| 多流连铸中间包停留时间分布曲线总体分析方法 |
| 雷洪1), 赵岩2), 鲍家琳1), 刘承军2), 陈海耿2), 赫冀成1) |
1) 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819
2) 东北大学材料与冶金学院, 沈阳 110819 |
|
| WHOLE ANALYSIS APPROACH FOR RESIDUE TIME DISTRIBUTION CURVE IN MULTI-STRAND CONTINUOUS CASTING TUNDISH |
| LEI Hong1), ZHAO Yan2), BAO Jialin1), LIU Chengjun2), CHEN Haigeng2), HE Jicheng1) |
1) Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819
2) School of Materials and Metallurgy, Northeastern University, Shenyang 110819 |
引用本文:
雷洪 赵岩 鲍家琳 刘承军 陈海耿 赫冀成. 多流连铸中间包停留时间分布曲线总体分析方法[J]. 金属学报, 2010, 46(9): 1109-1114.
,
,
,
,
,
.
WHOLE ANALYSIS APPROACH FOR RESIDUE TIME DISTRIBUTION CURVE IN MULTI-STRAND CONTINUOUS CASTING TUNDISH[J]. Acta Metall Sin, 2010, 46(9): 1109-1114.
| [1] Sahai, Y. Ahuja, R.. Ironmaking Steelmaking, 1986; 13: 241
[2] Sahai Y, Emi T. ISIJ Int, 1996; 36: 667
[3] Singh S, Koria S C. Ironmaking Steelmaking, 1996; 23: 255
[4] Mazumdar D, Guthrie R I L. Steel Res, 1997; 68: 293
[5] Mazumdar D, Guthrie R I L. ISIJ Int, 1999; 39: 524
[6] Zong J H. Yi K W, Yoon J K. ISIJ Int, 1999; 39: 139
[7] Jha P, Dash S K. ISIJ Int, 2002; 42: 670
[8] Jha P K, Dash S K. Int J Numer Methods Heat Fluid Flow, 2002; 12: 560
[9] Lopez-Ramirez S, Barreto J D J, Vite-Martinez P, Serrano J A R, Duran-Valencia C. Metall Mater Trans B, 2004 ; 35: 957
[10] Solorio-Diaz G, Morales R D, Ramos-Banderas A. Int J Heat Mass Transfer, 2005; 48: 3574
[11] Liu S X, Yang X M, Du L, Li L, Liu C Z. ISIJ Int, 2008; 48: 1712
[12] Yan J X, Huang Y, Liu S T. J Iron Steel Res, 1998; 10: 64
(阎建新, 黄晔, 柳寿亭. 钢铁研究学报, 1998; 10: 64)
[13] Fan J F, Zhang Q L, Zhu M Y, Lei H, Wang W Z.. Iron Steel, 1998; 33: 24
(樊俊飞, 张清朗, 朱苗勇, 雷洪, 王文忠. 钢铁, 1998; 33: 24)
[14] Fu P Y, Chen W Q, Jin Z C. Steelmaking, 1998; 14: 33
(富平原, 陈伟庆, 靳自成. 炼钢, 1998; 14: 33)
[15] Zheng S G, Zhu M Y, Jiang G L, Gong J P. Iron Steel; 2004, 39: 23
(郑淑国, 朱苗勇, 姜桂连, 宋嘉鹏. 钢铁2004; 39: 23)
[16] Zheng S G, Zhu M Y. Acta Metall Sinica. 2005; 41: 1073
(郑淑国, 朱苗勇. 金属学报, 2005; 41: 1073)
[17] Zheng S G, Zhu M Y. Chin J Process Eng. 2006; 6: 522
(郑淑国, 朱苗勇. 过程工程学报, 2006; 6: 522)
[18] Xiao X G. Metallurgical Reaction Engineering. Shenyang: Northeastern University Press. 1989: 72
(肖兴国. 冶金反应工程学.沈阳: 东北大学出版社. 1989: 72)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|