| 93W-5.6Ni-1.4Fe高比重合金放电等离子主烧结曲线的建立* |
胡可, 李小强( ), 屈盛官, 杨超, 李元元 |
| 华南理工大学国家金属材料近净成形工程技术研究中心, 广州 510640 |
|
| DEVELOPMENT OF MASTER SINTERING CURVE FOR SPARK PLASMA SINTERING OF 93W-5.6Ni-1.4Fe HEAVY ALLOY |
HU Ke, LI Xiaoqiang( ), QU Shengguan, YANG Chao, LI Yuanyuan |
| National Engineering Research Center of Near-Net-Shape Forming for Metallic Materials, South China University of Technology, Guangzhou 510640 |
引用本文:
胡可, 李小强, 屈盛官, 杨超, 李元元. 93W-5.6Ni-1.4Fe高比重合金放电等离子主烧结曲线的建立*[J]. 金属学报, 2014, 50(6): 727-736.
Ke HU,
Xiaoqiang LI,
Shengguan QU,
Chao YANG,
Yuanyuan LI.
DEVELOPMENT OF MASTER SINTERING CURVE FOR SPARK PLASMA SINTERING OF 93W-5.6Ni-1.4Fe HEAVY ALLOY[J]. Acta Metall Sin, 2014, 50(6): 727-736.
| [1] |
Su H, Johnson D L. J Am Ceram Soc, 1996; 79: 3211
|
| [2] |
Hansen J D, Rusin R P, Teng M, Johnson D L. J Am Ceram Soc, 1992; 75: 1129
|
| [3] |
Ewsuk K G, Ellerbyz D T, DiAntonio C B. J Am Ceram Soc, 2006; 89: 2003
|
| [4] |
Kutty T R G, Khan K B, Hegde P V, Banerjee J, Sengupta A K, Majumdar S, Kamath H S. J Nucl Mater, 2004; 327: 211
|
| [5] |
Mazaheri M, Simchi A, Dourandish M. Golestani-Fard F. Ceram Int, 2009; 35: 547
|
| [6] |
Blaine D C, Gurosik J D, Park S J, German R M, Heaney D F. Metall Mater Trans, 2006; 37A: 715
|
| [7] |
Park S J, Martin J M, Guo J F, Johnson L J, German R M. Metall Mater Trans, 2006; 37A: 2837
|
| [8] |
Blaine D C, Park S J, German R M, Suri P. Metall Mater Trans, 2006; 37A: 2827
|
| [9] |
Marković S, Uskoković D. J Eur Ceram Soc, 2009; 29: 2309
|
| [10] |
An K, Johnson D L. J Mater Sci, 2002; 37: 4555
|
| [11] |
An K, Han M K. Mater Sci Eng, 2005; A391: 66
|
| [12] |
Guillon O, Langer J. J Mater Sci, 2010; 45: 5191
|
| [13] |
Enneti R K, Bothara M G, Park S J, Atre S V. Ceram Int, 2012; 38: 4369
|
| [14] |
Hong S H, Ryu H J. Mater Sci Eng, 2003; A344: 253
|
| [15] |
Zhu Y B, Wang Y, Zhang X Y, Qin G W. Int J Refract Met Hard Mater, 2007; 25: 275
|
| [16] |
German R M. Sinteing Theory and Practice. New York: John Wiley & Sons, 1996: 78
|
| [17] |
Hu K, Li X Q, Qu S G, Li Y Y. Metall Mater Trans, 2013; 44A: 923
|
| [18] |
Hu K, Li X Q, Qu S G, Li Y Y. Metall Mater Trans, 2013; 44A: 4323
|
| [19] |
Räthel J, Herrmann M, Beckert W. J Eur Ceram Soc, 2009; 29: 1419
|
| [20] |
Zavaliangos A, Zhang J, Krammer M, Groza J R. Mater Sci Eng, 2004; A379: 218
|
| [21] |
Zhang J. PhD Dissertation, Drexel University, Philadelphia, 2004
|
| [22] |
Vanmeensel K, Laptev A, Hennicke J, Vleugels J, Van der Biest O. Acta Mater, 2005; 53: 4379
|
| [23] |
Wang X, Casolco S R, Xu G, Garay J E. Acta Mater, 2007; 55: 3611
|
| [24] |
Anselmi-Tamburini U, Gennari S, Garay J E, Munir Z A. Mater Sci Eng, 2005; A394: 139
|
| [25] |
Langer J, Hoffmann M J, Guillon O. Acta Mater, 2009; 57: 5454
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|