| Al-Cu合金中PLC效应时域和空域行为的实验研究 |
| 江慧丰 张青川 蒋震宇 伍小平 |
| 中国科技大学中国科学院材料力学行为和设计重点实验室; 合肥 230027 |
|
| Experimental Investigations on the Temporal and Spatial Behaviors of the PLC Effect in Al--Cu Alloys |
| JIANG Huifeng; ZHANG Qingchuan; JIANG Zhenyu; WU Xiaoping |
| CAS Key Laboratory of Mechanical Behavior and Design of Materials; University of Science and Technology of China; Hefei 230027 |
引用本文:
江慧丰; 张青川; 蒋震宇; 伍小平 . Al-Cu合金中PLC效应时域和空域行为的实验研究[J]. 金属学报, 2005, 41(7): 727-732 .
,
,
,
.
Experimental Investigations on the Temporal and Spatial Behaviors of the PLC Effect in Al--Cu Alloys[J]. Acta Metall Sin, 2005, 41(7): 727-732 .
[1] Portevin A, Le Chatelier F. Comp Rend Acad Sci Paris, 1923; 176: 507 [2] Bell J F. Encyclopedia of Physics, Mech Solids I, Vol. VIa/1. Berlin, 1973; Sect. 2.11:41-44, Sect. 4.31: 649 [3] Cottrell A H. Dislocations and Plastic Flow in Crystals, London: Oxford University Press, 1953 [4] Lebyodkin M, Dunin-Barkowskii L, Brechet Y, Estrin Y, Kubin L P. Acta Mater, 2000; 48: 2529 [5] Pink E, Weinhandl H. Scr Mater, 1998; 39: 1309 [6] Tian B H, Zhang Y G, Chen C L. Acta Metall Sin, 1996; 32: 249 (田宝辉,张永刚,陈昌麟.金属学报, 1996;32:249) [7] Tian B H, Li H X, Zhang Y G, Chen C L Q. Acta Metall Sin, 1998; 34: 603 (田宝辉,李焕喜,张永刚,陈昌麒.金属学报,1998;34:603) [8] Ziegenbein A, Hahner P, Neuhauser H. Comput Mater Sci, 2000; 19: 27 [9] Zhang Q C, Toyooka S, Meng Z B. Process SPIE, 1999; 3585 [10] Pink E, Grinberg A, Mater Sci Eng, 1981; A51: 1 [11] Chihab K, Estrin Y, Kubin L P. Scr Metall, 1987; 21: 203 [12] Jiang H F, Zhang Q G, Jiang Z Y, Zhao S M, Chen Z J, Wu X P. J Exp Mech, in press (江慧丰,张青川,蒋震宇,赵思敏,陈忠家,伍小平.实验力 学,in press) [13] Hahner P, Ziegenbein A, Rizzi E, Neuhauser H. Phys Rev , 2002; 65B: 134/09-1 [14] Klose F B, Zigenbein A, Hagemann F, Neuhauser H, Hahner P, Abbsdi M, Zeghloul A. Mater Sci Eng, 2004; 369A: 76 [15] Miguel M C, Vespignani A, Zapperi S, Weiss J, Grasso J R. Nature, 2001; 410: 667 [16] McGormick P G. Ada Metall, 1972; 20: 351 [17] Wang Y, Srolovitz J, Rickman J M, Lesar R. Acta Mater, 2000; 48: 2163 [18] Kubin L P, Estrin Y. Acta Metall Mater, 1990; 38: 697 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|