| 双相钢在流动中性含砂氯化物中的磨损腐蚀 |
| 雍兴跃 林玉珍 刘景军 刘淑静 |
| 北京化工大学材料科学与工程学院;北京100029 |
|
引用本文:
雍兴跃; 林玉珍; 刘景军; 刘淑静 . 双相钢在流动中性含砂氯化物中的磨损腐蚀[J]. 金属学报, 2001, 37(7): 745-748 .
[1] Madson B W. Corrosion'80, NACE, Paper No.242, 1980 [2] Matsumura M. Corros Rev, 1994; 12(3-4): 321 [3] Jiang X X, Li S Z. Chem Eng Mach, 1991; 18: 150 (姜晓霞,李诗卓,化工机械, 1991; 18: 150) [4] Zhou S, Stack M M, Newman R C. Corrosion, 1996; 52:934 [5] Zheng Y G, Yao Z M, Li S C, Wang S C, Ke W. J ChinSoc Corros Protect, 1993; 13: 390 (郑玉贵,姚治铭,李生春,王世才,柯伟.中国腐蚀与防护学报,1993;13:390) [6] Lin Y Z. Total Corros Protect, 1996; 10(4): 1 (林玉珍.全面腐蚀控制,1996; 10(4):1) [7] Lin Y Z, Liu J J, Yong X Y, Li H W, Cao C N. J ChinSoc Corros Protect, 1999; 19: 1 (林玉珍,刘景军,雍兴跃,李焕文,曹楚南.中国腐蚀与防护学报.1999;19:1) [8] Yong X Y. PhD Thesis, Institute of Corrosion and Protection of Metals, The Chinese Academy of Sciences,Shenyang, 2000 (雍兴跃.中国科学院金属腐蚀与防护研究所博士学位论文,沈阳,2000) [9] Yong X Y, Liu J J, Lin Y Z, Li H W, Han J Y, Wu J.Corros Sci Protect Technol, 1999; 11: 295 (雍兴跃,刘景军,林玉珍,李焕文,韩俊媛,吴玖、腐蚀科学与防护技术,1999;11:295) [10] Cao C N. Corrosion Electrochemistry. Beijing: ChemicalIndustry Press, 1994) (曹楚南.腐蚀电化学.北京:化学工业出版社,1994) [11] Cao C N, Wang J, Lin H C. J Chin Soc Corros Protect,1989; 9: 261 (曹楚南,王佳,林海潮.中国腐蚀与防护学报,1989;9:261) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|