| 非晶态铝合金晶化过程的形核与长大行为研究 |
| 张宏闻 王建强 卢柯 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室;沈阳110016 |
|
引用本文:
张宏闻; 王建强; 卢柯 . 非晶态铝合金晶化过程的形核与长大行为研究[J]. 金属学报, 2002, 38(6): 609-612 .
[1] Inoue A. Prog Mater Sci, 1998; 43:365 [2] Greer A L. Nature, 1993; 366: 303 [3] Gangopadhyay A K, Croat T K, Kelton K F. Acta Mater,2000; 48: 4035 [4]Calin M, Koster U. Mater Sci Forum, 1998; 269-272:749 [5] Foley J C, Allen D R, Perepezko J H. Scr Mater, 1996;35: 555 [6]Allen D R, Foley J C, Perepezko J H. Acta Mater, 1998;46: 431 [7] Kwong V, Koo Y C, Thorpe S J, Aust K T. Acta MetallMater, 1991; 39: 1563 [8]Wang Y P, Lu K. Sci Chin, 2000; 30E: 193(王亚平,卢 柯. 中国科学,2000;30E:193) [9]Perepezko J H, Wilde G. J Non-Cryst Solids, 2000; 274:271 [10] Tjong S C, Wang J Q. Z Metallkd, 2001; 92: 610 [11]Chen L C, Spaepen F. Nature, 1988; 336: 366 [12]Chen L C, Spaepen F. J Appl Phys, 1991; 69: 679 |
|