| 等通道转角挤压Al-Cu合金的冲击性能 |
| 房大然;段启强;黄崇湘;吴世丁;张哲峰;李家俊;赵乃勤 |
| 中科院金属所 |
|
| Impact properties of Al-Cu alloy subjected to equal channel angular pressing |
| ;;;;;; |
| 中科院金属所 |
引用本文:
房大然; 段启强; 黄崇湘; 吴世丁; 张哲峰; 李家俊; 赵乃勤 . 等通道转角挤压Al-Cu合金的冲击性能[J]. 金属学报, 2007, 43(12): 1251-1255 .
[1]Segal V M.Mater Sci Eng,1995;A197:157 [2]Valiev R Z,Langdon T G.Prog Mater Sci,2006;51:881 [3]Fang D R,Duan Q Q,Zhao N Q,Li J J,Wu S D,Zhang Z F.Mater Sci Eng,2007;A459:137 [4]Zhao Y H,Liao X Z,Zhu Y T,Valiev R Z.J Mater Res, 2005;20:288 [5]Horita Z,Furukawa M,Nemoto M,Barnes A J,Langdon T G.Acta Mater,2000;48:3633 [6]Lee S,Utsunomiya A,Akamatsu H,Neishi K,Furukawa M,Horita Z,Langdon T G.Acta Mater,2002;50:553 [7]Zhang Z F,Wu S D,Li Y J,Liu S M,Wang Z G.Mater Sci Eng,2005;A412:279 [8]Fang D R,Zhang P,Duan Q Q,Wu S D,Zhang Z F,Li J J,Zhao N Q.Adv Eng Mater,2007;9:860 [9]Vinogradov A,Hashimoto S.Adv Eng Mater,2003;5:351 [10]Mughrabi H,Hoppel H W,Kautz M.Scr Mater,2004;51: 807 [11]Ma A B,Suzuki K,Nishida Y,Saito N,Shigematsu I,Tak- agi M,Iwata H,Watazu A,Imura T.Acta Mater,2005; 53:211 [12]Ma A B,Suzuki K,Saito N,Nishida Y,Takagi M,Shige- matsu I,Iwata H.Mater Sci Eng,2005;A399:181 [13]Polmear I J.Light Alloys.London:Edward Arnold,1981: 45 [14]Iwahashi Y,Horita Z,Nemoto M,Longdon T G.Acta Mater,1998;46:3317 [15]Horita Z,Fujinami T,Nemoto M,Langdon T G.J Mater Process Technol,2001;117:288 [16]Kim W J,Chung C S,Ma D S,Hong S I,Kim H K.Scr Mater,2003;49:333 [17]Shin D H,Park K T.Mater Sci Eng,2005;A410-411:299 [18]Máthis K,Gubicza J,Nam N H.J Alloys Compd,2005; 394:194 [19]Dalla T F,Lapovok R,Sandlin J,Thomson P F,Davies C H J,Pereloma E V.Acta Mater,2004;52:4819 [20]Menzemer C C,Srivatsan T S,Al-Hajri M,Ortiz R.Mater Sci Eng,2000;A289:198 [21]Li Z,Samuel A M,Samuel F H,Ravindran C,Doty H W, Valtierra S.Mater Sci Eng,2004;A367:111 [22]Gür C H,Yildiz I.Mater Sci Eng,2004;A382:395 [23]William D,Callister J.Fundamentals of Materials Sci- ence and Engineering.New York:John Wiley & Sons Inc,2001:164X |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|