| 吹氩板坯连铸结晶器内钢/渣界面行为的数值模拟 |
| 曹娜;朱苗勇 |
| 东北大学材料与冶金学院 |
|
| Numerical Simulation for the Interfacial Behavior of Steel and Slag in a Slab Continuous Casting Mold with Blowing Argon Gas |
| Na CAO |
| 东北大学材料与冶金学院 |
引用本文:
曹娜; 朱苗勇 . 吹氩板坯连铸结晶器内钢/渣界面行为的数值模拟[J]. 金属学报, 2008, 44(1): 79-84 .
,
.
Numerical Simulation for the Interfacial Behavior of Steel and Slag in a Slab Continuous Casting Mold with Blowing Argon Gas[J]. Acta Metall Sin, 2008, 44(1): 79-84 .
[1]Zhang J M,He J C,Li B K.Acta Metall Sin,1995;31: 269 (张炯明,赫冀成,李宝宽.金属学报,1995;31:269) [2]Ma F J,Wen G H,Li G.Steelmaking,2000;16(3):42 (马范军,文光华,李刚.炼钢,2000;16(3):42) [3]Yu H X,Zhu G S,Wang X H,Zhang J M,Wang W J.J Univ Sci Technol Beijing,2003;25:215 (于会香,朱国森,王新华,张炯明,王万军.北京科技大学学报,2003;25:215) [4]Thomas B G,Huang X,Sussman R C.Metall Mater Trans,1994;25B:527 [5]Iguchi M,Kasai N.Metall Mater Trans,2000;31B:453 [6]Noriko K,Toshio I,Jun K,Norichika A.ISIJ Int,2002; 42:1251 [7]Singh V,Dash S K,Sunitha J S,Ajmani S K,Das A K. ISIJ Int,2006;46:210 [8]Hua B,Thomas B G.Metall Mater Trans,2001;32B:1143 [9]Sanchez-Perez R,Morales R D,Garcia-Demedices L, Palafox R J,Diaz-Cruz M.Metall Mater Trans,2004; 35B:85 [10]Kasai N,Iguchi M.Tetsu Hagané,2005;91:546 (笠井宣文,井口学.铁钢,2005;91:546) [11]Zhang Y L,Zhu M Y,Zhang S J,Zheng S G,Cheng N L, Song J X.Spec Steel,2006;27(5):27 (张永亮,朱苗勇,张胜军,郑淑国,程乃良,宋景欣.特殊钢,2006;27(5):27) [12]Lu J X,Wang W K,Zhang J M,Wang X H,Wang W J, Qie F.J Univ Sci Technol Beijing,2006;28:34 (卢金雄,王文科,张炯明,王新华,王万军,郄芳.北京科技大学学报,2006;28:34) [13]Lu Q T,Yang R G,Wang X H,Zhang J M,Wang W J Iron Steel,2006;41(7):29 (陆巧彤,杨荣光,王新华,张炯明,王万军.钢铁,2006;41(7):29) [14]Zhang S J,Zhu M Y,Zhang Y L,Zheng S G,Cheng N L, Song J X.Acta Metall Sin,2006;42:1087 (张胜军,朱苗勇,张永亮,郑淑国,程乃良,宋景欣.金属学报,2006;42:1087) [15]Yamashita S,Iguchi M.ISIJ Int,2001;41:1529 [16]Cao N,Zhu M Y.Acta Metall Sin,2007;43:834 (曹娜,朱苗勇.金属学报,2007;43:834) [17]CD-Adapco.STAR-CD Methodology,Version 3.10,Lon- don:Computational Dynamics Limited,1999 [18]Assar M B,Dauby P H,Lawson G D.In:Steelmaking Division of Iron and Steel Society Proceedings,USA,ed., 83rd Steelmaking Conference,Warrendale,PA:Iron and Steel Society,2000:397W |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|