| 带锈碳钢在流动海水中的长期腐蚀行为 |
| 彭欣1,王佳1,2,山川1,王海杰1,刘在健1,邹妍3 |
1. 中国海洋大学化学化工学院, 青岛 266100
2. 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
3. 山东省科学院海洋仪器仪表研究所, 青岛 266100 |
|
| CORROSION BEHAVIOR OF LONG–TIME IMMERSED RUSTED CARBON STEEL IN FLOWING SEAWATER |
| PENG Xin 1, WANG Jia 1,2, SHAN Chuan 1, WANG Haijie 1, LIU Zaijian 1, ZOU Yan 3 |
1.The College of Chemistry and Chemical Engineering, Ocean University of China, Qingdao 266100
2. State Key Laboratory for Corrosion and Protection of Metals, Shenyang 110016
3. Shandong Provincial Key Laboratory of Ocean Environment Monitoring Technology, Institute of Oceanographic Instrumentation, Shandong Academy of Sciences, Qingdao 266100 |
引用本文:
彭欣 王佳 山川 王海杰 刘在健 邹妍. 带锈碳钢在流动海水中的长期腐蚀行为[J]. 金属学报, 2012, 48(10): 1260-1266.
PENG Xin WANG Jia SHAN Chuan WANG Haijie LIU Zaijian ZOU Yan.
CORROSION BEHAVIOR OF LONG–TIME IMMERSED RUSTED CARBON STEEL IN FLOWING SEAWATER[J]. Acta Metall Sin, 2012, 48(10): 1260-1266.
| [1] Javaherdashti R. Anti corros Methods Mater, 2000; 47(1): 30[2] Zheng W L, Yu Q. Environment Sensitive Fraction of Steel. Beijing: Chemical Industry Press, 1988: 12(郑文龙, 于 青. 钢的环境敏感断裂. 北京: 化学工业出版社, 1988: 12)[3] Zhu Y L, Zhou J, Xiong C J, Ma Z F, Liu Z S. PetrolChem Equip, 2002; 31(1): 14(朱岳麟, 周健, 熊常健, 马志锋, 刘中生. 石油化工设备, 2002; 31 (1): 14)[4] Yan M, Huang G Q. Marine Sci, 2005; 29(7): 73(颜 民, 黄桂桥. 海洋科学, 2005; 29(7): 73)[5] Cao C N. Corrosion of Chinese Materials in Nature Environment. Beijing: Chemical Industry Press, 2005: 1(曹楚南. 中国材料的自然环境腐蚀. 北京: 化学工业出版社, 2005: 1)[6] Xia L T, Huang G Q, Ding L P. Res Studies Foundry Equip, 2002; 4: 14(夏兰廷, 黄桂桥, 丁路平. 铸造设备研究, 2002; 4: 14)[7] Huang G Q. Corros Sci Prot Technol, 2001; 13: 81(黄桂桥. 腐蚀科学与防护技术, 2001; 13: 81)[8] Qiu Y B, Qi G T, Guo Z H. China Offshore Oil Gas, 1996;8(5): 18 (邱于兵, 齐公台, 郭稚弧. 中国海上油气, 1996; 8(5): 18)[9] Zhang W, Wang J, Li Y N, Wang W. Acta Phys Chim Sin, 2010; 26: 2941(张 伟, 王佳, 李玉楠, 王伟. 物理化学学报, 2010; 26: 2941)[10] Bousselmi L, Fiaud C, Tribollet B, Triki E. Electrochim Acta, 1999; 44: 4357[11] John D G, Searosn P C, Dawson J L. Br Corros J, 1981; 16(2): 102[12] Liu G Z, Wang J M, Zhang J Q, Cao C N. Acta Metall Sin, 2011; 47: 1600(刘光洲, 王建明, 张鉴清, 曹楚南. 金属学报, 2011; 47: 1600)[13] Zhang J B, Wang J, Wang Y H. Acta Phys Chim Sin, 2005; 21: 993(张际标, 王佳, 王燕华. 物理化学学报, 2005; 21: 993)[14] Gonz´alez J A, Miranda J M, Otero E, Feliu S. Corros Sci, 2007; 49: 436[15] Zou Y, Zheng Y Y, Wang Y H, Wang J. Acta Metall Sin, 2010; 46: 123(邹妍, 郑莹莹, 王燕华, 王佳. 金属学报, 2010; 46: 123)[16] Zou Y, Wang J, Zheng Y Y. Acta Phys Chim Sin, 2010;26: 2361 (邹妍, 王佳, 郑莹莹. 物理化学学报, 2010; 26: 2361)[17] Zou Y, Wang J, Zheng Y Y. Corros Sci, 2011; 53: 208[18] Antony H, Perrin S, Dillmann P, Legrand L, Chauss´e A. Electrochim Acta, 2007; 52: 7754[19] Andrade C, Keddam M, N´ovoa X R, P´erez M C, Rangel C M, Takenouti H. Electrochim Acta, 2001; 46: 3905[20] Nov´ak P, Mal´aR, Joska L. Cement Concrete Res, 2001; 31: 589[21] Copson H R. Corrosion, 1960; 16: 130[22] Shalaby H M, Attari S, Riad W T. Corrosion, 1992; 48: 206[23] Nesic S, Solvi G T, Enerhaug J. Corrosion, 1995; 51: 773[24] Huang G Q. Corros Sci Prot Technol, 2001; 22: 384(黄桂桥. 腐蚀科学与防护技术, 2001; 22: 384)[25] Martinez S. Mater Chem Phys, 2002; 77: 97[26] Stern M, Geary A L. J Electrochem Soc, 1957; 104: 56 |
|