回火温度对Mn系低碳贝氏体钢的低温韧性的影响 |
高古辉, 张寒, 白秉哲 |
清华大学材料科学与工程系先进材料教育部重点实验室, 北京 100084 |
|
EFFECT OF TEMPERING TEMPERATURE ON LOW TEMPERATURE IMPACT TOUGHNESS OF A LOW CARBON Mn-SERIES BAINITIC STEEL |
GAO Guhui ZHANG Han BAI Bingzhe |
Key Laboratory of Advanced Materials of Ministry of Education, Department of Material Science and Engineering, Tsinghua University, Beijing 100084 |
引用本文:
高古辉 张寒 白秉哲. 回火温度对Mn系低碳贝氏体钢的低温韧性的影响[J]. 金属学报, 2011, 47(5): 513-519.
,
,
.
EFFECT OF TEMPERING TEMPERATURE ON LOW TEMPERATURE IMPACT TOUGHNESS OF A LOW CARBON Mn-SERIES BAINITIC STEEL[J]. Acta Metall Sin, 2011, 47(5): 513-519.
[1] Thompson S W, Colvin D J, Krauss G. Metall Trans, 1990; 21A: 1493[2] Park K T, Kim Y S, Lee J G. Mater Sci Eng, 2000; A293: 165[3] Feng C. PhD Thesis, Tsinghua University, Beijing, 2010(冯春. 清华大学博士学位论文, 北京, 2010)[4] Feng C, Fang H S, Bai B Z, Zheng Y K. Acta Metall Sin, 2010; 46: 473(冯春, 方鸿生, 白秉哲, 郑燕康. 金属学报, 2010; 46: 473)[5] Yoo J Y, Choo W Y, ParkTW, KimYW. ISIJ Int, 1995; 35: 1034[6] Dhua S K, Ray A, Sarma D S. Mater Sci Eng, 2001; A318: 197[7] Andrzej K L. J Mater Sci Technol, 2000; 106: 212[8] Marder A R, Krauss G. Trans ASM, 1967; 60: 651[9] Zhu K Y, Bouaziza Olivier, Oberbilliga Carla, Huang M X. Mater Sci Eng, 2010; A527: 6614[10] Naylor J P, Blondeau R. Metall Trans, 1976; 7A: 891[11] Shin S Y, Hong S M, Bae J H, Kim K, Lee S. Metall Mater Trans, 2009; 40A: 2333[12] Takamura J, Mizoguchi S. Proc 6th Int Iron Steel Congr, Nagoya: ISIJ, 1990: 591[13] Han S Y, Shin S Y, Seo C H, Lee H, Bae J H, Kim K, Lee S, Kim N J. Metall Mater Trans, 2009; 40A: 1851[14] Wu H B, Shang C J, Yang S W, Hou H X, Ma Y P, Yu G L. Acta Metall Sin, 2004; 11: 1143(武会宾, 尚成嘉, 杨善武, 侯华兴, 马玉璞, 于功利. 金属学报, 2004; 11: 1143)[15] Dunn C G, Daniels F W. Trans AIME, 1951; 191: 147 |
|