| Zn/CuxTiy体系固态反应周期层片型结构研究* |
巩宇1,2,3,陈永翀1( ),刘丹丹1,张艳萍1,3,CSERHÁTICsaba4,CSIKAttila5 |
1 中国科学院电工研究所, 北京 100190
2 中国科学院大学, 北京 100049
3 北京好风光储能技术有限公司, 北京 100085
4 Department of Solid State Physics, University of Debrecen, H-4010 Debrecen, Hungary
5 Institute for Nuclear Research, Hungarian Academy of Sciences, H-4001 Debrecen, Hungary |
|
| INVESTIGATION OF PERIODIC-LAYERED STRUCTURE DURING SOLID STATE REACTIONS OF Zn/CuxTiy SYSTEMS |
Yu GONG1,2,3,Yongchong CHEN1( ),Dandan LIU1,Yanping ZHANG1,3,Csaba CSERHÁTI4,Attila CSIK5 |
1 Institute of Electrical Engineering, Chinese Academy of Sciences, Beijing 100190, China
2 University of Chinese Academy of Sciences, Beijing 100049, China
3 Beijing HAWAGA Power Storage Technology Company Ltd., Beijing 100085, China
4 Department of Solid State Physics, University of Debrecen, H-4010 Debrecen, Hungary
5 Institute for Nuclear Research, Hungarian Academy of Sciences, H-4001 Debrecen, Hungary |
引用本文:
巩宇, 陈永翀, 刘丹丹, 张艳萍, CSERHÁTICsaba, CSIKAttila. Zn/CuxTiy体系固态反应周期层片型结构研究*[J]. 金属学报, 2016, 52(3): 349-354.
Yu GONG,
Yongchong CHEN,
Dandan LIU,
Yanping ZHANG,
Csaba CSERHáTI,
Attila CSIK.
INVESTIGATION OF PERIODIC-LAYERED STRUCTURE DURING SOLID STATE REACTIONS OF Zn/CuxTiy SYSTEMS[J]. Acta Metall Sin, 2016, 52(3): 349-354.
| [1] | Osinki K, Vriend A W, Bastin G F, van Loo F J J.Z Metallkde, 1982; 73: 258 | | [2] | van Loo F J J, Osinski K. In: Purdy G R ed., Periodic Structures in Multicomponent Diffusion Couples. Oxford: Pergamon Press, 1990: 109 | | [3] | Rijnders M R, van Loo F J J.Scr Metall Mater, 1995; 32: 1931 | | [4] | He M, Su X P, Yin F C,Wang J H, Li Z.Scr Mater, 2008; 59: 411 | | [5] | Su X P, Liu C, Yin F C,Wang J H.Scr Mater, 2010; 62: 485 | | [6] | Schiepers R C J, van Beek J A, van Loo F J J, De With G.J Eur Ceram Soc, 1993; 11: 211 | | [7] | Dunaev S F, Zver'kov S A.J Less-Common Met, 1989; 153: 143 | | [8] | Rijnders M R, Kodentsov A A, van Beek J A, van Den Akker J, van | | [8] | Loo F J J.Solid State Ionics, 1997; 95: 51 | | [9] | Chou T C, Joshi A, Wordsworth J.J Mater Res,1991; 6: 796 | | [10] | Rijnders M R, Kodentsov A A, van Beek J A, van den Akker J, van Loo F J J.Solid State Ionics, 1997; 95: 51 | | [11] | Rijnders M R, Kodentsov A A, Cserháti C, van den Akker J, van Loo F J J. Defect Diff Forum, 1996; 129-130: 253 | | [12] | Gutman I, Klinger L, Gotman I, Shapiro M.Scr Mater, 2001; 45: 363 | | [13] | He M, Su X P, Yin F C, Wang J H, Li Z.Scr Mater, 2008; 59: 411 | | [14] | Mazaudier F, Proye C, Hodaj F.J Nucl Mater, 2008; 377: 476 | | [15] | Oberhausera S, Strobla C H, Schreiberb G, Wuestefeldb C H, Rafajab D.Surf Coat Technol, 2010; 204: 2307 | | [16] | Lin S, Tsai M, Tsai P, Hsu B.Sci Reports, 2014; 4: 514 | | [17] | Chen Y C, Zhang X F, Li Y J, Ren Y K.Mater Lett, 2012; 85: 142 | | [18] | Chen Y C, Zhang X F, Han L, Du Z W.Mater Lett, 2012; 76: 151 | | [19] | Kodentsov A A, Rijnders M R, van Loo F J J. Acta Mater, 1998; 46: 6521 | | [20] | Chen Y C, Zhang Y G, Chen C Q.Mater Sci Eng, 2003; A362: 135 | | [21] | Kao C R, Chang Y A.Acta Metall Mater, 1993; 41: 3463 | | [22] | Klinger L, Gotman I, Gutman I.Scr Mater, 2001; 45: 1221 | | [23] | Gutman I, Gotman I, Shapiro M.Acta Mater, 2006; 54: 4677 | | [24] | Gutman I, Klinger L, Gotman I, Shapiro M.Solid State Ionics, 2009; 180: 1350 | | [25] | Chen Y C, Zhang Y G, Chen C Q.Mater Sci Eng, 2004; A368: 1 | | [26] | Chen Y C, Xu J, Fan X H, Zhang X F, Han L, Lin D Y, Li Q H, Uher C.Intermetallics, 2009; 17: 920 | | [27] | Tang R Z, Tian R Z.Binary Alloy Phase Diagams and Crystal Structure of Intermediate Phase. Changsha: Central South University Press, 2009: 1 | | [27] | (唐仁政, 田荣璋. 二元合金相图及中间相晶体结构. 长沙: 中南大学出版社, 2009: 1) | | [28] | Wu C J, Zhu C L, Su X P, Liu Y, Peng H P, Wang J H.Acta Metall Sin, 2014; 50: 930 | | [28] | (吴长军, 朱晨露, 苏旭平, 刘亚, 彭浩平, 王建华. 金属学报, 2014; 50: 930) |
|
|