| 板坯电磁制动结晶器内流体流动的研究 |
| 于湛,张振强,任忠鸣,雷作胜,邓康 |
| 上海大学现代冶金与材料制备重点实验室, 上海 200072 |
|
| STUDY ON THE FLUID FLOW IN SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE |
| YU Zhan, ZHANG Zhenqiang, REN Zhongming, LEI Zuosheng, DENG Kang |
| Shanghai Key Laboratory of Modern Metallurgy & Materials Processing, Shanghai University, Shanghai 200072 |
引用本文:
于湛 张振强 任忠鸣 雷作胜 邓康. 板坯电磁制动结晶器内流体流动的研究[J]. 金属学报, 2010, 46(10): 1275-1280.
,
,
,
,
.
STUDY ON THE FLUID FLOW IN SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE[J]. Acta Metall Sin, 2010, 46(10): 1275-1280.
| [1]Nagai J, Suzuki K, Kojima S, Kollberg S. Iron Steel Eng,
1984; 61: 41
[2]Yamamura H, Toh T, Harada H, Takeuchi E, Iahii T. ISIJ
Int, 2001; 41: 1229
[3]Suzuki M, Nakada M. ISIJ Int, 2001; 41: 1229
[4]Chen Z H, Wang E G, He J C. Steelmaking, 2004, 20: 48
(陈芝会, 王恩刚, 赫冀成. 炼钢, 2004, 20: 48)
[5]Zeze M, Harada H, Takeuchi E, Ishii T. 76th Steelmaking
Conference Proceedings. Dallas: Iron & steelmaker,1993:
53
[6]Zeze M, Tanaka H, Takeuchi E, Mizoguchi S. 79th
Conference of the Steelmaking. Pittsburgh: Iron and Steel
Society, 1996: 225
[7]Kollberg S, Lofgren P. Rev. Met, 2005,6: 431
[8]Harada H, Toh T, Ishii T, Kaneko K, Takeuchi E. ISIJ int,
2001; 41: 1236
[9]Li B K, He J C, Jia G L, Gao Y Y. Acta Metall Sin, 1997;
33:1207
(李宝宽, 赫冀成, 贾光霖, 高允彦. 金属学报, 1997;
33: 1207)
[10]Li B K, Tsukihashi F. ISIJ int, 2006; 46: 1833
[11]Hwang Y S, Cha P R, Nam H S, Moon K H, Yoon J K. ISIJ
int, 1997; 37: 659
[12]Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 1141
(于海歧, 朱苗勇. 金属学报, 2008; 44: 1141)
[13]Qian Z D, Wu Y L. ISIJ int, 2004; 44: 100
[14]Cukierski K, Thomas B G. Metall Mater Trans B, 2008;
39: 94
[15]Ha M Y, Lee H G, Seong S H. J. Mater. Process. Technol,
2003, 133: 322
[16]Takatani K. ISIJ int, 2003; 43: 915
[17]Yu H Q, Wang B F, Li H Q, Li J C.J. Mater. Process.
Technol, 2008, 202: 179 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|