| 垂直裂纹对EB-PVD热障涂层热循环失效模式的影响 |
| 陈立强 宫声凯 徐惠彬 |
| 北京航空航天大学材料科学与工程学院;北京 100083 |
|
| INFLUENCE OF VERTICAL CRACKS ON FAILURE MECHANISM OF EB-PVD THERMAL BARRIER COATINGS DURING THERMAL CYCLING |
| CHEN Liqiang; GONG Shengkai; XU Huibin |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
引用本文:
陈立强; 宫声凯; 徐惠彬 . 垂直裂纹对EB-PVD热障涂层热循环失效模式的影响[J]. 金属学报, 2005, 41(9): 979-984 .
,
,
.
INFLUENCE OF VERTICAL CRACKS ON FAILURE MECHANISM OF EB-PVD THERMAL BARRIER COATINGS DURING THERMAL CYCLING[J]. Acta Metall Sin, 2005, 41(9): 979-984 .
[1] Nusier S Q, Newaz G M, Chaudhury Z A. Int J Solid Struct, 2000; 37: 2495 [2] Wang J S, Evans A G. Acta Mater, 1999; 47: 699 [3] Evans A G, Mumm D R, Hutchinson J W, Meier G H, Pettit F S. Progr Mater Sci, 2001; 46: 505 [4] Sohn Y H, Kim J H,Jordan E H, Gell M. Surf Coat Technol, 2001; 146: 70 [5] AH M Y, Nusier S Q, Newaz G M. Int J Solid Struct,2001; 38: 3329 [6] Sfar K, Aktaa J, Munz D. Mater Sci Eng, 2002; A333: 351 [7] Rosier J, Baker M, Volgmann M. Acta Mater, 2001; 49: 3659 [8] Editor Committee of China Aviation Materials Manual. China Aviation Materials Manual. Vol.2, 2nd ed., Beijing: China Standard Press, 2002: 771 (中国航空材料手册编辑委员会.中国航空材料手册.第2卷, 第2版,北京:中国标准出版社, 2002:771) [9] Zhou Y C, Hashida T. Int J Solid Struct, 2001; 38: 4235 [10] Bi X F, Xu H B, Gong S K. Surf Coat Technol, 2000; 130: 122 [11] Xu H B, Gong S K, Zhang Y, Zhang C X. Intermetallics, 2005; 13: 3154 |
|