 2005, 8(1): 31 | | [24] | Du X D.Study on ageing and creep of Al-0.1Zr alloy[J]. Mater. Sci. Eng., 2006, A423: 84 | | [25] | Miresmaeili S M, Nami B.Impression creep behavior of Al-1.9%Ni-1.6%Mn-1%Mg alloy[J]. Mater. Des., 2014, 56: 286 | | [26] | Sun C Y, Shi B, Wu C B, et al.High temperature creep deformation mechanism of BSTMUF601 superalloy[J]. Acta Metall. Sin., 2015, 51: 349(孙朝阳, 石兵, 武传标等. BSTMUF601合金的高温蠕变变形机制[J]. 金属学报, 2015, 51: 349) | | [27] | Forbord B, Hallem H, Ryum N, et al.Precipitation and recrystallisation in Al-Mn-Zr with and without Sc[J]. Mater. Sci. Eng., 2004, A387: 936 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|