| 高能球磨形成具有明显玻璃转变的Ti50Cu20Ni24Si4B2非晶态合金 |
| 张来昌 徐坚 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室;沈阳 110016 |
|
引用本文:
张来昌; 徐坚 . 高能球磨形成具有明显玻璃转变的Ti50Cu20Ni24Si4B2非晶态合金[J]. 金属学报, 2002, 38(3): 299-302 .
[1]Weeber A W, Bakker H. Phys B, 1988; 153: 93 [2]Koch C C. Mater Sci Forum, 1992; 88-90: 243 [3]Seidel M, Eckert J, Schultz L. J Appl Phys, 1995; 77: 5446 [4]Seidel M, Eckert J, Bacher I, Reibold M, Schultz L. ActaMater, 2000; 48: 3657 [5] Sagel A, Wunderlich R K, Fecht H J. Mater Lett, 1997;33:123 [6]Seidel M, Eckert J, Bauer H D, Schultz L. Mater Sci Fo-rum, 1996; 225-227: 119 [7]Nishiyama N, Inoue A. Mater Trans JIM, 1999; 40: 64 [8]Zhang T, Inoue A. Mater Trans JIM, 1998; 39: 1001 [9]Inoue A, Amiya K, Katsuya A, Masumoto T. Mater TransJIM, 1995; 36: 858 [10]Zhang T, Inoue A. Mater Trans JIM, 1999; 40: 301 [11]Koster U. Z Metallkde, 1984; 75: 691 [12]Azaroff L, Buerger M J. The Powder Method in X-RayCrystallography, New York: McGraw-Hill, 1958: 238 [13]JCPDS files, No. 18-889 [14]Kissinger H E. Anal Chem, 1957; 29: 1702 [15] Lu Z P, Tan H, Li Y, Ng S C. Scr Mater, 2000; 42: 667 [16] Turnbull D. Contemp Phys, 1969; 10: 473 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|