金属学报  2014, Vol. 50 Issue (12): 1491-1497    DOI: 10.11900/0412.1961.2014.00251
  本期目录 | 过刊浏览 |
基于三维数字图像相关法的5456铝镁合金锯齿形屈服研究
蔡玉龙1, 符师桦1, 王玉辉1, 田成刚2, 高越1, 程腾1, 张青川1()
1 中国科学技术大学近代力学系中国科学院材料力学行为和设计重点实验室, 合肥 230027
2 中国科学院金属研究所, 沈阳 110016
SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION
CAI Yulong1, FU Shihua1, WANG Yuhui1, TIAN Chenggang2, GAO Yue1, CHENG Teng1, ZHANG Qingchuan1()
1 Chinese Academy Sciences Key Laboratory of Mechanical Behavior and Design of Materials, University of Science and Technology of China, Hefei 230027
2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
引用本文:

蔡玉龙, 符师桦, 王玉辉, 田成刚, 高越, 程腾, 张青川. 基于三维数字图像相关法的5456铝镁合金锯齿形屈服研究[J]. 金属学报, 2014, 50(12): 1491-1497.
Yulong CAI, Shihua FU, Yuhui WANG, Chenggang TIAN, Yue GAO, Teng CHENG, Qingchuan ZHANG. SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION[J]. Acta Metall Sin, 2014, 50(12): 1491-1497.

全文: PDF(1683 KB)   HTML
摘要: 

利用三维数字图像相关技术研究了常温下不同厚度5456铝镁合金板状试件在加载过程中的锯齿形屈服现象及其变形分布. 统计分析锯齿跌落幅值和周期发现, 2者均随应变增大而增大, 且锯齿周期随厚度增大而增大, 而锯齿幅值与厚度相关性较弱. 在拉伸方向应变场和离面位移场中观察到了Portevin-Le Chatelier (PLC)带, PLC带宽不随应力跌落幅值变化而变化, 随试件厚度增大而增大; PLC带倾角与应力跌落幅值、试件厚度无关, 约为60°. 将锯齿幅值和变形信息相联系, 获得了锯齿幅值与带内最大应变成正比关系这一规律. 通过变形时域分析发现, PLC带引起局部拉伸方向应变突增的同时, 也引起相同区域离面位移的突变.

关键词 : 5456铝镁合金,  三维数字图像相关法,  锯齿屈服,  动态应变时效    
Abstract:

One of the key issues to deeply understand the intrinsic mechanism of Portevin-Le Chatelier (PLC) phenomenon is to analyze the spatial distribution and the evolution of the deformation in PLC bands, associated with serrated yielding. In this work, an investigation was carried out with 5456 aluminium magnesium alloy sheet specimens of different thicknesses at room temperature by using three dimensional digital image correlation (3D-DIC) method, which focused itself on the deformation analysis within serrated yielding under different loading procedures. After statistically analyzing loading curves, it is found that the average amplitude and average period increase with increasing strain. Moreover, there is a positive correlation between the average period and the thickness of specimen, while the average amplitude and the thickness of specimen are independent to some degree. In addition, the experimental result also indicates that the width of the PLC band increases with increasing thickness of the specimen. However, the spatial analysis in PLC bands proves that the angle between the PLC band and the tensile direction is about 60°, which is irrelevant to the specimen thickness and the serration amplitude. Furthermore, it is also found that PLC bands of out-of-plane displacement coincide with bands of strain in the tensile direction by temporal analysis. Most importantly, the experimental result shows that the serration amplitude is proportional to the maximum strain in PLC band when PLC band occurs.

Key words: 5456 aluminium magnesium alloy    three dimensional digital image correlation    serrated yielding    dynamic strain aging
    
ZTFLH:  O348.1  
基金资助:* 国家自然科学基金项目11332010, 51271174和11372300及中央高校基本科研业务费专项资金项目WK2090050029资助
作者简介: null

