| 电弧压力对MIG焊接熔池几何形状的影响 |
| 孙俊生 武传松 |
| 山东大学连接技术研究所;济南250061 |
|
引用本文:
孙俊生; 武传松 . 电弧压力对MIG焊接熔池几何形状的影响[J]. 金属学报, 2001, 37(4): 434-438 .
[1] Wu C S, Dron L. Acta Metall Sin, 1997; 33: 774(武传松, Dron L. 金属学报, 1997; 33: 774) [2] Lancaster J F. The Physics of Welding. New York: Pergamon Press, 1986: 135 [3] Lin M L, Eagar T W. Metall Trans, 1986; 17B: 601 [4] Kim J-W, Na S-J. Weld J, 1995; 5: 141s [5] Choo R T C, Szekely J, Westhoff. Weld J, 1990; 69: 346s [6] Tsai M C, Kou S. Weld J, 1990; 69: 241 s [7] Tsai N S, Eagar T W. Metall Trans, 1985; 16B: 841 [8] Wu C S, Sun J S. Comput Mater Sci, 1998; 9: 397_ |
|