| 低碳钢在模拟海洋潮差区的腐蚀行为的电化学研究 |
| 穆鑫,魏洁,董俊华,柯伟 |
| 中国科学院金属研究所腐蚀与防护国家重点实验室, 沈阳 110016 |
|
| ELECTROCHEMICAL STUDY ON CORROSION BEHAVIORS OF MILD STEEL IN A SIMULATED TIDAL ZONE |
| MU Xin, WEI Jie, DONG Junhua, KE Wei |
| State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Science,Shenyang 110016\par |
引用本文:
穆鑫,魏洁,董俊华,柯伟. 低碳钢在模拟海洋潮差区的腐蚀行为的电化学研究[J]. 金属学报, 2012, 48(4): 420-426.
,
,
,
.
ELECTROCHEMICAL STUDY ON CORROSION BEHAVIORS OF MILD STEEL IN A SIMULATED TIDAL ZONE[J]. Acta Metall Sin, 2012, 48(4): 420-426.
| [1] Xia L T, Huang G Q. China Foundry Machine Technol,2002; (6): 1 (夏兰廷, 黄桂桥. 中国铸造装备与技术, 2002; (6): 1)[2] Jeffrey R, Melchers R E. Corrosion, 2009; 65: 695[3] Jeffrey R, Melchers R E. Corrosion, 2007; 63: 872[4] Al-Fozan S A, Malik A U. Desalination, 2008; 228: 61[5] LaQue F L. Proc ASTM Corrosion Testing, PA: ASTM International, 1951: 495[6] Larrabee C A. Corrosion, 1958; 14: 501t[7] Southwell C R, Bultman J D, Hummer C W. Seawater Corrosion Handbook,NJ: Noyes Data Corp., 1979: 1[8] Takamara A, Arakawa K, Fujiwara F, Hirose H. Trans. Iron Steel Inst Jpn, 1971; 11: 299[9] Farro N W, Veleva L, Aguilar P. 215th ECS Meeting, 2009: 1[10] Huang G Q. Corros Prot, 2000; 21(1): 8 (黄桂桥. 腐蚀与防护, 2000; 21(1): 8)[11] Lou Y N, Song S Z, Jin W X, Yin L H. J Chem Ind Eng,2008; 59: 2864 (雒娅楠, 宋诗哲, 金威贤, 尹立辉. 化工学报, 2008; 59: 2864)[12] Lou Y N. PhD Thesis, Tian Jing University, 2007 (雒娅楠. 天津大学博士论文, 2007)[13] Gao Z P, Yang F Y, Zhang J L, Hou B R. Chin Pat, 2252989, 1997 (高振泮, 杨芳英, 张经磊, 侯宝荣. 中国专利, 2252989, 1997)[14] Hou B R. Marine Corrosion and Protection. Beijing: Science Press,1997: 59 (侯宝荣. 海洋腐蚀与防护. 北京: 科学出版社, 1997: 59)[15] Wang S T, Gao K W. Int J Mineral Metall Mater, 2009; 16: 58[16] Matsushima R, translated by Jing Y K. Low-alloy Corrosion Resistant Steel Development and Research. Beijing: Metallurgical Industry Press, 2004: 230 (松岛岩著, 靳裕康译, 低合金耐蚀钢开发、发展及研究. 北京:冶金工业出版社, 2004: 230)[17] Moller H, Boshoff E T, Froneman H. J S Afr Inst Min Metall,2006; 106: 585[18] Yamashita M, Miyuki H, Matsuda Y, Nagano H, Misawa T. Corros Sci, 1994; 36: 283[19] Hou B R, Zhang J L. Br Corros J, 2001; 36: 310[20] Hao L, Zhang S X, Dong J H, Ke W. Corros Sci,2012; 54: 241[21] Chen X H, Dong J H, Han E H, Ke W. Mater Prot,2007; 40(10): 19 (陈新华, 董俊华, 韩恩厚, 柯伟. 材料保护, 2007; 40(10): 19)[22] Fu X X. PhD Thesis, Institute of Metal Research Chinese Academy of Sciences, Shenyang, 2011 (傅欣欣, 中国科学院金属研究所博士论文, 沈阳, 2011) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|