蔡玉龙, 男, 1989年生, 硕士生

图1  不同厚度5456铝镁合金试件的名义应力-应变曲线
图2  不同厚度5456铝镁合金试件应力跌落幅值与锯齿周期随应变变化关系
图3  3种厚度5456铝镁合金试件的锯齿跌落及相应的PLC带
图4  PLC带倾角和带宽计算示意图
图5  3种厚度试件PLC带夹角与PLC带宽随应力跌落幅值的变化关系
图6  3种厚度5456铝镁合金试件应力跌落幅值与带内最大应变的关系
图7  3 mm试件上P1, P2, P3 3点拉伸方向应变及离面位移随时间变化关系
[1] Cottrell A H. Philos Mag, 1953; 44: 829
[2] Cieslar M, Fressengeas C, Karimi A, Martin J L. Scr Mater, 2003; 48: 1105
[3] Nagarjuna S, Anozie F N, Evans J T. Mater Sci Technol, 2003; 19: 1661
[4] Lu J Y, Jiang Z Y, Zhang Q C. Acta Metall Sin, 2006; 42: 139
[4] (卢俊勇, 蒋震宇, 张青川. 金属学报, 2006; 42: 139)
[5] Sleeswyk A W. Acta Metall, 1958; 6: 598
[6] Mulford R A, Kocks U F. Acta Metall, 1979; 27: 1125
[7] McCormick P G. Acta Metall, 1988; 36: 3061
[8] Springer F, Nortmann A, Schwink C. Phys Status Solidi, 1998; 170A: 63
[9] Klose F B, Ziegenbein A, Weidenmuller J, Neuhauser H, Hahner P. Comput Mater Sci, 2003; 26: 80
[10] Wang C, Xu Y B, Han E-H. Acta Metall Sin, 2006; 42: 191
[10] (王 聪, 徐永波, 韩恩厚. 金属学报, 2006; 42: 191)
[11] Gupta C, Chakravartty J K, Wadekar S L, Dubey J S. Mater Sci Eng, 2000; A292: 49
[12] Gerland M, Mendez J, Lepinoux J, Violan P. Mater Sci Eng, 1993; A164: 226
[13] Cui C Y, Gu Y F, Yuan Y, Harada H. Scr Mater, 2011; 64: 502
[14] Fu S F, Cheng T, Zhang Q C, Hu Q, Cao P T. Acta Mater, 2012; 60: 6650
[15] Han G M, Cui C Y, Gu Y F, Hu Z Q, Sun X F. Acta Metall Sin, 2013; 49: 1243
[15] (韩国明, 崔传勇, 谷月峰, 胡壮麒, 孙晓峰. 金属学报, 2013; 49: 1243)
[16] Chihab K, Estrin Y, Kubin L, Vergnol P J. Scr Mater, 1987; 21: 203
[17] Ziegenbein A, Hahner P, Neuhauser H. Comput Mater Sci, 2000; 19: 27
[18] Zhang Q C, Jiang Z Y, Jiang H F, Chen Z J, Wu X P. Int J Plasticity, 2005; 21: 2150
[19] Jiang H F, Zhang Q C, Jiang Z Y, Chen Z J, Wu X P. Chin Phys Lett, 2005; 22: 99
[20] Gao Y, Fu S H, Cai Y L, Cheng T, Zhang Q C. Acta Phys Sin, 2014; 63: 066201
[20] (高 越, 符师桦, 蔡玉龙, 程 腾, 张青川. 物理学报, 2014; 63: 066201)
[21] Ranc N, Wagner D. Mater Sci Eng, 2008; A474: 188
[22] Ait-Amokhtar H, Fressengeas C, Boudrahema S. Mater Sci Eng, 2008; A488: 540
[23] Pan B, Li K, Tong W. Experiment Mech, 2013; 53: 1277
[24] Kang Y L, Zhang Z F, Wang H W, Qin Q H. Mater Sci Eng, 2005; A394: 312
[25] Guo B Q, Wang H X, Xie H M, Chen P W. Theory Appl Mech Lett, 2014; 4: 021010
[26] Jiang Z Y, Zhang Q C, Jiang H F, Chen Z J, Wu X P. Mater Sci Eng, 2005; A403: 154
[27] Xiang G F, Zhang Q C, Liu H W, Jiang H F, Wu X P. Chin Phys Lett, 2006; 15: 2378
[28] Lebedkina T A, Lebyodkin M A. Acta Mater, 2008; 56: 5567
[1] 李冬冬, 钱立和, 刘帅, 孟江英, 张福成. Mn含量对Fe-Mn-C孪生诱发塑性钢拉伸变形行为的影响[J]. 金属学报, 2018, 54(12): 1777-1784.
[2] 郭鹏程, 钱立和, 孟江英, 张福成. 高锰奥氏体TWIP钢的单向拉伸与拉压循环变形行为*[J]. 金属学报, 2014, 50(4): 415-422.
[3] 韩国明,崔传勇,谷月峰,胡壮麒,孙晓峰. 一种镍基高温合金PLC效应的温度依赖性研究[J]. 金属学报, 2013, 49(10): 1243-1247.
[4] 符师桦 程腾 张青川 曹鹏涛 胡琦. 5456铝合金PLC效应的两种临界机制研究[J]. 金属学报, 2012, 48(12): 1453-1458.
[5] 田成刚 崔传勇 谷月峰 孙晓峰. 固溶处理对Ni-Co基高温合金反常动态应变时效的影响[J]. 金属学报, 2012, 48(10): 1223-1228.
[6] 江慧丰 陈学东 范志超 董杰 姜恒 陆守香. 动态应变时效对316L不锈钢疲劳蠕变行为的影响[J]. 金属学报, 2009, 45(3): 326-330.
[7] 谭军 李聪 孙超 应诗浩 连姗姗 阚细武 冯可芹. Zr--4合金应力松弛过程中的热激活变形与动态应变时效[J]. 金属学报, 2009, 45(2): 173-177.
[8] 王聪; 徐永波; 韩恩厚 . LA41镁合金的PLC效应及其解释[J]. 金属学报, 2006, 42(2): 191-194 .
[9] 江慧丰; 张青川; 徐毅豪; 伍小平 . 时效对Al-Cu合金中锯齿形流动的影响[J]. 金属学报, 2006, 42(2): 139-142 .
[10] 孙亮; 张青川; 江慧丰 . 溶质浓度对Al-Cu合金中PLC效应的影响[J]. 金属学报, 2006, 42(12): 1248-1252 .
[11] 江慧丰; 张青川; 蒋震宇; 伍小平 . Al-Cu合金中PLC效应时域和空域行为的实验研究[J]. 金属学报, 2005, 41(7): 727-732 .
[12] 柴惠芬;阮征;范群成. Cu及Cu-Zn合金预变形和循环软化的滑移线形貌[J]. 金属学报, 1994, 30(11): 502-506.
[13] 彭开萍;陈文哲;钱匡武. 动态应变时效对18-8型奥氏体不锈钢低周疲劳行为的影响[J]. 金属学报, 1993, 29(6): 43-48.
[14] 钱匡武;李效琦;张好国. 高强度Al-Zn-Mg-Cu合金中锯齿屈服的特征[J]. 金属学报, 1991, 27(5): 77-78.
[15] 陈文哲;钱匡武. 动态应变时效对奥氏体不锈钢纯弯疲劳强度的影响[J]. 金属学报, 1989, 25(2): 56-60.