| 强度错配双层金属板垂直界面裂纹疲劳扩展行为 |
| 江峰 康伟 赵康 孙军 何家文 |
| 西安交通大学金属材料强度国家重点实验室;西安710049 |
|
引用本文:
江峰; 康伟; 赵康; 孙军; 何家文 . 强度错配双层金属板垂直界面裂纹疲劳扩展行为[J]. 金属学报, 2001, 37(10): 1053-1058 .
[1] Erdogan F, Biricikpglu V. Int J Eng Sci, 1973; 11: 745 [2] Delfin P, Gunnars J, Stahle P. Fatigue Fract Eng MaterStruct, 1995; 10: 1201 [3] Kim A S, Besson J, Pineau A. Int J Solids Struct, 1999;36: 1845 [4] He M Y, Hutchinson John V. Int J Solids Struct, 1989;11: 745 [5] Leguillon D, Lacroix C, Martin E. J Mech Phys Solids,2000; 48: 2137 [6] Suresh S, Sugimura Y, Tschegg E K. Scr Metall Mater,1992; 27: 1189 [7] Suresh S, Sugimura Y, Ogawa T. Scr Metall Mater, 1993;29: 237 [8] Sugimura Y, Grondin L, Suresh S. Scr Metall Mater, 1995;33: 2007 [9] Sugimura Y, Lim P G, Shih C F, Suresh S. Acta MetallMater, 1995; 43: 1157 [10] Kim A S, Suresh S. Int J Solids Struct, 1997; 26: 3415 [11] Pippan R, Riemelmoser F O. Comput Mater Sci, 1998;13: 108 [12] Pippan R, Flechsig K, Riemelmoser F O. Mater Sci Eng,2000; 283A: 225 [13] Zheng Y M, Zhang S J. Res Iron Steel, 1998; (1): 30(掷远谋,张胜军. 钢铁研究,1998;(1):30) [14] Zheng Y M, Huang R G, Chen S H. Eng Blast, 2000; 16:25(郑远谋.黄荣光.陈世红.工程爆破.2000;16:25) [15] Shih C F, O'Dowd N P, Kirk M T. ASTM STP 1171,1993, |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|