全幅二段电磁制动连铸复合钢坯的模拟研究 |
郑红霞 李宝宽 昌泽舟 |
鞍山钢铁学院冶金系;鞍山114002 |
|
引用本文:
郑红霞; 李宝宽; 昌泽舟 . 全幅二段电磁制动连铸复合钢坯的模拟研究[J]. 金属学报, 2001, 37(8): 877-881 .
[1] Yu C T. Metal matrix composite. Beijing: Metallurgyindustry press. 1995: 9(于春田 金属基复合材料.北京:冶金工业出版社,1995:9) [2] Sha C C. Metoll, 1998(3): 38(沙才智 冶金丛刊,1998(3):38) [3] Takeuchi E, Zeze M, Tanaka H, Harada H, Mizoguchi S.Ironmaking Steehaaking, 1997; 24(3): 257 [4] Takeuchi E, Hiroyuki Tanaka, Hiroyuki Kajioka. BPM1994; 364 [5] Takeuchi E, Zeze M, Tanaka H, Harada H, Mizoguchi S.Steelmaking Conf Proc, 1996; 225 [6] Cai K K. Continuous Castiny Steel. Beijing: SciencePress, 1990: 6(蔡开科.连续铸钢.北京:科学出版社,1990:6) |
|