| Ni3Al+NiAl双相合金的氢致开裂 |
| 李金许 李红旗 王燕斌 乔利杰 褚武扬 |
| 北京科技大学材料物理与化学系;北京100083 |
|
引用本文:
李金许; 李红旗; 王燕斌; 乔利杰; 褚武扬 . Ni3Al+NiAl双相合金的氢致开裂[J]. 金属学报, 2001, 37(10): 1049-1052 .
[1] Xu K, Arsenault R J. Acta Metall, 1999; 47: 3023 [2] Deevi S C, Sikka V K. Intermetallic, 1996; 4: 357 [3] Sikka V K. Mater Sci Eng, 1992, 153A: 714 [4] Lee J H, Choe B H, Kim H M. Mater Sci Eng. 1992; 152A:253 [5] Liu C T. Scr Metall Mater, 1992; 27: 25 [6] George E P, Liu C T, Pope D P. Acta Mater, 1996; 44,1757 [7] Cohron J W, George E P Heatherly L, Liu C T, Zee R H.Acta Mater, 1997, 45: 2801 [8] Schulson E M, Xu Y. Acta Mater, 1997, 45: 3491 [9] Wan X J, Zhu J H, Jin K L, Liu C T. Scr Metall Mater1994; 31: 677 [10] Bergmann G, Vehoff H. Mater Sci Eng, 1995; 192A: 309 [11] Wright J L, Zhu J H. Scr Mater, 1998, 38. 253 [12] Nishimura C, Liu C T, Scr Metall Mater, 1991; 25: 791 [13] Chu W Y, Yao J, Hsiao C M. Metall Trans, 1984; 15A:729 [14] Chu W Y. Hydrogen-Induced Plasticity Loss, and DelayedCracking. Beijing: Metallurgical Industry Press, 1988:254(褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社.1988:254) [15] Li M D, Lu H, Zhang T C, Chu W Y, Sci Chin, 1997;40E: 530 [16] Chu W Y, Qiao L J, Wang Y B, Corrosion, 1999: 55: 667J |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|