铝合金熔体中氢溶解度的计算模型
蒋光锐 刘 源 李言祥
清华大学机械工程系
A Model for Calculating Solubility of Hydrogen in Molten Alloys
;;;;
清华大学机械工程系
引用本文:

蒋光锐; 刘源; 李言祥 . 铝合金熔体中氢溶解度的计算模型[J]. 金属学报, 2008, 44(2): 129-133 .

全文: PDF(345 KB)  
摘要: 基于Sieverts 定律和多元合金组元活度系数计算模型,建立了一个计算氢在多元合 金熔体中溶解度的计算模型,该模型只需要氢在纯金属熔体的中溶解度参数,为预测多 元合金熔体中氢含量提供了有效的途径。以此计算了氢在多种铝合金熔体中的溶解度随 温度变化的情况,计算结果与实验值吻合较好。
关键词 : 氢溶解度,  热力学模型,  合金熔体    
Abstract:Based on the Sieverts law and the thermodynamic model for activity coefficient prediction, a new thermodynamic model has been developed for calculating the hydrogen so- lubility in molten multicomponent alloys in which only the hydrogen solubilities in pure met- als are required. The predicted hydrogen solubilities in several molten aluminum alloys at different temperatures and compositions have a good agreement with the experimental results.
Key words: Solubility of hydrogen    Thermodynamic model    Molten alloys
收稿日期: 2007-05-08     
[1]Lei Y Q.Physical Chemistry in the Cast Processing.Bei- jing:New Times Press,1982:155 (雷永泉.铸造过程物理化学.北京:新时代出版社,1982:155)
[2]Translated by Huang L Y,Yah M S.Gases in Nonferrous Metals and Alloys.Beijing:Met- allurgical Industry Press,1989:1,54,126 (著.黄良余,严名山译.有色金属及其合金中的气体.北京:冶金工业出版社,1989:1,54,126)
[3]Chen Y D.Hydrogen in Metals and Alloys.Beijing:Met- allurgical Industry Press,1988:12 (陈永定.金属和合金中的氢.北京:冶金工业出版社,1988:12)
[4]Xiong Y C,Huang Z G,Wang W Q.Spec Cast Nonferrous Alloys,1995;(4):12 (熊艳才,黄志光,王文清.特种铸造及有色合金,1995;(4):12)
[5]Baccepman A M,Kunin A A,Syrovoi I N;Translated by Zhang Z H,Jin Q G.Measurement of the Gas in Metals. Shanghai:Shanghai Science & Technology Press,1981:1 (著.张中豪,金钦漧译.金属中气体的测定.上海:上海科学技术出版社,1981:1)
[6]Manchester P D.Phase Diagrams of Binary Hydrogen Al- loys.Materials Park,OH:ASM International,2000:1
[7]Lin R Y,Hoch M.Metall Trans,1989;20A:1785
[8]Anyalebechi P N.Scr Mater,1996;34:513
[9]Anyalebechi P N.Scr Metall Mater,1995;33:1209
[10]Wagner C.Thermodynamics of Alloys. Cambridge: Addison-Wesley Press,1952:120
[11]Sokolov V M,Fedorenko I V.Int J Hydrogen Energy,1996; 11-12:931
[12]Jiang G R,Liu Y,Li Y X,Su Y Q,Guo J J.Acta Metall Sin,2007;43:503 (蒋光锐,刘源,李言祥,苏彦庆,郭景杰.金属学报,2007;43:503)
[13]Li M.Master Thesis,Harbin Institute of Technology,2006 (李敏.哈尔滨工业大学硕士学位论文,2006)
[14]Anyalebechi P N,Talbot D E J,Granger D A.Metall Trans,1988;19B:227
[15]Xu Z Y,Li L.Materials Thermodynamic.Beijing:Science Press,2005:265 (徐祖耀,李麟.材料热力学.北京:科学出版社,2005:265)
[16]Kung J K,Nazarlo F N,Joffe J,Tassios D.Ind Eng Chem Process Des Dev,1984;23:170
[17]Ding X Y,Wang W Z.Acta Metall Sin,1994;30:444 (丁学勇,王文忠.金属学报,1994;30:444)
[18]Gokcen N A.Statistical Thermodynamics of Alloys.New York:Plenum Press,1986:255
[19]Takamichi I,G.Roderick I L.The Physical Properties of Liquid Metals.New York:Oxford University Press,1988: 6
[20]Tao D P.Metall Mater Trans,2005;36A:3495
[21]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2007;43: 113 (张华伟,李言祥,刘源.金属学报,2007;43:113)
[22]Matysina Z A,Zaginaichenko S Y,Schur D V,Pishuk V K.J Alloy Compd,2002;330-332:85
[23]Mao Y W.Metallurgical Melts.Beijing:Metallurgical In- dustry Press,1993:1 (毛裕文.冶金熔体.北京:冶金工业出版社,1993:1)r
[1] 王寒玉, 李彩, 赵璨, 曾涛, 王祖敏, 黄远. 基于纳米活性结构的不互溶W-Cu体系直接合金化及其热力学机制[J]. 金属学报, 2023, 59(5): 679-692.
[2] 胡标, 张华清, 张金, 杨明军, 杜勇, 赵冬冬. 界面热力学与晶界相图的研究进展[J]. 金属学报, 2021, 57(9): 1199-1214.
[3] 王斌,刘振宇,周晓光,王国栋. 超快速冷却条件下亚共析钢中纳米级渗碳体析出的相变驱动力计算[J]. 金属学报, 2013, 49(1): 26-34.
[4] 陈福义; 介万奇 . Al-Cu-Zn合金溶质分凝的热力学模型[J]. 金属学报, 2003, 39(6): 597-600 .
[5] 陈福义; 介万奇 . 利用短程序改进Al-Cu熔体的热力学模型[J]. 金属学报, 2003, 39(6): 601-604 .
[6] 乐启炽; 张新建; 崔建忠; 路贵民 . 金属合金溶液热力学模型研究进展[J]. 金属学报, 2003, 39(1): 35-42 .
[7] 熊华平; 李晓红; 毛唯; 李建平; 马文利; 程耀永 . 表面渗硅处理提高钛铝基合金高温抗氧化性[J]. 金属学报, 2003, 39(1): 66-70 .
[8] 李卫红; 边秀房; 李海勇; 段佑峰 . Al-Cu共晶合金熔体中稀土Ce与氢的相互作用[J]. 金属学报, 2001, 37(8): 825-828 .
[9] 沈剑韵;郝耀武;周传华;凌铃. 不对称性定量化的三元系热力学模型[J]. 金属学报, 1996, 32(9): 943-948.