| Ni3Al+NiAl双相合金的氢致开裂过程研究 |
| 李金许 王燕斌 乔利杰 褚武扬 |
| 北京科技大学材料物理与化学系;北京100083 |
|
引用本文:
李金许; 王燕斌; 乔利杰; 褚武扬 . Ni3Al+NiAl双相合金的氢致开裂过程研究[J]. 金属学报, 2002, 38(5): 512-516 .
[1]Wan X J. Zhu J H, Jin K L. Liu C T. Scr Metall Mater,1994; 31: 677 [2]Bergmann G, Vehoff H. Mater Sci Eng, 1995; A192: 309 [3] Cohron J W. George E P, Heatherly L, Liu C T, Zee R H.Acta Mater, 1997; 45: 2801 [4] Schulson E M, Xu Y. Acta Mater, 1997; 45: 349 [5]Liu C T. Scr Metall Mater. 1992: 27: 25 [6]George E P, Liu C T. Pope D P. Acta Mater, 1996;44:1757 [7]Nishimura C, Liu C T. Acta Metall Mater, 1992; 40:723 [8] Wright J L, Zhu J H. Scr Mater, 1998; 38(2): 253 [9]Li J X, Li H Q, Wang Y B, Qiao L J, Chu W Y. Acta Metall Sin, 2001; 37: 1049 (李金许.李红旗.王燕斌.乔利杰.诸武扬.金属学报,2001;37:1049) [10] Chu W Y. Hydrogen-induced Plasticity Loss and Delayed Cracking. Beijing: Metallurgical Industry Press, 1988: 449 (褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社.1988:449)W |
|