| 缆式焊丝CO2气体保护焊工艺研究 |
| 方臣富1), 陈志伟1), 胥国祥1), 胡庆贤1), 周航宇1), 时振2) |
1) 江苏科技大学材料科学与工程学院, 镇江 212003
2) 江苏维特高科焊业有限公司, 淮安 223100 |
|
| STUDY ON THE PROCESS OF CTWW CO2 GAS SHIELDED WELDING |
| FANG Chenfu1), CHEN Zhiwei1), XU Guoxiang1), HU Qingxian1), ZHOU Hangyu2) |
1) School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003
2) Jiangsu Victor Hi-tech Welding Industry Co. LTD, Huaian 223100 |
引用本文:
方臣富 陈志伟 胥国祥 胡庆贤 周航宇 时振. 缆式焊丝CO2气体保护焊工艺研究[J]. 金属学报, 2012, 48(11): 1299-1305.
FANG Chenfu CHEN Zhiwei XU Guoxiang HU Qingxian ZHOU Hangyu.
STUDY ON THE PROCESS OF CTWW CO2 GAS SHIELDED WELDING[J]. Acta Metall Sin, 2012, 48(11): 1299-1305.
| [1] Wu C S, Zhang M X, Li K H, Zhang Y M. Acta Metall Sin, 2007; 43: 663(武传松, 张明贤, 李克海, 张裕明. 金属学报, 2007; 43: 663)[2] Harwig D, Gordon R. Proc 6th Int Conf Trends in Welding Research, OH: ASM International, 2003: 995[3] Guan Q, Lin S Y. Proc New Fusion Weld Technol Appl, Beijing: China Welding Society, 2003: 11(关 桥, 林尚扬. 熔焊新技术及应用研讨会论文集, 北京: 中国焊接学会, 2003: 11)[4] Lahnsteiner R. Weld Rev Int, 1992; 2: 17[5] Knapp I, Bartosik M. Weld Rev Int, 1998; 12: 25[6] Ma X L, Hua X M, Wu Y X. Weld Join, 2007; (7): 27(马晓丽, 华学明, 吴毅雄. 焊接, 2007; (7): 27)[7] Yin S Y. Weld Join, 2006; (10): 7(殷树言. 焊接, 2006; (10): 7)[8] Didling L A, Michael S, Ladwing B. Weld Cut, 2002; 5: 18[9] Feng Y H, Jin Q, Wang J P, Gu M L. Trans China Weld Inst, 2009; 30(6): 51(冯曰海, 金秋, 王克鸿, 顾民乐. 焊接学报, 2009; 30(6): 51)[10] Xu G X. PhD Thesis, Shandong University, Jinan, 2009(胥国祥. 山东大学博士学位论文, 济南, 2009)[11] Li P L, Lu H. Trans China Weld Inst, 2011; 32(6): 13(李培麟, 陆 皓. 焊接学报, 2011; 32(6): 13)[12] Zhang P Y, Gao C R, Zhu F X. Weld Technol, 2009; 38(6): 23(张朋彦, 高彩茹, 朱伏先. 焊接技术, 2009; 38(6): 23)[13] Chen S J, Wang J, Wang H X, Lu Z Y, Yin S Y, Bai S J. Trans China Weld Inst, 2005; 26(3): 45(陈树君, 王 军, 王会霞, 卢振洋, 殷树言, 白韶军. 焊接学报, 2005; 26(3): 45)[14] Hua A B, Yin S Y, Chen S J, Bai S J, Zhang X L. Chin J Mech Eng, 2010; 46(16): 142(华爱兵, 殷树言, 陈树君, 白韶军, 张晓亮. 机械工程学报, 2010; 46(16): 142)[15] Lu Z Y, Huang P F, Jiang G J, Yin S Y. Weld Join, 2006; (3): 16(卢振洋, 黄鹏飞, 蒋观军, 殷树言. 焊接, 2006; (3): 16)[16] Zhou H Y. Master Thesis, Jiangsu University of Science and Technology, Zhenjiang, 2012(周航宇. 江苏科技大学硕士学位论文, 镇江, 2012)[17] Hu X G. Master Thesis, Jiangsu University of Science and Technology, Zhenjiang, 2012(胡小光. 江苏科技大学硕士学位论文, 镇江, 2012)[18] Wang H S. Master Thesis, Jiangsu University of Science and Technology, Zhenjiang, 2012(王海松. 江苏科技大学硕士学位论文, 镇江, 2012)[19] Fang C F. PhD Thesis, Beijing University of Technology, 2005(方臣富. 北京工业大学博士学位论文, 2005)[20] Fang C F, Chen S J, Liu J, Yin S Y, Song Y L, Li H, Hou R S,Wen Y P. Trans China Weld Inst, 2005; 26(12): 1(方臣富, 陈树君, 刘嘉, 殷树言, 宋永伦, 李桓, 侯润石, 温永平. 焊接学报, 2005; 26(12): 1)[21] Fang C F, Ye Q L, Song Y L, Li H. Trans China Weld Inst, 2008; 29(4): 1(方臣富, 叶轻凌, 宋永伦, 李桓. 焊接学报, 2008; 29(4): 1)[22] Wu C S. Welding Thermal Process and Weld Pool Behaviour. Beijing: China Machine Press, 2007: 20(武传松. 焊接热过程与熔池形态. 北京: 机械工业出版社, 2007: 20)[23] Zhang M X. Master Thesis, Shandong University, Jinan, 2006(张明贤. 山东大学硕士学位论文, 济南, 2006)[24] Zhang M X, Wu C S, Li K H, Zhang Y M. Trans China Weld Inst, 2007; 28(2): 34(张明贤, 武传松, 李克海, 张裕明. 焊接学报, 2007; 28(2): 34)[25] Zhang W Y. Welding Metallurgy. Beijing: China Machine Press, 2002: 100(张文钺. 焊接冶金学. 北京: 机械工业出版社, 2002: 100) |
|