圆坯连铸结晶器传热的反算法
尹合壁;姚 曼
大连理工大学材料工程系; 大连 116023
Inverse Algorithm of Heat Transfer in Round Billet Continuous Casting Mould
YIN Hebi; YAO Man
Department of Materials Engineering ; Dalian University of Technology; Dalian 116023
引用本文:

尹合壁; 姚曼 . 圆坯连铸结晶器传热的反算法[J]. 金属学报, 2005, 41(6): 638-644 .
, . Inverse Algorithm of Heat Transfer in Round Billet Continuous Casting Mould[J]. Acta Metall Sin, 2005, 41(6): 638-644 .

全文: PDF(342 KB)  
摘要: 基于圆坯连铸结晶器实测温度数据, 建立了结晶器传热反问题数学模型, 通过确定结晶器和铸坯之间局部热阻大小及其分布, 计算出结晶器热流 场和坯壳厚度, 且分析了结晶器热流分布特征和铸坯凝固状态, 并比较 两者之间的关系. 计算结果准确地反映了实际生产过程中沿结晶器周向 非均匀传热特征, 为将数值模拟技术应用于连铸凝固过程监控和“可视 化结晶器”技术提供了可借鉴的实用方法.
关键词 : 连铸结晶器,  圆坯,  热流     
Abstract:Based on the measured data of mould temperatures during continuous casting of round billet, an inverse problem model was developed. Through identifying the local thermal resistance and its distribution between the mould and the strand, the mould heat flux and the shell thickness profiles were calculated, and the relationship between them was also analyzed. The calculated results could preciously and correctly reflect the characteristics of non-uniform heat transfer around the mould circumference, which provided an applicable method for applying numerical simulation technique to monitor the solidification process and the“visual mould”technology in continuous casting.
Key words: continuous casting mould    round billet
收稿日期: 2004-08-31     
ZTFLH:  TG249  
[1]Brimacombe J K.Metall Trans,1993;24B:917
[2]Bakshi I A,Brendzy J L,Walker B N,Chandra S,Sama- rasekera I V,Brimacombe J K.Ironmaking Steelmaking, 1993;20:54
[3]Emling W H,Dawson S.ISS 74th Steelmaking Conf Proc, Washington,DC:Iron and Steel Society of AIME,1991: 197
[4]Lang O,Federspiel C,Thalhammer M,Watzinger J.Steel World,2000;5:38
[5]Zhang J M,Zhang L,Wang X H,Wang L F.Ada.Metall Sin,2003;39:1285 (张炯明,张立,王新华,王立峰.金属学报,2003;39:1285)
[6]Zhang X Z,Na X Z,Wang Z Y,Liu A Q,Gan Y.Acta Metall Sin,2004;40:281 (张兴中,那贤昭,王忠英,刘爱强,干勇.金属学报,2004;40:281)
[7]Liu X,Yin H B.In:Li W X,ed.,CSM 2003 Annual Meeting Proc,Beijing:Metallurgical Industry Press,2003:413 (刘晓,尹合壁.见:李文秀主编,2003年中国钢铁年会论文集,北京:冶金工业出版社,2003:413)
[8]Sun J,Pan D H.Res Iron Steel,1998;(5):21 (孙冀,潘德惠.钢铁研究,1998;(5):21)
[9]Pinheiro C A M,Samarasekera I V,Brimacombe J K,Walker B N.Ironmaking Steelmaking,2000;27:37
[10]Huespe A E,Cardona A,Fachinotti V.Comput Methods Appl Mech Eng,2000;182:439
[11]Mahapatra R B,Brimacombe J K,Samarasekera I V.Metall Trans,1991;22B:875
[12]Mills K C,Fox A B.ISIJ Int,2003;43:1479
[13]Billany T J H,Normanton A S,Mills K C,Grieveson P.Ironmaking Steelmaking,1991;18:403
[14]Irving W R,Perkins A.Ironmaking Steelmaking,1977;4:292
[15]Ikeda M,Asano K,Nakano T,Fuji M,Mizoguchi S,Misumi H.Trans Iron Steel Inst Jpn,1981;21:B511
[16]Sugitani Y,Nakamura M,Okuda M,Kawasaki M,Naka-jima K.Trans Iron Steel Inst Jpn,1985;25:B91
[17]Mills K C,Billany T J H,Normanton A S,Walker B N,Grieveson P.Ironmaking Steelmaking,1991;18:253=
[1] 刘中秋, 李宝宽, 肖丽俊, 干勇. 连铸结晶器内高温熔体多相流模型化研究进展[J]. 金属学报, 2022, 58(10): 1236-1252.
[2] 蔡来强, 王旭东, 姚曼, 刘宇. 连铸圆坯非均匀传热/凝固行为的无网格计算方法[J]. 金属学报, 2020, 56(8): 1165-1174.
[3] 刘中秋,李宝宽,姜茂发,张立,徐国栋. 连铸结晶器内氩气/钢液两相非稳态湍流特性的大涡模拟研究[J]. 金属学报, 2013, 49(5): 513-522.
[4] 陈芝会 王恩刚 张兴武 王元华 朱明伟 赫冀成. 行波磁场下吹Ar过程中结晶器内气泡行为的研究[J]. 金属学报, 2012, 48(8): 951-956.
[5] 李宝宽 刘中秋 齐凤升 王芳 徐国栋. 薄板坯连铸结晶器非稳态湍流大涡模拟研究[J]. 金属学报, 2012, 48(1): 23-32.
[6] 冯明杰 王恩刚 赫冀成. 带钢热连轧机工作辊非稳态传热的数值模拟[J]. 金属学报, 2010, 46(8): 1009-1017.
[7] 许秀杰 邓安元 王恩刚 张林涛 张兴武 张永杰 赫冀成. 电磁软接触连铸圆坯表面振痕演变机理[J]. 金属学报, 2009, 45(4): 464-469.
[8] 孟祥宁 朱苗勇. 高拉速板坯连铸结晶器液态渣消耗机理分析[J]. 金属学报, 2009, 45(4): 485-489.
[9] 于海岐 朱苗勇. 圆坯结晶器电磁搅拌过程三维流场与温度场数值模拟[J]. 金属学报, 2008, 44(12): 1465-1473.
[10] 孟祥宁; 朱苗勇 . 高拉速板坯连铸结晶器液体摩擦机理分析[J]. 金属学报, 2008, 44(10): 1193-1197 .
[11] 孟祥宁; 朱苗勇; 程乃良 . 高拉速下连铸坯振痕形成机理及振动参数优化[J]. 金属学报, 2007, 43(8): 839-846 .
[12] 孟祥宁; 朱苗勇; 刘旭东; 程乃良; 江中块 . 高拉速连铸结晶器非正弦振动因子研究[J]. 金属学报, 2007, 43(2): 205-210 .
[13] 郭志鹏; 熊守美; 曺尚铉 ; 崔正吉 . 铝合金压铸过程铸件/铸型界面换热行为的研究II. 工艺参数对界面换热的影响[J]. 金属学报, 2007, 43(11): 1155-1160 .
[14] 郭志鹏; 熊守美; 曺尚铉; 崔正吉 . 铝合金压铸过程铸件/铸型界面换热行为的研究I. 实验研究和界面换热系数求解[J]. 金属学报, 2007, 43(11): 1149-1154 .
[15] 郭亮亮; 姚曼; 尹合壁; 王旭东; 方大成; 刘晓 ; 于艳 . 连铸圆坯结晶器的热流计算与讨论[J]. 金属学报, 2006, 42(9): 983-988 .